Background: Polymethyl methacrylate (PMMA) resin is extensively utilized in prosthodontics and orthodontics, particularly in fabricating artificial teeth, provisional crowns, denture bases, and orthodontic retainers. Aims: This study aimed to evaluate the effects of incorporating cerium oxide and polyether ether ketone nanoparticle (CP) composite into PMMA resin on transverse strength, impact strength, surface hardness, and denture base adaptation. Materials and Methods: A total of 120 PMMA specimens were divided into three groups based on the concentration of CP composite added to PMMA resin, with each group consisting of 40 specimens: a control group without fillers, group (A) containing 1% wt. of composite filler with a ratio of 30% cerium oxide and 70% polyether ether ketone, and group (B) comprising 3% wt. of composite with a ratio of 50% ceria, and 50% polyether ether ketone, as determined by the pilot study. Each group was tested for transverse strength, impact strength, surface hardness, and denture base adaptation, with 10 specimens for each test. The tested specimens were examined using Fourier transform infrared spectroscopy (FTIR), and field emission scanning electron microscopy (FE–SEM). The resulting data were statistically analyzed using SPSS at a significance level of P≤0.05. Results: Group B showed a significant statistical increase in transverse and impact strength compared with the other groups. Surface hardness and denture adaptation increased significantly in group A. FTIR analysis revealed transmission peaks and heightened intensity after the addition of the CP composite into the PMMA. The FE–SEM images showed a well-distributed nano CP composite within the PMMA matrix for all experimental groups, with increased agglomeration observed in group B (3%). Conclusion: The incorporation of 3% wt. CP into PMMA resin significantly improved transverse and impact strength compared with 1% wt. and the control. The surface hardness and denture base adaptation improved when 1% wt. CP was incorporated into the PMMA resin compared with the other tested groups.
Background: Poly (methyl methacrylate) has several disadvantages (poor mechanical properties) like impact and transverse strength. In order to overcome these disadvantages, several methods were used to strengthen the acrylic resin by using different fibers or fillers. This study was conducted to evaluate the effect of Plasma treatment of the fiber on mechanical properties Poly (methyl methacrylate) denture base material. Materials and methods: Specimens were prepared from poly methyl metha acrylic (PMMA) divided according to present of fiber into 4 groups (first group without fiber as control group, second group with Plasma treated polyester fibers, third group with Plasma treated polyamide fibers and fourth group Plasma treated combination
... Show MoreSludge from stone-cutting (SSC) factories and stone mines cannot be used as decorative stones, stone powder, etc. These substances are left in the environment and cause environmental problems. This study aim is to produce artificial stone composite (ASC) using sludge from stone cutting factories, cement, unsaturated resin, water, silicon carbide nanoparticles (SiC-NPs), and nano-graphene oxide (NGO) as fillers. Nano graphene oxide has a hydrophobic plate structure that water is not absorbed due to the lack of surface tension on these plates. NGO has a significant effect on the properties of artificial stone due to its high specific surface area and low density in the composite. Its uniform distribution in ASC is very low due to its hydropho
... Show MoreBackground: The mechanical properties of 3D-printed denture base resins are crucial factors for determining the quality and performance of dentures inside a patient’s mouth. Tensile strength and diametral compressive strength are two properties that could play significant roles in assessing the suitability of a material. Although they measure different aspects of material behavior, a conceptual link exists between them in terms of overall material strength and resilience. Aim: This study aims to investigate the correlation between tensile strength and diametral compressive strength after incorporating 2% ZrO2 nanoparticles (NPs) by weight into 3D-printed denture base resin. Methods: A total of 40 specimens (20 dumbbell-shaped and
... Show MoreThe dielectric properties of epoxy/palm oil fiber composites at different concentrations 1,3,5, and 10% by weight, and frequency ranging from 100 Hz to 1000kHz.Epoxy, zinc oxide and oil palm empty fruit bunch (OPEFB)fiber composites were prepared by hand –lay up into sheets. The effects of incorporated fibers on the electrical conductivity and thermal conductivity of the composites were investigated. The electrical conductivity of the composites decreased with increasing OPEFB fiber content. Despite the slight decrease in conductivity, the composites still sufficiently conductive relatively to applications such as sensors after the fiber addition, the thermal conductivity increased to 0.41
Objective This study evaluated the effects of adding titanium oxide (TiO2) nanofillers on the tear strength, tensile strength, elongation percentage, and hardness of room-temperature-vulcanized (RTV) VST50F and high-temperature-vulcanized (HTV) Cosmesil M511 maxillofacial silicone elastomers. Methods Two types of maxillofacial elastomers, VST50F RTV and Cosmesil M511 HTV, were used. Nano-TiO2 powder was applied as a nanofiller. A total of 120 specimens were fabricated, 60 each of VST50F and Cosmesil M511. The specimens of each type of elastomer were divided into three equal groups on which tests were conducted for tear strength, tensile strength, and hardness i.e., 20 specimens were used for each test. Each group of 20 specimens was further
... Show MoreABSTRACT Background: Improving the properties of heat- cured and self-cured acrylic resin have been studied by many researchers. However, little studies concerned with visible light cured resin (VLCR) improved through addition of nanofiller are available. The purpose of this study was to evaluate some properties of (VLCR) after addition of SiO2 nanofiller. Materials and Methods: SiO2 nanofiller were added to (VLCR) tray material after being dissolved in tetrahydrofuran (THF) solvent. According to the pilot study 2% SiO2 nanofiller addition exhibited better properties than the other percentages (1%, 3%). The main study conducted involved (100) specimens divided into 5 groups according to the test included. (20) Specimens were selecte
... Show MoreOverlapped have been prepared from epoxy resin material added to carbon Nanotube and percentages weight (0.1, 0.05, 0.01) % Studied the mechanical properties of the composite (bending, tensile an d hardness) has been found that the Flexural and tensile modulus of the composites were higher than the pure epoxy resin this may be due to the high mechanical strength of carbon nano tube (CNT). The hardness of the epoxy carbon Nanotube composites increased and the reason is due to increased overlap and stacking between the additives and material basis, which reduces the movement of polymer molecules leading to increased resistance to scratching material and cutting, will become more resistance to plastic deformation.
Objective Advantageous properties of silicone elastomer made it one of the favorable materials in maxillofacial prosthesis construction, but these properties may change after months of usage or after pigments addition. This study aimed to define the optimum concentration for a mixture of two types of intrinsic pigments that added to VST-50 maxillofacial silicone material and study their effects on mechanical properties before and after artificial aging. Methods After the pilot study was conducted, 0.1% by weight of rayon flocking and 0. 2% by weight of burnt sienna intrinsic pigment concentration was selected because of improvement in tested mechanical properties of VST-50 maxillofacial silicone. A total of one hundred and eighty samples we
... Show MoreInterest has largely centered on the use of plant fibers to reinforce plastics, because these fibers are abundant and cheap. Carrot fibers (Curran) have been extracted from carrot, left over from carrot juice manufacture. The fibers of two sizes fine (50<µm) and coarse (100-150 µm) have been mixed with epoxy in four levels of loading (10, 20, 30, 40 wt %) respectively. Impact test, shore d hardness test and three point bending test of epoxy and carrot fiber-epoxy composites samples have been determined. The impact strength values of samples prepared with fine and coarse fibers increased as compared with pure epoxy sample. Hardness values increased, and the Young’s modulus values decreased with fiber content of both sizes.