Preferred Language
Articles
/
aOaqtZ4BmraWrQ4dU2Vh
Structural Strengthening of Insufficiently Designed Reinforced Concrete T-Beams using CFRP Composites
...Show More Authors

This study aims to compare the response of reinforced concrete (RC) T-beams strengthened with carbon fibre-reinforced polymer (CFRP) composite with that of non-strengthened control beams when subjected to monotonic two-point loading until failure for flexural once and shear again. The experimental programme tested eight RC T-beams, which included two reference beams without strengthening and six strengthened beams. The eight beams were divided into two main groups according to strengthening (flexural and shear). Experimental analysis was performed to study the effect of the CFRP laminate width in the flexural group and the spacing of CFRP U-wrap sheets in the shear group on the ultimate load capacity, load-strain relationship, and load-deflection relationship. Results show that increasing the width of the CFRP laminate in the flexural group improves the ultimate strengths to approximately 9.5%, 35%, and 41% for beams with CFRP laminate widths of 50, 100, and 150 mm, respectively, compared with the reference non-strengthened beam. The stiffness of the beams increases in direct proportion to the width of the CFRP laminate. In the meantime, decreasing the spacing of the CFRP laminate in the shear group increases the ultimate strengths to approximately 13.2%, 17.7%, and 23.5% for beams with CFRP U-wrap sheet spacings of 166, 125, and 100 mm, respectively, compared with the reference non-strengthened beam. Therefore, the spacing of the CFRP sheet is inversely proportional to the stiffness of the beam. Doi: 10.28991/CEJ-2023-09-08-05 Full Text: PDF

Crossref
View Publication
Publication Date
Sat Jul 01 2023
Journal Name
Journal Of Engineering
Effect of Heat Treatments and Carbon Content on the Damping Properties of Structural Steel
...Show More Authors

Low- and medium-carbon structural steel components face random vibration and dynamic loads (like earthquakes) in many applications. Thus a modification to improve their mechanical properties, essentially damping properties, is required. The present study focuses on improving and developing these properties, significantly dampening properties, without losing the other mechanical properties. The specimens used in the present study are structural steel ribbed bar ISO 6935 subjected to heating temperatures of (850, 950, and 1050) ˚C, and cooling schemes of annealing, normalizing, sand, and quenching was selected. The damping properties of the specimens were measured experimentally with the area under the curve for the loadi

... Show More
View Publication Preview PDF
Crossref (1)
Scopus Crossref
Publication Date
Fri Jun 26 2026
Journal Name
Journal Of Baghdad College Of Dentistry
X-ray diffraction and biocompatibility of glass ionomer cement reinforced by different ratios of synthetic hydroxyapatite
...Show More Authors

Background: This study was done to assist X-ray diffraction and biocompatability of glass ionomer cement reinforced by different ratios of Hydroxyapatite. Materials and Methods: The powder of glass ionomer cement reinforced by different ratios of Hydroxyapatite were used to get X-ray diffraction pattern by X-ray diffraction machine, While for biocompatibility test, A polyethylene tubes containing glass ionomer cement reinforced by different ratios of Hydroxyapatite were implanted on the dorsal submucosal site of Rabbit's tissues and histological slide were prepared for histopathological study. Results: X-ray diffraction test showed that all elements of glass ionomer cement reinforced by different ratios of Hydroxyapatite were react with eac

... Show More
View Publication Preview PDF
Publication Date
Sat Feb 12 2022
Journal Name
Engineering, Technology & Applied Science Research
The Effect of Different Curing Temperatures on the Properties of Geopolymer Reinforced with Micro Steel Fibers
...Show More Authors

In this study, geopolymer mortar was designed in various experimental combinations employing 1% micro steel fibers and was subjected to different temperatures, according to the prior works of other researchers. The geopolymer mortar was developed using a variety of sustainable material proportions (fly ash and slag) to examine the influence of fibers on its strength. The fly ash weight percentage was 50%, 60%, and 70% by slag weight to study its effect on the geopolymer mortar's properties. The optimal ratio produced the most significant results when mixed at a 50:50 ratio of fly ash and slag with 1% micro steel fibers at curing temperature 240oC for 4 hours through two days. The compressive strength of the geopolymer mortar increas

... Show More
View Publication
Crossref (12)
Crossref
Publication Date
Fri Jul 21 2023
Journal Name
Journal Of Engineering
Effect of Fire Flame (High Temperature) on the Behaviour of Axially loaded Reinforced SCC Short Columns
...Show More Authors

Experimental research was carried out to investigate the effect of fire flame (high temperature) on specimens of short columns manufactured using SCC (Self compacted concrete). To simulate the real practical fire disasters, the specimens were exposed to high
temperature flame, using furnace manufactured for this purpose. The column specimens were cooled in two ways. In the first the specimens were left in the air and suddenly cooled using water, after that the specimens were loaded to study the effect of degree of
temperature, steel reinforcement ratio and cooling rate, on the load carrying capacity of the reinforced concrete column specimens. The results will be compared with behaviour of columns without burning (control specime

