Preferred Language
Articles
/
alkej-314
Mechanical Properties of MIG Joints for Dissimilar Aluminum Alloys
...Show More Authors

The research aims to investigate the effects of GMAW or MIG welding process on the mechanical properties of dissimilar aluminum alloys 2024-T351 and AA 6061- T651. A series of experimental techniques have been conducted to evaluate mechanical properties of the alloys, by carrying out hardness, tensile and bending tests for welded and un-welded specimens.

Metal inert gas (MIG) has been carried out on sheet metal using ER- 4043(AlSi5) as a filler metal and argon as shielded gas. The welded joints were tested by X-ray radiography and Faulty pieces were excluded.

Welding joints without defects are subjected to heat treatment including heating the joints in furnace to 170 °C for half an hour then air cooling to relief welding stress.

Tensile test was implemented for all specimens which prepared in the dimensions according to ASTM 17500 by using Testing machine smart series with preload value 100 kN. Vickers hardness test and microstructure examination were made, the last test was bending test which implemented on the welded and un welded specimens which machined into standard test specimen dimensions.

Results of mechanical properties Using MIG welding process appear a general decay compared with un welded and in the dissimilar joint comparing with parent metal that is due to the microstructure change during the welding process. The location of the failure for welded specimens after all mechanical test was found predominantly along the heat affected zone ( HAZ ).but Unwedded specimens were failed near the center line of the specimen.  

View Publication Preview PDF
Quick Preview PDF
Publication Date
Fri Jun 01 2018
Journal Name
Journal Of Taibah University Medical Sciences
Effect of nano-titanium oxide addition on some mechanical properties of silicone elastomers for maxillofacial prostheses
...Show More Authors

Objective This study evaluated the effects of adding titanium oxide (TiO2) nanofillers on the tear strength, tensile strength, elongation percentage, and hardness of room-temperature-vulcanized (RTV) VST50F and high-temperature-vulcanized (HTV) Cosmesil M511 maxillofacial silicone elastomers. Methods Two types of maxillofacial elastomers, VST50F RTV and Cosmesil M511 HTV, were used. Nano-TiO2 powder was applied as a nanofiller. A total of 120 specimens were fabricated, 60 each of VST50F and Cosmesil M511. The specimens of each type of elastomer were divided into three equal groups on which tests were conducted for tear strength, tensile strength, and hardness i.e., 20 specimens were used for each test. Each group of 20 specimens was further

... Show More
View Publication
Scopus (24)
Crossref (8)
Scopus Clarivate Crossref
Publication Date
Wed Sep 01 2021
Journal Name
Iop Conference Series: Earth And Environmental Science
Influence of Temperature on Mechanical Properties of Asphalt Concrete Mixture
...Show More Authors

Asphalt binder is a thermoplastic material that conducts as an elastic solid at lower service temperatures or throughout fast loading rate. At a high temperature or slow rate of loading, asphalt binder conducts as a different liquid. The classical duplication generates a required to assess the mechanical properties of asphalt concrete at the anticipated service temperature to reduce the stress cracking, which happens at lower temperatures, fatigue, and the plastic deformation at higher temperatures (rutting). In this study, an achievement was made to assess the effect of temperature on the mechanical characteristics of asphalt concrete mixes. A total of 132 asphalt concrete samples were attended utilizing two asphalt cement grades (40-50) a

... Show More
Preview PDF
Scopus (1)
Scopus Crossref
Publication Date
Sun Feb 10 2019
Journal Name
Iraqi Journal Of Physics
Study of the mechanical properties of Iron-Epoxy composite materials
...Show More Authors

Iron-Epoxy composite samples were prepared by added
different weight percentages (0, 5, 10, 15, and 20 wt %) from Iron
particles in the range of (30-40μm) as a particle size. The contents
were mixed carefully, and placed a circular dies with a diameter of
2.5 cm. Different mechanical tests (Shore D Hardness, Tensile
strength, and Impact strength ) were carried out for all samples. The
samples were immersed in water for ten weeks, and after two weeks
the samples were take-out and drying to conducting all mechanical
tests were repeated for all samples. The hardness values increased
when the Iron particle concentration increased while the Impact
strength is not affected by the increasing of Iron particles
c

... Show More
View Publication Preview PDF
Crossref
Publication Date
Tue May 01 2018
Journal Name
Thin Solid Films
Thermo-mechanical properties of cubic lanthanide oxides
...Show More Authors

This contribution investigates the effect of the addition of the Hubbard U parameter on the electronic structural and mechanical properties of cubic (C-type) lanthanide sesquioxides (Ln2O3). Calculated Bader's charges confirm the ionic character of Lnsingle bondO bonds in the C-type Ln2O3. Estimated structural parameters (i.e., lattice constants) coincide with analogous experimental values. The calculated band gaps energies at the Ueff of 5 eV for these compounds exhibit a non-metallic character and Ueff of 6.5 eV reproduces the analogous experimental band gap of cerium sesquioxide Ce2O3. We have thoroughly investigated the effect of the O/Ce ratios and the effect of hafnium (Hf) and zirconium (Zr) dopants on the reduction energies of C

