In this study, high quality ZnO/Ag-NPs thin transparent and conductive film coatings were fabricated
Cadmium Oxide thin films were deposited on glass substrate by spray pyrolysis technique at different temperatures (300,350,400, 500)oC. The optical properties of the films were studied in this work. The optical band-gap was determined from absorption spectra, it was found that the optical band-gap was within the range of (2.5-2.56)eV also width of localized states and another optical properties.
In the present work, silver nanoparticles were prepared. Nonlinear optical properties and
optical limiting of silver nanoparticles were investigated.Standard chemical synthesis method was used at
diffrent weight ratio(0.038, 0.058 and 0.078) of silver nitrate. Several testing were done to obtain the
characteristics of the sample. Z-Scan experiments were performed using 30 ns Q-switched Nd:YAG
laser at 1064 nm and 532 nm at different intensities. The results showed that the nonlinear refractive
index is directly proportional to the input intensities, which caused by the self-focusing of the material.
In addition, the optical limiting behavior has been studied. The results showed that the sample could be
used as an opt
In this work, (ZnO)1-x(MnO2)x compounds were synthesized with composition (x=0, 0.1, 0.2, 0.3, 0.4, and 0.5) of manganese oxide content using solid state reaction. Thin films were prepared from these compounds on glass substrates at room temperature using pulsed laser deposition method. The structure of the prepared compounds and thin films were analyzed using x-ray diffraction while the optical properties was measured using UV-visible spectrophotometry. It was found that the synthesized composites declared many peaks in the diffraction pattern which indicate polycrystalline structure with hexagonal wurtzite hexagonal structure of ZnO, and MnO2 and Mn2O3 secondary phases. A narrowing in the optical e
... Show MoreZnS:MnP2+P nanoparticles were prepared by a simple microwave irradiation method under mild condition. The starting materials for the synthesis of ZnS:MnP 2+P quantum dots were zinc acetate as zinc source, thioacetamide as a sulfur source, manganese chloride as manganese source (R & M Chemical) and ethylene glycol as a solvent. All chemicals were analytical grade products and used without further purification. The quantum dots of ZnS:MnP 2+P with cubic structure were characterized by X-ray powder diffraction (XRD), the morphology of the film is seen by scanning electron microscopy (SEM) also by field effect scanning electron microscopy (FESEM). The composition of the samples is analysed by EDS. UV-Visible absorption spectroscopy analysis
... Show MoreThe optical energy gap and optical constants such as the reflective index, dielectric constant have been evaluated due to The optical transmission and UV-VIS absorption spectra have been recorded in the wavelength (200 - 1100 nm) for PVA/PANI polymer blends and PVA/PANI/ZnO nanocomposites with different concentrations of ZnO (0.02, 0.05, 0.07, 0.1and 0.2) wt %. The results indicate that the materials have allowed direct transition. The reflection index and dielectric constant are increase with wavelength
Rare earth elements (Cerium, Lanthanum and Neodymium) doped CdS thin films are prepared using the chemical Spray Pyrolysis Method with temperature 200 oC. The X-ray diffraction (XRD) analysis refers that pure CdS and CdS:Ce, CdS:La and CdS:Nd thin films showed the hexagonal crystalline phase. The crystallite size determined by the Debye-Scherrer equation and the range was (35.8– 23.76 nm), and it was confirmed by field emission scanning electron microscopy (FE-SEM). The pure and doped CdS shows a direct band gap (2.57 to 2.72 eV), which was obtained by transmittance. The room-temperature photoluminescence of pure and doped CdS shows large peak at 431 nm, and two small peaks at (530 and 610 nm). The Current – voltage measurement in da
... Show More