In this work, a functional nanocomposite consisting of multi walled carbon nanotubes combined with nanoparticles of silver and Pomegranate peel extract (MWCNTs- SNPs -NPGPE) was successfully synthesized using ultra sonic technique. The nanocomposite has been characterized using Transmission electron microscope (TEM), XRD, Energy dispersive X-ray spectroscopy (EDS) UV-Vis and FTIR. The obtained results reveal that the MWCNTs-SNPs-NPGPE nanocomposite exhibits form of nanotubes with rough surfaces and containing black spots, which are the silver nanoparticles. The dimensions of this tube are 161 nm in length and 60 nm in width with nanoparticles of silver not exceeding 20 nm. The XRD pattern of the prepared MWCNTs-SNPs-NPGPE nanocomposite showed four main peaks corresponding to the carbon nanotubes and planes of face centered cubic silver nanoparticles. The IR spectra referring to the(O-H) group stretching vibrations in carboxylic acid groups might come from NPGPE, and the stretching vibration of aliphatic C-H in carbon nanotubes. The carbon nanotube was used in solar cells (CNSCs) fabricated with and/or without fluorine-doped tin oxide (FTO) on the glass substrate with poly(3-hexylthiophene) (P3HT) and [6,6]-phenyl C61-butyric acid methylester (PCBM) blends (P3HT: PCBM). The FTO-(MWCNTs-SNPs-NPGPE / P3HT: PCBM/CNT/FTO-glass revealed more efficient CNSCs.
In this research (100* 40* 4 cm) solar cell panel was used in Baghdad at autumn season (2010), to get best solar cell panel angles experimentally, and then a mirror (40*50 cm) is use to concentrate incident sunlight intensity on a panel. At first case we get (Tilt angle ?P =60°and Surface Azimuth angle ?P =36°E) is the best angles and other case, we add a mirror at angle = 120° at bottom of panel, then we get output power (27.48watt) is bigger than without using a mirror (25.16watt). We can benefit from these cases in variety applications.
In this research study Hardness (shore D), Water absorption,
Flexural, Impact Test, and Fracture Toughness of polymer nano
composites. The polymer nano composites based on unsaturated
polyester resin reinforced with Kevlar fibers (K.F). The samples are
attended by hand lay – up method according to (Rule mixture) for
various volume fractions of unsaturated polyester resin, fiber and
carbon nanotube. The polyester resin was matrix strengthened with
3% volume fraction from Kevlar fiber and (0.5%, 1%, 1.5%, 2%)
volume fractions of carbon nanotube. The water absorption, hardness
(shore D), flexural test, impact test and toughness fracture properties
were studied. Results showed that the water absorption increas
A newly flow injection-turbidimetric method characterized by it is speed and sensitivity has been developed for the determination of Amiloride in pure and pharmaceutical preparations. It is based on the formation of yellowish white precipitate for the Amiloride-phosphomolybidic acid ion pair in aqueous medium. Turbidity was measured by Ayah 6Sx1-T-1D solar cell CFI analyser via the attenuation of incident light from the surfaces precipitated particles at 0-180. The Chemical and physical parameters were investigated. Linear dynamic range for the attenuation of incident light versus Amiloride concentration was of 0.005-10 mmol.L-1, with the correlation coefficient (r) of 0.9986 , while the percentage linearity (r2%) was 99.71%. The L.O.
... Show MoreA newly flow injection-turbidimetric method characterized by it is speed and sensitivity has been developed for the determination of Amiloride in pure and pharmaceutical preparations. It is based on the formation of yellowish white precipitate for the Amiloride-phosphomolybidic acid ion pair in aqueous medium. Turbidity was measured by Ayah 6Sx1-T-1D solar cell CFI analyser via the attenuation of incident light from the surfaces precipitated particles at 0-180. The Chemical and physical parameters were investigated. Linear dynamic range for the attenuation of incident light versus Amiloride concentration was of 0.005-10 mmol.L-1, with the correlation coefficient (r) of 0.9986 , while the percentage linearity (r2%) was 99.71%. The L.O.
... Show MoreThe present research was conducted to reduce the sulfur content of Iraqi heavy naphtha by adsorption using different metals oxides over Y-Zeolite. The Y-Zeolite was synthesized by a sol-gel technique. The average size of zeolite was 92.39 nm, surface area 558 m2/g, and pore volume 0.231 cm3/g. The metals of nickel, zinc, and copper were dispersed by an impregnation method to prepare Ni/HY, Zn/HY, Cu/HY, and Ni + Zn /HY catalysts for desulfurization. The adsorptive desulfurization was carried out in a batch mode at different operating conditions such as mixing time (10,15,30,60, and 600 min) and catalyst dosage (0.2,0.4,0.6,0.8,1, and 1.2 g). The most of the sulfur compounds were removed at 10 min for all catalyst ty
... Show MoreIn this paper two axis sun tracking method is used to absorb maximum power from the sun's rays on the solar panel via calculating the sun’s altitude and azimuth angles, which describe the solar position on the Iraqi capital Baghdad for the hours 6:00, 7:00, 8:00, 9:00, 12:00, 15:00 and 17:00 per day. The angles were calculated in an average approach within one month, so certain values were determined for each month. The daily energy achieved was calculated for the solar tracking method compared with the fixed tracking method. Designed, modeled and simulated a control circuit consisting of reference position truth table, PI Controller and two servomotors that tracked the sun position to adjust the PV panel perpendicular
... Show MoreWe investigated at the optical properties, structural makeup, and morphology of thin films of cadmium telluride (CdTe) with a thickness of 150 nm produced by thermal evaporation over glass. The X-ray diffraction study showed that the films had a crystalline composition, a cubic structure, and a preference for grain formation along the (111) crystallographic direction. The outcomes of the inquiry were used to determine these traits. With the use of thin films of CdTe that were doped with Ag at a concentration of 0.5%, the crystallization orientations of pure CdTe (23.58, 39.02, and 46.22) and CdTe:Ag were both determined by X-ray diffraction. orientations (23.72, 39.21, 46.40) For samples that were pure and those that were doped with
... Show MoreThis research includes the use of CdTe in the design of a solar cell. The SCAPS-1D computer program was used to simulate thin cell capacity of CdTe/CdS by numerical analysis with the addition of a buffer layer (Zn2SnO4) to enhance cell efficiency. The thickness of the window layer (n-CdS) was reduced to 25nm with the inclusion of an insulating layer of 50 nm thickness to prevent leakage towards the forward bias with respect to the lower charge carriers. As for the absorber layer thickness (p-CdTe), it varied between 0.5µm and 6µm. The preferable thickness in the absorbent layer was 1.5µm. Different operating temperatures (298K-388K) were used, while the highest conversion efficiency (η=18.43%) was obtain
... Show More