This study evaluates the performance of magnetic abrasive finishing (MAF) of aluminum alloy in terms of achieving materials removal (MR). A vertical milling machine is used to perform the finishing process using a developed MAF unit that consists of an inductor made out of a 150 mm long and 20 mm diameter iron core wound with 1500 turns and 0.5 mm copper wire. The commutator and magnetic pole are attached at the top and bottom of the inductor, respectively. The required current is supplied using a DC power supply. The South Pole workpiece is a 100×50×3 mm3 plate of AA 1100 aluminum alloy, whereas the magnetic pole represented the North Pole. Pole rotational speed, applied current, and abrasive finishing time was selected as input parameters of the MAF with three-level of (270, 600. 930 rpm; 0.5, 1, 1.5 Amp; 6,9,12 min). The L9 orthogonal array of the Taguchi method was utilized to examine the impact of each independent input. The obtained results clarify that applied current was the most effective factor in terms of its contribution (63.16%) in the produced MR, followed by time finishing and rotational speed.
This research aims to find out the impact on the receptive style according to the specimen in the collection of material Brawner and retention as students at the Arabic Department at the Faculty of Education for Girls. For confirmation from the goal of the research, the researcher placed two hypotheses, one to two for collections and one for pods. - chosen as the College of Education for Girls / Department of Arabic language for the application of choice Intentionally search experience for reasons of researcher he is teaching them and thus ensures cooperation of teachers and students in them. - selected Division (b) of the fourth grade students of the Arabic language section at random to represent the experimental group, while the Division
... Show MoreAbstract: This paper presents the results of the structural and optical analysis of CdS thin films prepared by Spray of Pyrolysis (SP) technique. The deposited CdS films were characterized using spectrophotometer and the effect of Sulfide on the structural properties of the films was investigated through the analysis of X-ray diffraction pattern (XRD). The growth of crystal became stronger and more oriented as seen in the X-ray diffraction pattern. The studying of X-ray diffraction showed that; all the films have the hexagonal structure with lattice constants a=b=4.1358 and c=6.7156A°, the crystallite size of the CdS thin films increases and strain (ε) as well as the dislocation density (δ) decreases. Also, the optical properties of the
... Show MoreThe biggest problem of structural materials for fusion reactor is the damage caused by the fusion product neutrons to the structural material. If this problem is overcomed, an important milestone will be left behind in fusion energy. One of the important problems of the structural material is that nuclei forming the structural material interacting with fusion neutrons are transmuted to stable or radioactive nuclei via (n, x) (x; alpha, proton, gamma etc.) reactions. In particular, the concentration of helium gas in the structural material increases through deuteron- tritium (D-T) and (n, α) reactions, and this increase significantly changes the microstructure and the properties of the structural materials. T
... Show MoreBackground: Relapse of previously moved teeth, is major clinical problem in orthodontics with respect to the goals of successful treatment. This study investigated the effect of orthodontic relapse on the proliferation of fibroblast and epithelial rests of Malassez cells in periodontal ligament of rat molars. Materials and Methods: Sixteen ten-week- old male Wister rats were randomly divided into four groups composed of four animals each: Group I received no orthodontic force (control). In both Group II and Group III, uniform standardized expansive springs were used for moving the maxillary first molars buccally for periods of one and three weeks respectively. The spring initially generated an average expansive force of 20 g on each side.
... Show MoreThe paper presents an investigation to the flutter speed of composite wing for different ply orientation. Structurally the composite wing was idealized as a composite beam load carrying structure. Theodorsen’s expression was used to get the 2- dimension unsteady lifting force and pitching moment in the limit of incompressible flow and subsonic speed which were integrated over the wing span. A free vibration analysis was first carried out to get the natural frequencies and mode shapes .The velocity-damping (V-g) method was used to calculate the flutter speed and the flutter frequency. A wing of unmanned aerial vehicle was manufactured from woven glass and polyester resin where the flutter speed was calculated experimentally by the wind
... Show MorePortland cement is considered the most involved product in environmental pollution. It is responsible for about 10% of global CO2 emissions [1]. Limestone dust is a by-product of limestone plants and it is produced in thousands of tons annually as waste material. To fulfill sustainability requirements, concrete production is recommended to reduce Portland cement usage with the use of alternative or waste materials. The production of sustainable high strength concrete by using nanomaterials is one of the aims of this study. Limestone dust in 12, 16, and 20% by weight of cement replaced cement in this study. The study was divided into two parts: the first was devoted to the investigation of the best percentage of replacement of waste
... Show MoreThe present studies are focused on the modification of the properties of epoxy resin with different additives namely aluminum, copper by preparing of composites systems with percentage (20%, 40% and 50%) of the above additives. The experimental results show that the D.C of conductivity on wt% filler content at ( 293-413 ) K electrical conductivity of all above composites increased with temperature for composites with filler contact and find the excellent electrical conductivity of copper and lie between (2.6*10-10 - 2.1*10-10)?.cm . The activation energy of the electrical conductivity is determined and found to decrease with increasing the filler concentration.