1-[4-(2-Hydroxy-4, 6-dimethyl-phenylazo)-phenol]-ethanone (HL1) and 2-(4-methoxy-phenylazo)-3, 5- dimethyl-phenol (HL2) were produced by combination the diazonium salts of amines with 3, 5- dimethylphenol. The geometry of azo compounds was resolved on the basis of (C.H.N) analyses, 1H and 13CNMR, FT-IR and UV-Vis spectroscopic mechanisms. Complexes of La (III) and Rh (III) have been performed and depicted. The formation of complexes has been identified by using elemental analysis, FTIR and UV-Vis spectroscopic process as well, conductivity molar quantifications. Nature of complexes produced have been studied obeyed mole ratio and continuous alteration ways, Beer's law followed through a concentration scope (1×10-4 - 3×10-4 M). High molar absorbtivity from the compound solutions were noticed. Analytical data showed that all the complexes offered 1:3 metal-ligand ratios. In the radix from physicochemical datum an octahedral structure was described of the complexes. Biological activity of these compounds was assayed. Other than, the dyeing carried out of the produced compounds was practical in cotton fabric. The dyes were checked into light and detergent firmness.
In this research, Schiff bases derived from the reaction of anthrone with different heterocyclic amines have been described. The resulted Schiff base compounds were reacted with various nucleophiles in order to obtain new heterocyclic derivatives. Chemical structures of all products were confirmed by IR, 1H-, 13C-NMR spectral data and elemental analysis. All synthesized compounds were in vitro tested against a standard strain of pathogenic microorganism including Gram +ve bacteria (Staphylococcus aureus), Gram –ve bacteria (Escherichia coli), and fungi (Candida albicans).
The study was conducted during spring seasons of 2000 and 2001.The aim was to study the changes in the moisture content of sunflower plants during growth stages under hardening conditions to drought tolerance .Agricultural practices were made according to recommendation. Asplit-split plots design was used with three replications. The main plots included irrigation treatments:irrigation to100%(full irrigation),75and50%of available water. The sub plots were the cultivars Euroflor and Flame.The sub-sub plots represented four seed soaking treatments: Control (unsoaked), soaking in water ,Paclobutrazol solution(250ppm),and Pix solution(500ppm). The soaking continued for 24 hours then seeds were dried at room temperature until they regained t
... Show MoreThis study includes using green or biosynthesis-friendly technology, which is effective in terms of low cost and low time and energy to prepare V2O5NPs nanoparticles from vanadium sulfate VSO4.H2O using aqueous extract of Punica Granatum at a concentration of 0.1M and with a basic medium PH= 8-12. The V2O5NPs nanoparticles were diagnosed using several techniques, such as FT-IR, UV-visible with energy gap Eg = 3.734eV, and the X-Ray diffraction XRD was calculated using the Debye Scherrer equation. It was discovered to be 34.39nm, Scanning Electron Microscope (SEM), Transmission Electron Microscopy TEM. The size, structure, and composition of synthetic V2O5NPs were determined using the (EDX) pattern, Atomic force microscopy AFM. The a
... Show MoreThis study includes using green or biosynthesis-friendly technology, which is effective in terms of low cost and low time and energy to prepare V2O5NPs nanoparticles from vanadium sulfate VSO4.H2O using aqueous extract of Punica Granatum at a concentration of 0.1M and with a basic medium PH= 8-12. The V2O5NPs nanoparticles were diagnosed using several techniques, such as FT-IR, UV-visible with energy gap Eg = 3.734eV, and the X-Ray diffraction XRD was calculated using the Debye Scherrer equation. It was discovered to be 34.39nm, Scanning Electron Microscope (SEM), Transmission Electron Microscopy TEM. The size, structure, and composition of synthetic V2O5
