Different polymers were prepared by condensation polymerization of sebacic anhydride and adipic anhydride with ethylene glycol and poly(ethylene glycol). Their number average molecular weights were determined by end group analysis. Then, they were grafted on the prepared phthalocyaninatocopper(II) compounds with the general formula (NH2)4PcCu(II) having amino groups of 3,3',3'',3'''- or 4,4',4'',4'''- positions. All prepared polymers, compounds, and phthalocyaninatocopper(II)-grafted polymers were characterized by FTIR. The sizing measurements were carried out in 3,3',3'',3'''- (NH2)4PcCu(II) and 4,4',4'',4'''- (NH2)4PcCu(II) compounds with and without grafting polymers. The results showed that the grafting process led to decreasing in particle size and increasing in surface area. The grafting process was reflected positively on the thermal degradation of 3,3',3'',3'''- (NH2)4PcCu(II) and 4,4',4'',4'''- (NH2)4PcCu(II) grafted polymers. They had higher thermal stability accompanied with higher char residue and T50% weight loss with 3,3',3'',3'''-(NH2)4PcCu(II) and their grafted polymers being the best.
Thin a-:H films were grown successfully by fabrication of designated ingot followed by evaporation onto glass slides. A range of growth conditions, Ge contents, dopant concentration (Al and As), and substrate temperature, were employed. Stoichiometry of the thin films composition was confirmed using standard surface techniques. The structure of all films was amorphous. Film composition and deposition parameters were investigated for their bearing on film electrical and optical properties. More than one transport mechanism is indicated. It was observed that increasing substrate temperature, Ge contents, and dopant concentration lead to a decrease in the optical energy gap of those films. The role of the deposition conditions on value
... Show MoreThin films of highly pure (99.999%) Tellurium was prepared by high vacuum technique (5*10-5torr), on glass substrates .Thin films have thickness 0.6m was evaporated by thermal evaporation technique. The film deposited was annealed for one hour in vacuum of (5*10-4torr) at 373 and 423 K. Structural and electrical properties of the films are studies. The x-ray diffraction of the film represents a poly-crystalline nature in room temperature and annealed film but all films having different grain sizes. The d.c. electrical properties have been studied at low and at relatively high temperatures and show that the conductivity decreases with increasing temperature at all range of temperature. Two types of conduction mechanisms were found to d
... Show MoreA new carbonyl complexes of triazole and oxadiazole were synthesized. These complexes were identified and their structural geometric were suggested by using FT-IR and UV-Vis spectra, conductivity measurements and other chemical and physical properties. The spectra data (FT-IR, UV, Vis.) with the substantial aid of group theoretical calculations gave so many evidences for the proposed geometries and the type of bonding of these compounds
Gelatin a promising biomaterial which is useful and interesting natural polymer which offer possibilities of chemical modification through grafted copolymerization with an saturated acid anhydride such as methyl nadic anhydride formatted gelatin –g- methyl nadic anhydride copolymer (A1), then modified to its corresponding polymer (A2) by substituted salbutamol as useful derivative as biomaterial .the prepared drug biopolymer was characterization by FTIR spectroscopy and thermal analysis was studied controlled drug release was measured in different buffer solution at 37C0 .
Polyimide/polyaniline nanofiber composites were prepared by in situ polymerization with various weight percentages of polyaniline (PANI) nanofibers. X-ray diffraction (XRD) and Fourier transform infrared spectra (FT-IR), proved the successful preparation of PANI nanofiber composite films. In addition, thermal stability of PI/PANI nanofiber composites was superior relative to PI, having 10 % gravimetric loss in the range of 623 °C to 671 °C and glass transition temperature of 289 °C to 297 °C. Furthermore, the values of the loss tangent tanδ and AC conductivity σAC of the nanocomposite films were notably higher than those of pure polyimide. The addition of 5 wt.% to 15 wt.% PANI
The plant licorice is considered important plants as nutritionally and medically and economically, as a rich in phytochemical, vitamins and minerals, and being widely available, Research indicated the presence of many nutrients such as (proteins, Carbohydrates, vitamins and minerals) as well as presence of Glycyrrhizin which responsible of sweet taste, that allowing the possibility to use it as natural intensity sweetener with few calories in Sweetening of many food. This research is aimed to study the Stability of Glycyrrhizin toward the various manufacturing conditions such as (thermal treatment, pH of foods and microwaves), so three factorial experiments was implemented to find out the Stability as following: 100C° - 121C° - Microwa
... Show MoreA novel metal complexes Cu (II), Co (II), Cd (II), Ru (III) from azo ligand 5-((2-(1H-indol-2-yl)
ethyl) diazinyl)-2-aminophenol were synthesized by simple substitution of tryptamine with 2-aminophenol.
Structures of all the newly synthesized compounds were characterized by FT IR, UV-Vis, Mass spectroscopy
and elemental analysis. In addition measurements of magnetic moments, molar conductance and atomic
absorption. Then study their thermal stability by using TGA and DSC curves. The DCS curve was used to
calculate the thermodynamic parameters ΔH, ΔS and Δ G. Analytical information showed that all complexes
achieve a metal:ligand ratio of [1:1]. In all complex examinations, the Ligand performs as a tri
Indium oxide In2O3 thin films fabricated using thermal evaporation of indium metal in vacuum on a glass substrate at 25oC using array mask, after deposition the indium films have been subjected to thermal oxidation at temperature 400 °C for 1h. The results of prepared Indium oxide reveal the oxidation method as a strong effect on the morphology and optical properties of the samples as fabricated. The band gap (Eg) of In2O3 films at 400 °C is 2.7 eV. Then, SEM and XRD measurements are also used to investigate the morphology and structure of the indium oxide In2O3 thin films. The antimicrobial activity of indium oxide In2O3 thin films was assessed against gram-negative bacterium using inhibition zone of bacteria which improved higher ina