This research examines the electrical, optical, and structural properties of zinc oxide (ZnO) and tin(IV) oxide (ZnO)1-x (SnO2)x composite thin films made by pulsed laser deposition, as well as the impact of composition concentration. The structural study of (ZnO)1-x (SnO2)x composites and thin films was conducted by X-ray analysis (XRD). Optical properties were investigated by UV–Vis infrared spectroscopy. The structural analysis revealed that all prepared thin-film composites were polycrystalline, exhibiting both hexagonal wurtzite and tetragonal phases for pure ZnO and SnO2, as well as a mixture of both phases for x=0.2 and 0.4. In contrast, the SnO2 phase was predominant for x=0.6 and 0.8. The increase in crystal size in the (ZnO)1-x (SnO2)x composite thin films was observed at x = 0.4 and 1.0. The optical band gap of (ZnO)1-x (SnO2)x composites exhibited a distinct trend as the concentration of tin oxide increased. The average optical transmission ranges from 33% to 65% in the visible region. The maximum electrical conductivity of 1.13×102 (Ωcm)-1 was obtained in the film (ZnO)0.8 (SnO2)0.2. Based on our findings, thin-film solar cells and touchpad control panels could benefit from (ZnO)1-x (SnO2)x composite films due to their enhanced electrical and optical properties.
(Sb2S3)1-xSnx thin films with different concentrations (0, 0.05 and
0.15) and thicknesses (300,500 and 700nm) have been deposited by
single source vacuum thermal evaporation onto glass substrates at
ambient temperature to study the effect of tin content, thickness and
on its structural morphology, and electrical properties. AFM study
revealed that microstructure parameters such as crystallite size, and
roughness found to depend upon deposition conditions. The DC
conductivity of the vacuum evaporated (Sb2S3)1-x Snx thin films was
measured in the temperature range (293-473)K and was found to
increase on order of magnitude with
This work compares the changes in optical and structural properties of cerium oxide (CeO2) when doped with different concentrations (3%,5%,7%, and 9%) of two oxides, In2O3 and Eu2O3. X-ray diffraction and spectrophotometry were employed in the visible, ultraviolet, and near-infrared regions. The findings demonstrated that CeO2 doped with In2O3 and Eu2O3 thin films were polycrystalline and had a cubic structure. The crystal size increased from 20.5 to 32.15 when Eu2O3 doping ratio increased from 0% to 7% and then decreased to 28.46 nm at 9%. While the crystal size showed an increase from 20.5 to 21.42 nm with the increase of the In2O3 doping ratio, while the lattice constant measured for cubic CeO2 changed opposite to that
... Show MoreIt is shown that pure and 3% boron doped a-Si0.1Ge0.9:H and a-Si0.1Ge0.9:N thin films
could be prepared by flash evaporation processes. The hydrogenation and nitrogenation
are very successful in situ after depositing the films. The FT-IR analysis gave all the
known absorbing bonds of hydrogen and nitrogen with Si and Ge.
Our data showed a considerable effect of annealing temperature on the structural and
optical properties of the prepared films. The optical energy gap (Eopt.) of a-Si0.1Ge0.9
samples showed to have significant increase with annealing temperature (Ta) also the
refractive index and the real part of dielectric constant increases with Ta, however the
extinction coefficient and imaginary part of dielect
Tin dioxide doped silver oxide thin films with different x content (0, 0.03, 0.05, 0.07) have been prepared by pulse laser deposition technique (PLD) at room temperatures (RT). The effect of doping concentration on the structural and electrical properties of the films were studied. Atomic Force Measurement (AFM) measurements found that the average value of grain size for all films at RT decrease with increasing of AgO content. While an average roughness values increase with increasing x content. The electrical properties of these films were studied with different x content. The D.C conductivity for all films increases with increasing x content. Also, it found that activation energies decrease with increasing of AgO content for all films.
... Show MoreThe largest use of x-ray in medical by dentists, employers or persons that needed by patients with specific conditions, lead to higher exposure of x-ray that may cause many diseases. In the present work radiography films have been used in evaluating the efficiency of using unsaturated polyester polymer reinforced with lead oxide (PbO) as shield material for medical x-ray devices, many parameters studied like concentration and thickness that they are increasing the attenuation of x-ray in them. The results show that the attenuation of X-ray increasing with concentration of reinforced material and with thickness, and the optical density decreases with increasing concentration from 0% to 50%, we chose 30% as suitable concentration to increase
... Show MoreChalcogenide glasses SeTe have been prepared from the high purity constituent elements .Thin films of SeTe compound have been deposited by thermal evaporation onto glass substrates for different values of film thickness . The effect of varying thickness on the value of the optical gap is reported . The resultant films were in amorphous nature . The transmittance spectra was measured for that films in the wavelength range (400-1100) nm . The energy gap for such films was determined .
InSb alloy was prepared then InSb:Bi films have been prepared successfully by thermal evaporation technique on glass substrate at Ts=423K. The variation of activation energies(Ea1,Ea2)of d.c conductivity with annealing temperature (303, 373, 423, 473, 523 and 573)K were measured, it is found that its values increases with increasing annealing temperature. To show the type of the films, the Hall and thermoelectric power were measured. The activation energy of the thermoelectric power is much smaller than for d.c conductivity and increases with increasing annealing temperature .The mobility and carrier concentration has been measured also.
CuInSe2(CIS) thin films have been prepared by use vacuum thermal evaporation technique, of thickness750 nm with rate of deposition 1.8±0.1 nm/sec on glass substrate at room temperature and pressure (10-5) mbar. Heat treatment has been carried out in the range (400-600) K for all samples. The optical properties of the CIS thin films are been studied such as (absorption coefficient, refractive index, extinction coefficient, real and imaginary dielectric constant) by determined using Measurement absorption and transmission spectra. Results showed that through the optical constants we can make to control it are wide applications as an optoelectronic devices and photovoltaic applications.