... Show More
View Publication Preview PDF
Crossref (5)
Crossref
Publication Date
Mon Oct 01 2018
Journal Name
Journal Of Engineering
Performance of Self-Compacting Concrete Slab with Grinded Local Rocks
...Show More Authors

The effect of using grinded rocks of (quartzite and porcelanite) as powder of (10 and 20) % replacement by weight of cement for self-compacting concrete slabs was investigated in this study. Five slabs with 15 concrete cubes were tested experimentally at 28 days to study the compressive strength, ultimate load, ultimate deflection, ductility, crack load and steel strain. The test results show that, the compressive strength improvement when replacement of local rock powder reached to (7.3, 4.22) % for (10 and 20) % quartzite powder and (11.3, 16.1) % for (10 and 20) % porcelanite powder, respectively compared to the reference specimen. The ultimate load percentage increase for slabs with (10 and 20) % rep

... Show More
View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Mon Dec 11 2017
Journal Name
The First Mohesr And Hced Iraqi Scholars Conference In Australasia
Creep Strain Development of Self-compacting Portland-Limestone Cement Concrete
...Show More Authors

Prediction of the structural response of reinforced concrete to the time-dependent, creep and shrinkage, volume changes is complex. Creep is usually determined by measuring the change, with time, in the strain of specimens subjected to a constant stress and stored under appropriate conditions. This paper brings into view the development of creep strain for four self-compacting concrete mixes: A40, AL40, B60 and BL60 (where 40 and 60 represent the compressive strength level at 28 days and L indicates to Portlandlimestone cement). Specimens were put under sustained load and exposed to controlled conditions in a creep chamber (ASTM C512). The test results showed that normal strength Portland-limestone mixes have yielded lower ultimate c

... Show More
Publication Date
Fri Jun 02 2017
Journal Name
Kufa Journal Of Engineering
COMPRESSIVE STRENGTH OF CONCRETE CONTAINING WATER ABSORPTION POLYMER BALLS (WAPB)
...Show More Authors

Water absorbent polymers (WAP) are new component in producing building materials. They provide internal curing which reduces autogenous cracking, eliminates autogenous shrinkage, mortar strength increased, enhance early age strength to withstand strain, improve the durability, introduce higher early age compressive strength, have higher performance and reduce the effect of insufficient external curing. This research used different percent of polymer balls to choose the percent that provides good development in compressive strength with time for both water and air curing. The water absorption polymer balls in this research have the ability to absorb water and after usage in concrete they spill out the water (internal curing) and shri

... Show More
Publication Date
Sat Oct 01 2011
Journal Name
Journal Of Engineering
EMBEDDED LENGTH OF STEEL BARS IN SELF COMPACTED CONCRETE (SCC)
...Show More Authors

Experimental research was carried out on eight reinforced concrete beams to study the embedded length of the longitudinal reinforcement. Six beams were casted using self compacted concrete, and the two other beams were casted using normal concrete. The test was carried out on beams subjected to two point loads. The strain and the slip of the main reinforcement have been measured by using grooves placed during casting the beams at certain places. The measured strain used to calculate the longitudinal stresses (bond stress) surrounding the bar reinforcement, The study was investigated the using of self compacted concrete SCC on the embedded length of reinforcing bars, and comparing the results with normal concrete. The test results show th

... Show More
View Publication Preview PDF
Crossref (1)
Crossref
Publication Date
Tue Dec 03 2019
Journal Name
Civil Engineering Journal
Moisture Susceptibility of Asphalt Concrete Pavement Modified by Nanoclay Additive
...Show More Authors

Durability of hot mix asphalt (HMA) against moisture damage is mostly related to asphalt-aggregate adhesion. The objective of this work is to find the effect of nanoclay with montmorillonite (MMT) on Marshall properties and moisture susceptibility of asphalt mixture. Two types of asphalt cement, AC(40-50) and AC(60-70) were modified with 2%, 4% and 6% of Iraqi nanoclay with montmorillonite. The Marshall properties, Tensile strength ratio(TSR) and Index of retained strength(ISR) were determined in this work. The total number of specimens was 216 and the optimum asphalt content was 4.91% and 5% for asphalt cement (40-50) and (60-70) respectively. The results showed that the modification of asphalt cement with MMT led to increase Marsh

... Show More
Scopus (20)
Crossref (15)
Scopus Clarivate Crossref
Publication Date
Tue Apr 07 2009
Journal Name
The 6th Engineering Conference
Bond-Slip Relationship of Reinforcing Steel Bars Embedded in Concrete
...Show More Authors

An experimental investigation based on thirty three simple pullout cylinder specimens was conducted to study the bond-slip trend between concrete and steel reinforcement. Plain and deformed steel reinforcement bars were used in this investigation. The effect of bar diameter, concrete compressive strength and development length on bond-slip relation was detected. The results showed that the bond strength increases with increasing of compressive strength and with decreasing of bar diameter and development length. A nonlinear regression analysis for the experimental results yields in a mathematical correlation to predict the bond strength as a function of concrete compressive strength, reinforcing bar diameter and its yield stress. The minimum