... Show MoreManganese sulfate and Punica granatum plant extract were used to create MnO2 nanoparticles, which were then characterized using techniques like Fourier transform infrared spectroscopy, ultraviolet-visible spectroscopy, atomic force microscopy, X-ray diffraction, transmission electron microscopy, scanning electron microscopy, and energy-dispersive X-ray spectroscopy. The crystal's size was calculated to be 30.94nm by employing the Debye Scherrer equation in X-ray diffraction. MnO2 NPs were shown to be effective in adsorbing M(II) = Co, Ni, and Cu ions, proving that all three metal ions may be removed from water in one go. Ni(II) has a higher adsorption rate throughout the board. Co, Ni, and Cu ion removal efficiencie
... Show MoreManganese sulfate and Punica granatum plant extract were used to create MnO2 nanoparticles, which were then characterized using techniques like Fourier transform infrared spectroscopy, ultraviolet-visible spectroscopy, atomic force microscopy, X-ray diffraction, transmission electron microscopy, scanning electron microscopy, and energy-dispersive X-ray spectroscopy. The crystal's size was calculated to be 30.94nm by employing the Debye Scherrer equation in X-ray diffraction. MnO2 NPs were shown to be effective in adsorbing M(II) = Co, Ni, and Cu ions, proving that all three metal ions may be removed from water in one go. Ni(II) has a higher adsorption rate throughout the board. Co, Ni, and Cu ion removal efficiencies were 32.79%, 75
... Show MoreThe study involves removing of [Alizarin Red S (ARS) and Alizarin yellow R (AYR)] by using Iraqi Siliceous Rocks Powder (SRP). Adsorption isotherms were studied and the factors which influence it, such as temperature and salt effect. Adsorption isotherms of (ARS) were found to be comparable to Temkin equation. Adsorption isotherms of (AYR) were found to be comparable to Freundlich equation. The adsorption process on this surface was studied at different temperatures. The results showed that the adsorption of (ARS,AYR) on surface increased with increasing temperature (Endothermic process). According to the above results the thermodynamic functions (ΔH, ΔG, ΔS) were calculated. The adsorption quantity increasing for (ARS, AYR) with increas
... Show MoreThe present study aimed to synthesize selenium nanoparticles (SeNPs) using aqueous extract of black currant as a reducing agent. The green synthesized black currant selenium nanoparticles (BCSeNPs) were identified by color change. The characterization of SeNPs was achieved by Ultraviolet-visible (UV–VIS) spectroscopy, scanning electron microscopy (SEM), X–ray diffraction analysis (XRD), and Fourier transform infrared spectroscopy (FTIR). These tests were used to detect: stability, morphology, size, crystalline nature, and functional groups present on the surface of BCSeNPs. The results revealed appearance of the brick-red color indicating the specific color of selenium nanoparticles, and UV-Vis spectroscopy showed band absorbanc
... Show MoreIn the present work, 9-fluorenone-2-carboxylic acid methyl ester (1) was prepared from 9-fluorenone-2-carboxylic acid and then converted into the acid hydrazide (2). Compound (2), is the key intermediate for the synthesis of several series of new compounds such as substituted 1,3,4-oxadiazole derivatives (3-6) were synthesized from the condensation of different substituted benzoic acids with compound (2) using POCl3 as condensing agent. Treatment of compound (2) with formic acid gave the N-formyl hydrazide (7), which upon refluxing with phosphorous pentoxide in benzene yielded the corresponding 5-(9-fluorenone-2-yl)-1,3,4-oxadiazole (8). Reaction of hydrazide (2) with phenyl isocyanate to give N-phenyl semicarbazide derivative (9), then thi
... Show MoreCarbon nanospheres (CNSs) were successfully prepared and synthesized by Catalytic Chemical Vapor Deposition (CCVD) by using camphor as carbon source only, over iron Cobalt (Fe-Co) saturated zeolite at temperature between (700 oC and 900 °C), with different concentrations of camphor, and reaction time. The synthesized CNSs were characterized using Scanning Electron Microscopy (SEM), X-ray diffraction spectroscopy (XRD), and Fourier Transform Infrared (FTIR). The carbon spheres in different sizes between 100 nm and 1000 nm were investigated. This work has done by two parts, first preparation of the metallic catalyst and second part formation CNSs by heat treatment.