... Show More
View Publication
Scopus (13)
Crossref (11)
Scopus Clarivate Crossref
Publication Date
Wed Mar 10 2021
Journal Name
Baghdad Science Journal
Mechanical properties of epoxy-polyurethane polymer blends
...Show More Authors

Configured binary polymer blends of epoxy and Polyurethane was chosen varying proportions of these materials led to the production of homogeneous mixtures of Althermust Althermust and descent was poured polyurethane models required in the form of 4 mm thick plates

View Publication Preview PDF
Publication Date
Wed Jun 01 2022
Journal Name
Iraqi Journal Of Physics
Evaluation of Mechanical Properties for Epoxy reinforced with palm oil /Zinc oxide composites
...Show More Authors

In this research, the effect of reinforcing epoxy resin composites with a filler derived from chopped agriculture waste from oil palm (OP). Epoxy/OP composites were formed by dispersing (1, 3, 5, and 10 wt%) OP filler using a high-speed mechanical stirrer utilizing a hand lay-up method. The effect of adding zinc oxide (ZnO) nanoparticles, with an average size of 10-30 nm, with different wt% (1,2,3, and 5wt%) to the epoxy/oil palm composite,  on the behavior of an epoxy/oil palm composite was studied with different ratios (1,2,3, and 5wt%) and an average size of  10-30 nm.  Fourier Transform Infrared (FTIR) spectrometry and mechanical properties (tensile, impact, hardness, and wear rate) were used to examine the composites. The FTIR

... Show More
View Publication Preview PDF
Crossref (4)
Crossref
Publication Date
Mon Apr 24 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
Effect Of Additive Al On the Optical Properties Of Polystyrene-Aluminum Composites
...Show More Authors

 Additive aluminum powder to the polystyrene to prepare the composites Polystyrene– Aluminum.The samples were prepared by using mechanical  compressed method at low pressure and a temperature 120°C.         Measurements  of absorbance and reflectance spectra were carried out by UV-Visible  spectrophotometer , the effect of additive aluminum  on the optical band  gap Eop and  optical constants ( refractive index n, extinction coefficient k ,dielectric constant ε and optical conductivity σop)  were studied for the prepared composites .         Results showed a decrease in the Eop with increasing  perc

... Show More
View Publication Preview PDF
Publication Date
Fri Mar 01 2019
Journal Name
Al-khwarizmi Engineering Journal
Study the Factors Effecting on Welding Joint of Dissimilar Metals
...Show More Authors

The aim of this work is to study the factors that affect the welding joint of dissimilar metals. Austenitic stainless steel-type AISI (316L) with a thickness of (2mm) was welded to carbon steel (1mm) using an MIG spot welding.  The filler metal is a welding wire of the type E80S-G (according to AWS) is used with (1.2mm) diameter and CO2 is used as shielding gas with flow rate (7L/min) for all times was used in this work.

        The results indicate that the increase of the welding current tends to increase the size of spot weld, and also increases the sheer force.  Whereas the sheer force increased inversely with the time of welding. Furthermore, the results indicate that i

... Show More
View Publication Preview PDF
Publication Date
Tue Jun 12 2007
Journal Name
Iraqi Journal Of Laser
Nonlinear Optical Properties of CdS Thin Film Nanoparticles Using z-Scan Technique
...Show More Authors

In the present work, a z-scan technique was used to study the nonlinear optical properties, represented by the nonlinear refractive index and nonlinear absorption coefficients of nanoparticles cadmium sulfide thin film. The sample was prepared by the chemical bath deposition method. Several testing were done including, x-ray, transmission and thickness of thin film. z-Scan experiment was performed at two wavelengths (1064 nm and 532 nm) and different energies. The results showed the effect of self-focusing in the material at higher intensities, which evaluated n2 to be (0.11-0.16) cm2/GW. The effect of two-photon absorption was studied, which evaluated β to be (24-106) cm/GW. In addition, the optical limiting behavior has been studied.

... Show More
View Publication Preview PDF
Publication Date
Sat Jul 28 2018
Journal Name
Journal Of Engineering
Evaluation Microstructure and the Mechanical Properties of Composite Material for Al-Matrix Reinforced by Ceramic Materials (Sic And Al2O3)
...Show More Authors

In this investigation, the mechanical properties and microstructure of Metal Matrix Composites (MMCs) of Al.6061 alloy reinforced by ceramic materials SiC and Al2O3 with different additive percentages 2.5, 5, 7.5, and 10 wt.% for the particle size of 53 µm are studied. Metal matrix composites were prepared by stir casting using vortex technique and then treated thermally by solution heat treatment at 530 0C for 1 hr. and followed by aging at 175 0C with different periods. Mechanical tests were done for the samples before and after heat treatment, such as impact test, hardness test, and tensile test. Also, the microstructure of the metal matrix composites was examine

... Show More
View Publication Preview PDF
Crossref