Role of Tin Oxide on the Structural, Optical and Electrical Properties of Pulsed Laser Deposited (ZnO)<sub>1-x</sub>(SnO<sub>2</sub>)<sub>x </sub>Composite Thin Films
...Show More Authors

This research examines the electrical, optical, and structural properties of zinc oxide (ZnO) and tin(IV) oxide (ZnO)1-x (SnO2)x composite thin films made by pulsed laser deposition, as well as the impact of composition concentration. The structural study of (ZnO)1-x (SnO2)x composites and thin films was conducted by X-ray analysis (XRD). Optical properties were investigated by UV–Vis infrared spectroscopy. The structural analysis revealed that all prepared thin-film composites were polycrystalline, exhibiting both hexagonal wurtzite and tetragonal phases for pure ZnO and SnO2, as well as a mixture of both phases for x=0.2 and 0.4. In contrast, the SnO2 phase was predominant for x=0.6 and 0.8. The increase in crystal size in the (ZnO)1-x (SnO2)x composite thin films was observed at x = 0.4 and 1.0. The optical band gap of (ZnO)1-x (SnO2)x composites exhibited a distinct trend as the concentration of tin oxide increased. The average optical transmission ranges from 33% to 65% in the visible region.  The maximum electrical conductivity of 1.13×102 (Ωcm)-1 was obtained in the film (ZnO)0.8 (SnO2)0.2.  Based on our findings, thin-film solar cells and touchpad control panels could benefit from (ZnO)1-x (SnO2)x composite films due to their enhanced electrical and optical properties.

Crossref
View Publication
Publication Date
Mon Jun 04 2018
Journal Name
Baghdad Science Journal
Effects of Non-Thermal Argon Plasma Produced at Atmospheric Pressure on the Optical Properties of CdO Thin Films
...Show More Authors

In this paper the effect of nonthermal atmospheric argon plasma on the optical properties of the cadmium oxide CdO thin films prepared by chemical spray pyrolysis was studied. The prepared films were exposed to different time intervals (0, 5, 10, 15, 20) min. For every sample, the transmittance, Absorbance, absorption coefficient, energy gap, extinction coefficient and dielectric constant were studied. It is found that the transmittance and the energy gap increased with exposure time, and absorption. Absorption coefficient, extinction coefficient, dielectric constant decreased with time of exposure to the argon plasma

View Publication Preview PDF
Scopus (29)
Crossref (17)
Scopus Clarivate Crossref
Publication Date
Tue Apr 05 2022
Journal Name
Nano Hybrids And Composites
Structural and Optical Properties of ZnO Nanostructures Synthesized by Hydrothermal Method at Different Conditions
...Show More Authors

ZnO nanostructures were synthesized by hydrothermal method at different temperatures and growth times. The effect of increasing the temperature on structural and optical properties of ZnO were analyzed and discussed. The prepared ZnO nanostructures were characterized by X-ray diffraction (XRD), UV–Vis. absorption spectroscopy (UV–Vis.), Photoluminescence (PL), and scanning electron microscopy (SEM). In this work, hexagonal crystal structure prepared ZnO nanostructures was observed using X-ray diffraction (XRD) and the average crystallite size equal 14.7 and 23.8 nm for samples synthesized at growth time 7 and 8 hours respectively. A nanotubes-shaped surface morphology was found using scanning electron microscopy (SEM). The optic

... Show More
View Publication
Crossref (4)
Clarivate Crossref
Publication Date
Tue Apr 05 2022
Journal Name
Nano Hybrids And Composites
Structural and Optical Properties of ZnO Nanostructures Synthesized by Hydrothermal Method at Different Conditions
...Show More Authors

Zinc oxide (ZnO) nanoparticles were synthesized using a modified hydrothermal approach at different reaction temperatures and growth times. Moreover, a thorough morphological, structural and optical investigation was demonstrated using scanning electron microscopy (SEM), x-ray diffraction (XRD), ultra-violate visible light spectroscopy (UV-Vis.), and photoluminescence (PL) techniques. Notably, SEM analysis revealed the occurrence of nanorods-shaped surface morphology with a wide range of length and diameter. Meanwhile, a hexagonal crystal structure of the ZnO nanoparticles was perceived using XRD analysis and crystallite size ranging from 14.7 to 23.8 nm at 7 and 8 ℎ𝑟𝑠., respectively. The prepared ZnO samples showed good abso

... Show More
Publication Date
Wed Jun 10 2026
Journal Name
Applied Physics A
Annealing-temperature-dependent structural, optical, and NO2 gas-sensing properties of Ag-doped NiO thin films prepared by dip coating
...Show More Authors

Ag-doped NiO thin films were fabricated by dip coating and subsequently annealed at 373, 473, 573, and 673 K to elucidate the influence of annealing temperature on their structural, morphological, optical, and NO2-sensing characteristics. X-ray diffraction confirmed the formation of polycrystalline Ag/NiO films, with progressively improved crystallinity and larger crystallite size at elevated annealing temperatures. Atomic force microscopy revealed a homogeneous surface morphology with grain growth, with the average grain diameter increasing from 26.40 to 34.2 nm. Optical analysis showed high visible-region transmittance (65–70%) and a gradual reduction in the optical band gap from 2.75 to 2.07 eV with increasing annealing temperature. Ga

