Preferred Language
Articles
/
bsj-2663
Fracture Toughness and Hardness studying for Polymer-Ceramic Composite
...Show More Authors

A particulate composite material was prepared by adding the Titanium dioxide (TiO2) with a particle size of (75-150) µm to Epoxy resin at weight percentage of (10%,20%,30%,40%,50%).The following some mechanical properties were studied,fracture toughness, hardness.casting preparation methods were used in this study includes preparing plate of matrix and composites. specimens were prepared according to ASTM for the Mechanical properties tests. After that Another samples were heat treated for three and six hour at 65C?. Fracture toughness (Kic) represent for stress intensity factor results were showed that the curve of three hours aging increases in fracture toughness (Kic) for composites but for six hours aging increases fracture toughness (Kic) for polymer matrix. Hardness tests was showed that hardness results increased with the increase in weight fraction while a samples that not treated thermally have higher hardness than the samples for treated thermally. Finally, fracture surfaces were showed morphology failure surfaces by using an optical Microscope.

Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Sat Mar 01 2008
Journal Name
Iraqi Journal Of Physics
Interlaminar fracture toughness of some polymer blends reinforced by fiber glass
...Show More Authors

The interlaminar fracture toughness of polymer blends reinforced by glass fiber has
been investigated. Epoxy (EP), unsaturated polyester(UPE), polystyrene (PS),
polyurethane (PU) and their blends with different ratios (10%PS/90%EP),
(20%PS/80%EP), (20%PU/80%EP) and (20%PU/80%UPE) were chosen as a matrices A
sheet of composites were prepared using hand lay -up method, these sheet were cut as the
double cantilever beam (DCB) specimen to determine interlaminar fracture toughness of
these composites .Its found that, blending of EP,UPE with 20% of PU will improve the
interlaminar fracture toughness ,but the adding of 10% PS, 20%PS to EP will decrease
the interlaminar toughness of these composites.

View Publication Preview PDF
Publication Date
Tue Jan 01 2019
Journal Name
Aip Conference Proceedings
Studying some of mechanical properties (tensile, impact, hardness) and thermal conductivity of polymer blend reinforce by magnesium oxide
...Show More Authors

View Publication
Scopus (3)
Crossref (1)
Scopus Clarivate Crossref
Publication Date
Tue Sep 04 2018
Journal Name
Al-khwarizmi Engineering Journal
Studying the Mechanical Properties of Denture Base Materials Fabricated from Polymer Composite Materials
...Show More Authors

In this research, the effect of adding two different types of reinforcing particles was investigated, which included: nano-zirconia (nano-ZrO2) particles and micro-lignin particles that were added with different volume fractions of 0.5%, 1%, 1.5% and 2% on the mechanical properties of polymer composite materials. They were prepared in this research, as a complete prosthesis and partial denture base materials was prepared, by using cold cure poly methyl methacrylate (PMMA) resin matrix. The composite specimens in this research consist of two groups according to the types of reinforced particles, were prepared by using casting methods, type (Hand Lay-Up) method. The first group consists of PMMA resin reinforced by (nano-ZrO

... Show More
View Publication Preview PDF
Crossref (8)
Crossref
Publication Date
Mon Jan 01 2018
Journal Name
Aip Conference Proceedings
Study optoelectronic properties for polymer composite thick film
...Show More Authors

View Publication
Scopus (6)
Crossref (2)
Scopus Clarivate Crossref
Publication Date
Mon Oct 01 2012
Journal Name
Iraqi Journal Of Physics
Effect of nano and micro SiO2 weight percent on interlaminar fracture toughness of woven roving/ epoxy composites
...Show More Authors

Effect of nano and micro SiO2 particles with different weight percent (2,4,6,8 and 10) %wt on the Interlaminar fracture toughness (GIc) of 16-plies of woven roving glass fiber /epoxy composites prepared by hand lay – up technique were investigated. The specimens were tested using DCB test (mode I).
Area method was used to compute the interlaminar fracture toughness. The results show that, GIc would increase with the increasing in the filler content, the main failure in microcomposites and nanocomposites was delamination in the layers, the delamination reduced with increasing in the filler content.

