A batch adsorption system was applied to study the adsorption of methylene blue from aqueous solution by Iraqi bentonite and treated bentonite with different amount of zinc oxide (ZnO). The adsorption capacities of methylene blue onto bentonite were evaluated. The equilibrium between liquid and solid phase was described by Langmuir model better than the Freundlich model. Langmuir and Freundlich constants have been determined. The separation factor or equilibrium parameter, RL which is used to predict if an adsorption system is favourable or unfavourable was calculated for all cases.
In this study the adsorption of cefixime on to selected Iraqi clay bentonite. The aim of this study is to search for selective active surface in adsorption of the drug and to act as physical antidotes in treatment of poisoning if the drug is taken in quantities higher than the recommended dosages. Quantitative estimation of the drug adsorption has been done by utilizing the technique of UV spectrophotometry in λmax (273) nm at different conditions of temperature (25, 37, 45) ˚C found the adsorption decrease with increase the temperature. Study of clay weight of bentonite (0.1-1.5) gm found the adsorption increase with increase of clay weight, study effect of pH (1.2, 3, 5, 7) on adsorption of bentonite found the optimum adsorption
... Show MoreIn this research, design of advanced material for sunlight conversion requires focused research to obtain efficient photocatalytic system. Nanostructured ZnO was synthesized using spin coating technique. The structural, morphological and optical properties of annealed nanostructured ZnO thin film at 390 Co for 3 hours were characterized by x-ray diffraction, atomic force microscope AFM and UV-VIS spectrophotometer. Nanostructured ZnO was applied for removal Methylene Blue (MB) dye from water using sunlight induced photocatalytic process. Overall degradation of MB/ZnO was achieved after 120 minutes of sunlight irradiation while it needs more time for MB alone. The reaction rate constant fit pseudo first order for MB/ZnO degradation was 0.
... Show MoreKE Sharquie, SA Al-Mashhadani, AA Noaimi, AA Hasan, Journal of Cutaneous and Aesthetic Surgery, 2012 - Cited by 19
The research discussed the possibility of adsorption of Brilliant Blue Dye (BBD) from wastewater using 13X zeolite adsorbent, which is considered a byproduct of the production process of potassium carbonate from Iraqi potash raw materials. The 13X zeolite adsorbent was prepared and characterized by X-ray diffraction that showed a clear match with the standard 13X zeolite. The crystallinity rate was 82.15% and the crystal zeolite size was 5.29 nm. The surface area and pore volume of the obtained 13X zeolite were estimated. The prepared 13X zeolite showed the ability to remove BBD contaminant from wastewater at concentrations 5 to 50 ppm and the removal reached 96.60% at the lower pollutant concentration. Adsorption measurements versus tim
... Show MoreBackground: This study aimed to examine the efficacy of methylene blue (MB) and toluidine blue O (TBO) photodynamic therapy (PDT) as adjuncts to root surface debridement (RSD). Methods: This split-mouth, randomized, controlled clinical trial included eighteen patients, and a total of 332 sites (control = 102, MB = 124 and TBO = 106) were examined. Two sessions of PDT were completed at baseline and two weeks after RSD. Clinical parameters of bleeding on probing (BOP), plaque index (PI), probing pocket depth (PPD), and clinical attachment level (CAL) were measured pre- and post-treatment. Results: PPD and BOP reductions in sites treated by RSD with adjunctive photosensitizers (MB and TBO) were significantly higher than in control site
... Show MoreIn this work, a ceramic model has obtained from Iraqi bentonite as a base material with limited additions of alumina and silica. The selected material can bear temperatures higher than the bearing temperature of bentonite as it achieved tolerance temperatures (1300°C) based on X-ray diffraction patterns. It was found that the addition of alumina and silica led to the occurrence of basic phases such as mullite, quartz, cordierite and feldspar in percentages that depended on the percentage of addition in the mixture and the firing temperature, which was (1000-1300)°C.
KE Sharquie, AA Noaimi, SD Hameed, Journal of Cosmetics, Dermatological Sciences and Applications, 2013 - Cited by 15
KE Sharquie, AA Al-Nuaimy, FA Al-Shimary, Saudi medical journal, 2005 - Cited by 20