This study involves adding nano materials and interaction with cement mortar behavior for several mortar samples under variable curing time with constant water to cement ratio (W/C = 0.5). The effects of adding nano materials on the microstructure of cement mortar were studied by (Scanning Electronic Microscopy (SEM) and X-Ray (for samples at different curing time 28 and 91 days. Small ratio replacements of nano particles (SiO2 or Al2O3) were added to Ordinary Portland Cement (OPC) type (I). The percentage of nano materials additives replacement by weight of ordinary Portland cement includes (1, 2, 3, 4 and 5%) for both types of nano materials with constant (W/C) ratio, also the amount of the fine aggregate used was three times the amount of cement. The results showed that, the mortar consist of both nano materials had better microstructure than mortar without nano materials in all test. Best enhancements in properties and microstructure for mortars with nano silica were achieved with (3%) additives while were achieved with nano alumina at (2%) additives.
أظهرت نتائج تقدير التركيب الكيميائي لمعزول بروتين بقول العدس المنبت التي تم الحصول عليها من الأسواق المحلية في محافظة بغداد وذلك باستخدام الاستخلاص القلوي عند الرقم الهيدروجيني 9.5 PH ثم الترسيب عند نقطة التعادل الكهربائي 4.5 PH،كانت نسبة البروتين، الرطوبة، الرماد، الألياف، الدهن والكربوهيدرات (71.58، 6.44، 2.58، 1.09، 0.25، 8.66) % على التوالي، وبينت نتائج تقدير المعادن في المعزول البروتيني لكل من الكالسيوم والفسفور والحد
... Show MoreAim: To evaluate the effect of ultrasonic agitation for retrograde biodceramic root repair, MTA and biodentine filling materials on push-out bond strength to dentine walls. Materials and Methods: Ninety extracted human teeth with single straight roots were selected randomly. After disinfection and cleaning, the coronal portions were sectioned to standardize the root canal length at 15mm. following root canal shaping, obturation and apical roots resection, retrograde cavities were prepared. Teeth were categorized depending on the filling material used into three groups, 30 teeth each. Group A filled with bioceramic root repair material, B with MTA and C with Biodentine material. These groups were divided in to three subgroup (n= 10). Subgrou
... Show MoreFailure in asphalt mixture and distress in pavement are major issues to roads infrastructure. Selecting an appropriate chemical composition of asphalt cement is a key component in avoiding these issues. This work aimed to investigate the effect of the chemical composition of different polar fractions on the rheological and physical properties of asphalt cement. Four types of asphalt cement with penetration grades of 20/30, 40/50, 60/70 and 85/100 were divided into four fractions. Complex shear modules, rutting resistance and rotational viscosity of the asphalt cement were determined by using a Dynamic Shear Rheometer and a Rotation Viscometer, respectively. The results show that an increase in the asphaltene content and Gastel index resulte
... Show MoreThis research studied the effect of magnetized water in concrete preparation and its effect on the presenting of cement in concrete mixtures also to find the ability of reducing the amount of cement in preparing one cubic meter, this is not exceed than 10% in one mixture , The experiments showed the preparation of standard cubes from the concrete which was used two kind of water magnetized water which was prepared by passing the tap water through the systems of different magnetic strength in terms of (6000,9000) Gauss and the ordinary water . The velocity of water through the magnetic field, which gives us the highest value for the compressive strength, was up to 1m/sec. to determine the best magnetic intensity, we examined The comp
... Show MoreSteel–concrete–steel (SCS) structural systems have economic and structural advantages over traditional reinforced concrete; thus, they have been widely used. The performance of concrete made from recycled rubber aggregate from scrap tires has been evaluated since the early 1990s. The use of rubberized concrete in structural construction remains necessary because of its high impact resistance, increases ductility, and produces a lightweight concrete; therefore, it adds such important properties to SCS members. In this research, the use of different concrete core materials in SCS was examined. Twelve SCS specimens were subjected to push-out monotonic loading for inspecting their mechanical performance. One specimen was constructed from co
... Show MoreThe research topic was chosen as a result of the importance of human resource in business organizations in general and the industrial process in particular. Without the human resource, business organizations cannot continue and achieve success and excellence, and the research problem has been diagnosed in the lack of sales of General Cement Company’s northern products, despite their distinctiveness, standing, and reputation in The market and its products with standard specifications, and through this problem, the following questions were raised: &nbs
... Show MoreBeryllium Zinc Oxide (BexZn1-xO) ternary nano thin films were deposited using the pulsed laser deposition (PLD) technique under a vacuum condition of 10-3 torr at room temperature on glass substrates with different films thicknesses, (300, 600 and 900 nm). UV-Vis spectra study found the optical band gap for Be0.2Zn0.8O to be (3.42, 3.51 and 3.65 eV) for the (300, 600 and 900nm) film thicknesses, respectively which is larger than the value of zinc oxide ZnO (3.36eV) and smaller than that of beryllium oxide BeO (10.6eV). While the X-ray diffraction (XRD) pattern analysis of ZnO, BeO and Be 0.2 Zn 0.8 O powder and nano-thin films indicated a hexa
... Show MoreHigh-volume traffic with ultra-heavy axle loads combined with extremely hot weather conditions increases the propagation of rutting in flexible pavement road networks. Several studies suggested using nanomaterials in asphalt modification to delay the deterioration of asphalt pavement. The current work aims to improve the resistance of hot mix asphalt (HMA) to rutting by incorporating Nano Silica (NS) in specific concentrations. NS was blended into asphalt mixtures in concentrations of 2, 4, and 6% by weight of the binder. The behavior of asphalt mixtures subjected to aging was investigated at different stages (short-term and long-term aging). The performance characteristics of the asphalt mixtures were evaluated using the Marshall s
... Show MoreMoisture damage is described as a reduction in stiffness and strength durability in asphalt mixtures due to moisture. This study investigated the influence of adding nano silica (NS) to the Asphalt on the moisture susceptibility of hot-mix-asphalt (HMA) mixtures under different aging conditions. NS was mixed with asphalt binder at concentrations of 2%, 4%, and 6% by weight of the binder. To detect the microstructure changes of modified Asphalt and estimate the dispersion of NS within the Asphalt, the field emission scanning electron microscope (FE-SEM) was used. To examine the performance of Asphalt mixed with NS at different aging stages (short-term and long-term aging), asphalt mixture tests such as Marshall stability,
... Show More