The induced photodegradation of methyl cellulose (MC) films in air was investigated in the absence and presence of aromatic carbonyl compounds(photosenssitizers): 1,4-naphthaquinone (NQ) and benzophenone (BPH) by accelerated weathering tester. The addition of (0.01 wt %) of low molecular weight aromatic carbonyl compounds to cellulose derivatives films(25µm in thickness) enhanced the photodegradation of the polymer films.The photodegradation rate was measured by the increase in carbonyl absorbance. Decreases in solution viscosity and reduction of molecular weight were also observed in the irradiated samples. Changes in the number-average chain scission, the degree of deterioration and in the quantum yield of chain scission values are also observed, and it was concluded that branching or cross-linking has occurred for cellulose derivative with NQ and BPH. Findings from all analytical techniques indicated that the 1,4-naphthaquinone (NQ) photosensitizer enhance the photodegradation of methyl cellulose more than benzophenone (BPH). The effect of the photosensitizer concentration, (ranging from 0.01 to 0.1 %), on the rate of photodegradation was also monitored for MC films. The rates are increased with increasing the photosensitizer concentration. The effect of film thickness is also studied at fixed sensitizer concentration (0.05%), and results show that the rate of cellulose derivative photodegradation decreases with increasing film thickness. The rate constants of the photodegradation of the photosensitizers deduced in cellulose derivatives films, [at concentration of (0.1%)by weight and thickness (25µm)]. Biodegradation of irradiated cellulose derivatives films was conclusively established with bacteria type Pseudomonas aeuroginosa Rb-19 isolated from crude oil. The amount of bacteria growth on MC after 30 days was lower, while there was no growth observed in MC with BPH
Background: Thermocycling simulates the temperature dynamics in the oral environment. This in vitro study done to measure and compare the effect of thermocycling on the shear bond strength of stainless steel and sapphire brackets bonded to human enamel teeth using light cured orthodontic adhesive and debonded at various time, and to measure adhesive remnant index after debonding. Materials and Methods: one-hundred-twenty extracted upper first premolars for orthodontic reason were used in this study; depending on weather thermocycled or not, the sample was divided into two main groups, then within each group 30 teeth were used for stainless-steel brackets (Bionic®) and for sapphire brackets (Pure®). Both groups were subdivided into three
... Show MoreNigella sativa seeds (NSS) are reputed traditionally and scientifically as a potent agent that promote milk secretion (galactagogue), but their mechanism of action is studied trivially. One suggestion was that these seeds are bio-transformed to sex hormones within the ovaries. Therefore, this investigation was designated to throw light on the action of these seeds in the absence of ovaries i.e. in male rats. Thirty Norway male albino rats were used in this investigation. They were divided into experimental (n=20,fed NSS 2g/ Kg body weight /day for 14 days) and control (n=10, fed placebo for 14 days). After sacrifice mammary gland and blood samples were obtained. Experimental rats revealed a significant increase (p (0.01>in
... Show MoreExperiment Factorial conducted with two factor in field texture silt clay loam soil, the first factor were Two Rotavator plow which different in number of rotary blades on flanges, weight, width, made and type, the second factor were four speeds tractor 2.62, 5.10, 7.55, 9.23 km/hr to compare performance two Rotavator under depth 12 cm and knowledge slippage, distance between beat blades, practical productivity, disturbed soil volume, percentage of the soil clods which have diameter less than 5 cm under complete block design with three replications using Least Significant Design 0.05. Results showed Galucho Rotavator recorder the higher practical productivity 0>7089 ha/hr, disturbed soil volume 809.8 m3/hr, percentage of the soil clods 96.1
... Show MoreIn this work, corrosion parameters were evaluated using potentiodynamic polarization curves. In order to determine corrosion parameters of potential and current density of the interesting metal, carbon steel, environmental conditions of external corrosion of buried carbon steel pipeline in Iraqi soil were prepared in the laboratory using simulated prepared conditions. Solutions of sodium chloride at different concentrations (300, 1100, 1900, 2700, and 3500 ppm) were used. pH of solution were acidic at pH =5, and alkaline at pH = 9. Laboratory conditions were similar to those of Iraqi soil where the pipelines were buried. Temperature was constant at 20 °C. Potentiodynamic polarization curves, of potential vs. log current density, were ob
... Show MoreThe effect of saline magnetized water irrigation on seed germination and seedling growth of wheat cultivar Iraq were studied. Irrigation water was supplemented with different levels of Sodium chloride 6, 12 or 18 mmhos/ cm in addition control treatment, and passed through a proper magnetic felid with 1000, 1250, 1500 or 2000 gaus in addition control treatment. The results showed significantly stimulated shoot development and led to the increase of germination, seedling emergence, area leaf, length of shoot and root and fresh and dry weight compared to the controls. Results also showed significant interaction between saline water and magnetized water. So, using magnetic treatment of saline water could be a promising technique
... Show MoreEffect of nano and micro SiO2 particles with different weight percent (2,4,6,8 and 10) %wt on the Interlaminar fracture toughness (GIc) of 16-plies of woven roving glass fiber /epoxy composites prepared by hand lay – up technique were investigated. The specimens were tested using DCB test (mode I).
Area method was used to compute the interlaminar fracture toughness. The results show that, GIc would increase with the increasing in the filler content, the main failure in microcomposites and nanocomposites was delamination in the layers, the delamination reduced with increasing in the filler content.