... Show More
View Publication
Scopus (1)
Scopus Crossref
Publication Date
Tue Jan 08 2019
Journal Name
Iraqi Journal Of Physics
The structure and optical properties of organic semiconductor bulk hetrojunction blend (NiPcTs/Alq3) thin films
...Show More Authors

The effect of heat treatment on the optical properties of the bulk heterojunction blend nickel (II) phthalocyanine tetrasulfonic acid tetrasodium salt and Tris (8-hydroxyquinolinato) Aluminum (NiPcTs/Alq3) thin films which prepared by spin coating was described in this study. The films coated on a glass substrate with speed of 1500 rpm for 1.5 min and treated with different annealing temperature (373, 423 and 473) K. The samples characterized using UV-Vis, X ray diffraction and Fourier transform Infrared (FTIR) spectra, XRD patterns indicated the presence of amorphous and polycrystalline blend (NiPcTs/Alq3). The results of UV visible shows that the band gap increase with increasing the annealing temperature up to 373 K and decreases with

... Show More
View Publication Preview PDF
Crossref
Publication Date
Tue Jan 01 2019
Journal Name
Energy Procedia
Synthesis and study of some physical properties of cadmium oxide CdO thin films
...Show More Authors

View Publication
Publication Date
Thu Dec 01 2011
Journal Name
Iraqi Journal Of Physics
Structural and D.C. conductivity investigation of the ternary alloy System a-AlXGa1-x As:H films prepared by new deposition method
...Show More Authors

In this paper Alx Ga1-x As:H films have been prepared by using new deposition method based on combination of flash- thermal evaporation technique. The thickness of our samples was about 300nm. The Al concentration was altered within the 0 x 40.
The results of X- ray diffraction analysis (XRD) confirmed the amorphous structure of all AlXGa1-x As:H films with x  40 and annealing temperature (Ta)<200°C. the temperature dependence of the DC conductivity GDC with various Al content has been measured for AlXGa1-x As:H films.
We have found that the thermal activation energy Ea depends of Al content and Ta, thus the value of Ea were approximately equal to half the value of optical gap.

View Publication Preview PDF
Publication Date
Sun Dec 01 2002
Journal Name
Iraqi Journal Of Physics
Preparation of thin films of SiCN from gas-phase reaction induced by TEA-CO2 laser and study of their optical properties
...Show More Authors

In this paper, silicon carbonitried thin films were prepared by the method of photolysis of the silane (SiH4) and ethylene (C2H4) gases, with and without ammonia gas (NH3), which is represented by the ratio between the (PNH3) and (PSiH4 + PC2H4 + PNH3), (which assign by the letter X), X has the values (0, 0.13, 0.33). This method carried out by using TEA-CO2 laser, on glass substrate at (375 oC), deposition rate (0.416-0.833) nm/pulse thin film thickness of (500-1000) nm. The optical properties of the films were studied by using Absorbance and Transmittance spectrums in wavelength range of (400-1100) nm, the results showed that the electronic transitions is indirect and the energy gap for the SiCN films increase with increasing of nitrog

... Show More
View Publication Preview PDF
Publication Date
Thu Oct 14 2021
Journal Name
Iraqi Journal Of Physics
Investigation of nonlinear optical properties for laser dyes-doped polymer thin film
...Show More Authors

Solutions of dyes Rhodamine 6G (Rh6G) and Coumarin480(C480) were prepared at five concentrations (1x10-3, 5x10-4, 1x10-4, 5x10-5 and1x10-5) mol/l, the mixing was stirred to obtain on a homogenous solution, the(poly methyl-methacrylate) (PMMA) was solved by chloroform solvent with certain ratio, afterward (PMMA+Rh6G) and (PMMA+C480) thin films were prepared by casting method on glass block which has substrate with dimensions (7.5 x2.5)cm2, the prepared samples were left in dark place at room temperature for 24 hours to obtain uniform and homogenous thin films. UV-VIS absorption spectra, transmission spectra and fluorescence spectra were done to measure linear refractive index and linear absorption coefficient. The nonlinear optical proper

... Show More
View Publication Preview PDF
Publication Date
Sat Aug 31 2019
Journal Name
Iraqi Journal Of Physics
Manufacturing Zener diode using ZnO-CuO-ZnO/Si structures deposited laser induced plasma technique
...Show More Authors

        In this paper Zener diode was manufactured using ZnO-CuO-ZnO/Si heterojunction structure that used laser induced plasma technique to prepare the nanofilms. Six samples were prepared with a different number of laser pulses, started with 200 to 600 pulses on ZnO tablet with fixed the number of laser pulses on CuO tablet at 300 pulses. The pulse energy of laser deposited was 900mJ using ZnO tablet and 600mJ using CuO tablet. All prepared films shown good behavior as Zener diode when using porous silicon as substrate.

View Publication Preview PDF
Crossref (2)
Crossref