Determination of threshold random gain medium in dye: Polymer films containing TiO<sub>2</sub> nanoparticles
...Show More Authors

Crossref
View Publication
Publication Date
Tue May 01 2012
Journal Name
Iraqi Journal Of Physics
Studying the optical properties of ( Cr2O3:I ) thin films prepared by spray pyrolysis technique
...Show More Authors

Undoped and Iodine (I)–doped chrome oxide (Cr2O3)thin films have been prepared by chemical spray pyrolysis technique at substrate temperatures(773K) on glass substrate. Absorbance and transmittance spectra have been recorded as a function of wavelength in the range (340-800 nm) in order to study the optical properties such as reflectance, Energy gap of allowed direct transition, extinction coefficient refractive index, and dielectric constant in real and imagery parts all as a function of wavelength. It was found that all the investigated parameters affect by the doping ratios.

View Publication Preview PDF
Publication Date
Sun Feb 24 2019
Journal Name
Iraqi Journal Of Physics
Laser energy effect on the properties of ZnS thin films prepared by PLD technique
...Show More Authors

Zinc sulfide (ZnS) thin films were deposited on glass substrates using pulsed laser deposition technique. The laser used is the Q-switched Nd: YAG laser with 1064nm wavelength and 1Hz pulse repetition rate and varying laser energy 700mJ-1000mJ with 25 pulse. The substrate temperature was kept constant at 100°C. The structural, morphological and optical properties of ZnS thin films were characterized with X-ray diffraction (XRD), scanning electron microscopy (SEM), atomic force microscope (AFM) and UV-VIS spectrophotometer.

View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Wed May 29 2019
Journal Name
Iraqi Journal Of Physics
Synthesis and characterization of Iron tungstate oxide films by advanced controlled spray pyrolysis technique
...Show More Authors

For the first time Iron tungstate semiconductor oxides films (FeWO4) was successfully synthesized simply by advanced controlled chemical spray pyrolysis technique, via employed double nozzle instead of single nozzle using tungstic acid and iron nitrate solutions at three different compositions and spray separately at same time on heated silicone (n-type) substrate at 600 °C, followed by annealing treatment for one hour at 500 °C. The crystal structure, microstructure and morphology properties of prepared films were studied by X-ray diffraction analysis (XRD), electron Scanning Electron Microscopy (SEM) and Atomic Force Microscopy (AFM) respectively. According to characterization techniques, a material of well-crystallized monoclinic ph

... Show More
View Publication Preview PDF
Crossref
Publication Date
Fri Dec 29 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Structure and Optical Properties of BhSe3 Thin Films Prepared by Chemical Bath Deposition Method
...Show More Authors

Thin films of  BhSe3  have being deposited on glass substrates of

about 80 - 172 ± 14 nm thickness from an aqueous solution bath at temperature 293 K for period 0.5 to 6.0 hours  using alchemical bath deposition method .

The  films  are  characterized   by  X-ray  diffraction,     X-ray

florescent techniques and optical transmittance spectra measurements in the rang 350 - 400 nm at 293 K. And shows that as deposited  films are amorphous and a  transition to polycrystalline state has taken place after  annealing  them  at  373  K,  for  30  minutes,  But  they  will  be dan1aged

... Show More
View Publication Preview PDF
Publication Date
Wed Jul 17 2019
Journal Name
Aip Conference Proceedings
Annealing effect on characterization of nano crystalline SnSe thin films prepared by thermal evaporation
...Show More Authors

Tin Selenide (SnSe) Nano crystalline thin films of thickness 400±20 nm were deposited on glass substrate by thermal evaporation technique at R.T under a vacuum of ∼ 2 × 10− 5 mbar to study the effect of annealing temperatures (as-deposited, 100, 150 and 200) °C on its structural, surface morphology and optical properties. The films structure was characterized using X-ray diffraction (XRD) which showed that all the films have polycrystalline in nature and orthorhombic structure, with the preferred orientation along the (111) plane. These films was synthesized of very fine crystallites size of (14.8-24.5) nm, the effect of annealing temperatures on the cell parameters, crystallite size and dislocation density were observed.

