Hybrid architecture of ZnO nanorods/graphene oxide ZnO-NRs@GO synthesized by electrostatic self-assembly methods. The morphological, optical and luminescence characteristics of ZnO-NRs@GO and ZnO-NRs thin films have been described by FESEM, TEM, HRTEM, and AFM, which refers to graphene oxide have been coated ZnO-NRs with five layers. Here we synthesis ZnO-NRs@GO by simple, cheap and environmentally friendly method, which made it favorable for huge -scale preparation in many applications such as photocatalyst. ZnO-NRs@GO was applied as a photocatalyst Rodamin 6 G (R6G) dye from water using 532 nm diode laser-induced photocatalytic process. Overall degradation of R6G/ ZnO-NRs@GO was achieved after 90 minutes of laser irradiation while it needs more time for R6G alone. The reaction rate constant fit pseudo first order for R6G / ZnO-NRs@GO degradation was 0.41 min−1 compared to 0.015 min-1 using blank sample. The ZnO-NRs@GO thin film was considered as an excellent candidate to enhance the photocatalytic system.
The outstanding evidence of phthalimide pharmacophore in securing enhanced biological activities had encouraged further research and development into phthalimide-based derivatives as potential new drugs. In this study, phthalimide core was hybridized with aldehydes giving integrated imines displaying different types of functionalities and at alternating positions. The resulting compounds, therefore, provide an innovative window to explore possible differential biological effects as antioxidants and anticancer agents. A total of sixteen compounds were synthesized, and each was verified by FT-IR, H NMR, C NMR, and MS characterization. Herein, a facile single-step synthesis method was employed substituting the conventional two-step che
... Show MoreIn this work, nanostructure zinc sulfide (ZnS) thin films at temperature of substrate 450 oC and thickness (120) nm have been produced by chemical spray pyrolysis method. The X-Ray Diffraction (XRD) measurements of the film showed that they have a polycrystalline structure and possessed a hexagonal phase with strong crystalline orientation of (103). The grain size was measured using scanning electron microscope (SEM) which was approximately equal to 80 nm. The linear optical measurements showed that ZnS nanostructure has direct energy gap. Nonlinear optical properties experiments were performed using Q-switched 532 nm Nd:YAG laser Z-scan system. The nonlinear refractive index (n2) and nonlinear absorption coefficient (β) estimated for Z
... Show MoreCopper oxide thin films were deposited on glass substrate using Successive Ionic Layer Adsorption and Reaction (SILAR) method at room temperature. The thickness of the thin films was around 0.43?m.Copper oxide thin films were annealed in air at (200, 300 and 400°C for 45min.The film structure properties were characterized by x-ray diffraction (XRD). XRD patterns indicated the presence of polycrystalline CuO. The average grain size is calculated from the X-rays pattern, it is found that the grain size increased with increasing annealing temperature. Optical transmitter microscope (OTM) and atomic force microscope (AFM) was also used. Direct band gap values of 2.2 eV for an annealed sample and (2, 1.5, 1.4) eV at 200, 300,400oC respect
... Show MoreNano TiO2 thin films on glass substrates were prepared at a constant temperature of (373 K) and base vacuum (10-3 mbar), by pulsed laser deposition (PLD) using Nd:YAG laser at 1064 nm wavelength. The effects of different laser energies between (700-1000)mJ on the properties of TiO2 films was investigated. TiO2 thin films were characterized by X-ray diffraction (XRD) measurements have shown that the polycrystalline TiO2 prepared at laser energy 1000 mJ. Preparation also includes optical transmittance and absorption measurements as well as measuring the uniformity of the surface of these films. Optimum parameters have been identified for the growth of high-quality TiO2 films
... Show MoreNanocrystalline ZnO/Zeolite type A composite was prepared by simple method of operation by . the precipitation of zinc oxide and loading on zeolite 5A in one step. Characterization was made by X-ray diffraction (XRD), X-ray fluorescence(XRF), N2 adsorption- desorption for BET surface area, and Atomic force microscopy (AFM). Results showed that zinc oxide was loaded on zeolite as noticed by the characteristic peaks and was of nano scale having an average diameter of 88.57nm. The percentage loading of ZnO on zeolite A was 28.37% and the surface area was 222m2/g. The activity of the prepared catalyst was examined in the desulfurization of double hydrogenated diesel fuel. The process was investigated in a
... Show More