A low-cost, effective green porous composite was prepared and used for the sorption of Zn+2 ions from aqueous solutions. The effect of contact time, sorbent dosage, initial ion concentration, solution pH, and temperature on the sorption of Zn+2 ions was investigated. The results showed higher removal efficiency of Zn+2 ions (83%), which was achieved at a contact time of 120 minutes, a normal pH of 6.4, and a temperature of 313 K. The Langmuir isotherm model successfully described the experimental results of the sorption process with a theoretical maximum sorption capacity of 4.819 mg/g. The kinetics of sorption showed that the pseudo-second-order model fitted the experimental results better than the pseudo-first-order model. The intra-particle diffusion kinetics indicated that the boundary film was the rate-determining step of the sorption process. The thermodynamic parameters showed that the sorption of Zn+2 ions was spontaneous and endothermic under the studied conditions. The solidification of spent composite by kaolin was able to keep the leachate cations at an acceptable level in the solution after 12 weeks of exposure to a salty medium.
Antibiotics must be fully eliminated before they are released into the environment. In most cases, conventional wastewater treatment systems are not built to handle polar microcontaminants such as antibiotics. Oxytetracycline (OTC) is one of these antibiotics, an environmental hazard contaminant in aqueous solutions. Therefore, an advanced treatment method is needed for wastewater contaminated with antibiotics. In this study, we employed zinc oxide nanoparticles (ZnO), and the catalytic ozonation procedure was employed to increase the ozonation efficiency. A continuous experiment was carried out to compare the effectiveness of catalytic and single ozonation in degrading OTC in a continuous reactor. The flow rate of OTC solution, the initial
... Show MoreThe 17 α-ethinylestradiol (EE2) adsorption from aqueous solution was examined using a novel adsorbent made from rice husk powder coated with CuO nanoparticles (CRH). Advanced analyses of FTIR, XRD, SEM, and EDSwere used to identify the classification parameters of a CRH-like surface morphology, configuration, and functional groups. The rice husk was coated with CuO nanoparticles, allowing it to create large surface area materials with significantly improved textural qualities with regard to functional use and adsorption performance, according to a detailed characterization of the synthesized materials. The adsorption process was applied successfully with elimination effectiveness of 100% which can be kept up to 61.3%. The parameters of ads
... Show MoreThe cathodic deposition of zinc from simulated chloride wastewater was used to characterize the mass transport properties of a flow-by fixed bed electrochemical reactor composed of vertical stack of stainless steel nets, operated in batch-recycle mode. The electrochemical reactor employed potential value in such a way that the zinc reduction occurred under mass transport control. This potential was determined by hydrodynamic voltammetry using a borate/chloride solution as supporting electrolyte on stainless steel rotating disc electrode. The results indicate that mass transfer coefficient (Km) increases with increasing of flow rate (Q) where .The electrochemical reactor proved to be efficient in removing zinc and was abl
... Show MoreThe degradation of Toluidine Blue dye in aqueous solution under UV irradiation is investigated by using photo-Fenton oxidation (UV/H2O2/Fe+). The effect of initial dye concentration, initial ferrous ion concentration, pH, initial hydrogen peroxide dosage, and irradiation time are studied. It is found put that the removal rate increases as the initial concentration of H2O2 and ferrous ion increase to optimum value ,where in we get more than 99% removal efficiency of dye at pH = 4 when the [H2O2] = 500mg / L, [Fe + 2 = 150mg / L]. Complete degradation was achieved in the relatively short time of 75 minutes. Faster decolonization is achieved at low pH, with the optimal value at pH 4 .The concentrations of degradation dye are detected by spectr
... Show MoreIn this work magnetite/geopolymer composite (MGP) were synthesized using a chemical co-precipitation technique. The synthesized materials were characterized using several techniques such as: “X-ray diffraction (XRD), Fourier-transform infrared spectroscopy (FTIR), vibrating sample-magnetometer (VSM), field-emission scanning electron microscopy (FE-SEM), energy dispersive X-ray spectroscopy (EDS), Brunauer–Emmett–Teller (BET) and Barrentt-Joyner-Halenda (BJH)” to determine the structure and morphology of the obtained material. The analysis indicated that metal oxide predominantly appeared at the shape of the spinel structure of magnetite, and that the presence of nano-magnetite had a substantial impact on the surface area and pore st
... Show More