View Publication Preview PDF
Publication Date
Sun Apr 08 2018
Journal Name
Al-khwarizmi Engineering Journal
Study the Effect of Welding Heat Input on the Microstructure, Hardness, and Impact Toughness of AISI 1015 Steel
...Show More Authors

In the present study, MIG welding is carried out on low carbon steel type (AISI 1015) by using electrode ER308L of 1.5mm diameter with direct current straight polarity (DCSP). The joint geometry is of a single V-butt joint with one pass welding stroke for different plate thicknesses of 6, 8, and 10 mm. In welding experiments, AISI 1015 plates with dimensions of 200×100mm and edge angle of 60o from both sides are utilized. In this work, three main parameters related to MIG welding process are investigated, which are welding current, welding speed, heat input and plate thickness, and to achieve that three groups of plates are employed each one consists of three plates. The results indicate that increasing the weld heat input (t

... Show More
View Publication Preview PDF
Publication Date
Fri Mar 01 2019
Journal Name
Al-khwarizmi Engineering Journal
Studying the Effect of Volume Fraction of Glass Fibers on the Thermal Conductivity of the Polymer Composite Materials
...Show More Authors

In this study the effect of fiber volume fraction of the glass fiber on the thermal conductivity of the polymer composite material was studied. Different fiber volume fraction of glass fibers were used (3%, 6%, 9%, 12%, and 15%). Specimens were made from polyester which reinforced with glass fibers .The fibers had two arrangements according to the direction of the thermal flow. In the first arrangement the fibers were parallel to the direction of the thermal flow, while the second arrangement was perpendicular; Lee's disk method was used for testing the specimens. The experimental results proved that the values of the thermal conductivity of the specimens was higher when the fibers arranged in parallel direction than that when the fibers

... Show More
View Publication Preview PDF
Publication Date
Mon Dec 23 2024
Journal Name
Journal Of Baghdad College Of Dentistry
The influence of cavity design for cusp coverage on fracture strength of weakened maxillary first premolars using two esthetic restorative systems (CAD/CAM hybrid ceramic and nanohybrid composite) (An in vitro study)
...Show More Authors

Background: Maxillary first premolar with wide MOD cavity more susceptible to fracture. The aim of this study was to assess the influence of cavity design for cusp coverage on the fracture resistance of weakened maxillary first premolar restored with CAD/CAM hybrid ceramic versus nanohybide composite. Materials and Methods: Fifty six intact maxillary first premolars of approximately comparable sizes were divided into seven groups eight for each: Group A: Intact teeth (control group); Group B: teeth prepared for MOD inlay; Group C: teeth prepared for MOD onlay covering the lingual cusp; Group D: teeth prepared for MOD covering buccal and lingual cusps ,the previous three groups indirectly restored with nanohybrid composite (3M ESPE Z 250 X

... Show More
View Publication Preview PDF
Publication Date
Tue Oct 20 2020
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Synthesis and some Features of Three-Phases Polymer/Metal/Ceramic Multilayers Nanocomposite
...Show More Authors

      Layer by layer development two features of pulsed laser deposition PLD, with a high kinetic energy and sharp instantaneous deposition rating. Layered films of polymer/metal/ceramic nanocomposites consisting of polystyrene PS(as substrate) , tin Sn and cadmium oxide CdO were deposited by PLD. Structure for layered samples were measured  by XRD X ray diffraction, there were appearance of peaks  which reflected  to formation of new compounds result of  reaction between layers. Particles size  was calculated using two methods and it give nanoscale. Microstrain was also calculated  and exhibited  high value (0.01) for sample p/m.

 

View Publication Preview PDF
Crossref
Publication Date
Fri Aug 10 2018
Journal Name
Ceramics International
Application of zirconia surface coating to improve fracture resistance and stress distribution of zirconia ceramic restorations
...Show More Authors

Zirconia ceramic restoration (ZCR) has a higher fracture incidence rate than metal ceramic restoration. Different surface treatments were used to improve fracture performance of ZCR such as grit blasting (GB) by aluminium oxide powder. This type of surface treatment generate residual stresses on veneering ceramic causing crack initiation and ending with a fracture. In order to overcome the stress generated by GB, zirconia surface coating is used as a surface treatment to improve fracture resistance and to accommodate stresses along the ZCR layers. Fifty zirconia ceramic crowns were fabricated and divided according to the type of surface treatment into three groups; the first group is (ZG), involving 20 cores were coated with a mixture of pa

... Show More
Scopus (3)
Scopus