... Show More
View Publication Preview PDF
Scopus (10)
Crossref (10)
Scopus Clarivate Crossref
Publication Date
Sun Mar 17 2019
Journal Name
Baghdad Science Journal
Enhancement of Hydrothermally Co3O4 Thin Films as H2S Gas Sensor by Loading Yttrium Element
...Show More Authors

The gas sensing properties of Co3O4 and Co3O4:Y nano structures were investigated. The films were synthesized using the hydrothermal method on a seeded layer. The XRD, SEM analysis and gas sensing properties were investigated for Co3O4 and Co3O4:Y thin films. XRD analysis shows that all films are polycrystalline in nature, having a cubic structure, and the crystallite size is (11.7)nm for cobalt oxide and (9.3)nm for the Co3O4:10%Y. The SEM analysis of thin films obviously indicates that Co3O4 possesses a nanosphere-like structure and a flower-like structure for Co3O4:Y.

The sen

... Show More
View Publication Preview PDF
Scopus (4)
Scopus Clarivate Crossref
Publication Date
Mon Aug 04 2014
Journal Name
Photonic Sensors
Crystalline structure and surface morphology of tin oxide films grown by DC reactive sputtering
...Show More Authors

View Publication
Scopus (9)
Crossref (6)
Scopus Crossref
Publication Date
Mon Dec 01 2014
Journal Name
Photonic Sensors
Crystalline Structure and Surface Morphology of Tin Oxide Films Grown by DC Reactive Sputtering
...Show More Authors

Abstract: Tin oxide thin films were deposited by direct current (DC) reactive sputtering at gas pressures of 0.015 mbar – 0.15 mbar. The crystalline structure and surface morphology of the prepared SnO2 films were introduced by X-ray diffraction (XRD) and atomic force microscopy (AFM). These films showed preferred orientation in the (110) plane. Due to AFM micrographs, the grain size increased non-uniformly as the working gas pressure increased.

Preview PDF
Publication Date
Wed Jun 01 2016
Journal Name
Chalcogenide Letters
Characterization, morphology and electrical properties of chemically deposited nanocrystalline PbS/Si heterojunction thin films
...Show More Authors

A nanocrystalline thin films of PbS with different thickness (400, 600)nm have been prepared successfully by chemical bath deposition technique on glass and Si substrates. The structure and morphology of these films were studied by X-ray diffraction and atomic force microscope. It shows that the structure is polycrystalline and the average crystallite size has been measured. The electrical properties of these films have been studied, it was observed that D.C conductivity at room temperature increases with the increase of thickness, From Hall measurements the conductivity for all samples of PbS films is p-type. Carrier's concentration, mobility and drift velocity increases with increasing of thickness. Also p-PbS/n-Si heterojunction has been

... Show More
Publication Date
Tue Feb 27 2018
Journal Name
Iraqi Journal Of Laser
Investigation of Densified SiO2 Sol-Gel Thin Films Using Conventional and DPSS Laser Techniques
...Show More Authors

The prepared nanostructure SiO2 thin films were densified by two techniques (conventional and Diode Pumped Solid State Laser (DPSS) (532 nm). X-ray diffraction (XRD), Field Emission Scanning electron microscopy (FESEM), and Atomic Force Microscope (AFM) technique were used to analyze the samples. XRD results showed that the structure of SiO2 thin films was amorphous for both Oven and Laser densification. FESEM and AFM images revealed that the shape of nano silica is spherical and the particle size is in nano range. The small particle size of SiO2 thin film densified by DPSS Laser was (26 nm) , while the smallest particle size of SiO2 thin film densified by Oven was (111 nm).

View Publication Preview PDF