Background: Cutaneous leishmaniasis (CL) is a neglected disease in tropical countries, including Iraq. Several studies have sought to examine chemotherapies for leishmaniasis treatment but most of them are of toxic and/or undesirable side effect, therefore, the need for investigating new fewer toxic therapies is essential. Aim of study: In this study, the cytotoxic effect of Artemisinin (ART), a novel herbal compound, was screened against the two forms, promastigotes and amastigotes, of the Iraqi isolate of Leishmania tropica, the causative agent of Baghdad boil. Material and methods: Different concentrations (1000, 500, 250, 125, 62.5, 31.25, 15.6 and 7.8) µM of Artemisinin were screened to investigate the leishmanicidal activity of the herbal compound against the two forms of the parasite along three times of follow up (24, 48, 72) hour using MTT cytotoxicity assay. Results: The results showed that growth rate and cell viability were significantly decreased at all studied concentrations. The IC50 was measured after 72 hours of follow up and was 2.625 µM and 2.636 µM for promastigotes and amastigotes, respectively. Conclusion: These findings approved the leishmanicidal efficacy of Artemisinin against the of L. tropica and can be further studied to screen its effectiveness in vivo for exploring a safer herbal drug for treatment of cutaneous leishmaniasis.
Hydroxide upon the chemical composition and dry matter(DM) and organic matter(OM) digestibility . Rice straw was treated with 4% sodium hydroxide using 30% of DM basis moisture, and incubated at 40 ºC for 40 days., DM digestibility (DMD) was significantly affected (P<0.01) by the treatment , where DMD increased The objective of this experiment was to study the effect of physical form (long ,chopped and ground ) and washing rice straw treated with sodium from 42.32 to 45.41% , OM digestibility (OMD) and total digestible nutrient (TDN) increased(P<0.05) from 47.38 and 49.33 to 49.67 and 52.83% ,respectively. While hemicellulose content increased (P<0.05 ) from 261.71 to 268.17 gm/kg DM ,and metabolizable energy (ME) from 7.11 to 7.48 MJ/
... Show MoreABSTRACT Background: Color changes that are detectable to human eye can affect the esthetic appearance of ceramic veneers. The purpose of this study was to evaluate and compare the effect of artificial accelerated aging on the color of ceramic veneers cemented with different resin cements. Materials and Methods: Sixty discs were prepared with 0.5 mm thickness, 30 discs made from IPS e.max press (Ivoclar Vivadent) and 30 discs were made from VITA Enamic (VITA Zahnfabrik). The discs were cemented with three resin cements: Variolink Veneer MV 0 shade (Ivoclar Vivadent), Rely X veneer Translucent shade (3M ESPE) and NX3 Nexus Clear shade (Kerr Corporation) with 0.1 mm thickness. The spectrophotometer Easyshade Advance was used to measure the co
... Show MoreBackground: Studying and investigating the transverse strength(Ts), impact strength(Is), hardness (Hr) and surface roughness(Ra) of conventional and modified autopolymerizing acrylic resin with different weight percentages of biopolymer kraftlignin, after curing in different water temperatures; 40°C and 80°C. Material and Methods: Standard acrylic specimens were fabricated according to ADA specification No.12 for transverse strength, ISO 179 was used for impact testing, Shore D for hardness and profilometerfor surface roughness. The material lignin first dispersed in the monomer, then the powder PMMA is immediately added. Ligninadded in different weight percentages. Then cured using pressure pot (Ivomet) in two temperatures;40°C a
... Show MoreABSTRACT Background: This study measured the effects of three parameters pH value, length of immersion and type of archwire on metal ions released from orthodontic appliances. Materials and Methods: Ninety maxillary halves simulated fixed orthodontic appliances that were immersed in artificial saliva of different pH values (6.75, 5 and 3.5) during 28 day period. Three types of archwires were used: stainless steel, nickel titanium and thermal activated nickel titanium. The quantity of nickel and chromium ions was determined with the use of atomic force spectrophotometer while iron ions by spectrophotometer. Each orthodontic set was weighted two times, before the ligation and immersion in the artificial saliva and after 28 days at the end of
... Show MoreBackground: The aim of this study was to evaluate the shear bond strength (SBS) and adhesive remnant index (ARI) of different orthodontic adhesive systems after exposure to aging media (water storage and acid challenge). Materials and methods: Eighty human upper premolar teeth were extracted for orthodontic purposes and randomly divided into two groups (40 teeth each): the first group in which the bonded teeth were stored in distilled water for 30 days at 37°C, and the second group in which the bonded teeth were subjected to acid challenge. Each group was further subdivided into four subgroups (10 teeth each) according to the type of adhesive system that would be bonded to metal brackets: either non-fluoride releasing adhesive (NFRA),
... Show MoreAbstract: The aim of this study is to assess the effectiveness of 940 nm diode laser in comparison to Endoactivator in elimination of smear layer in terms of radicular dentin permeability and ultra-structural changes of root canal walls by SEM evaluation. Twenty-eight single-rooted extracted lower premolars were instrumented up to size X4 (protaper Next, Dentsaply) and divided into two experimental groups according to the irrigation system, G1; activated by EndoActivator and G2; activated by Diode laser 940 nm, CW mode, 1.7 W. Afterward, the roots were made externally impermeable, filled with 2%methylene blue dye, divided horizontally into three segments representing the apical, middle, and coronal thirds then examined under stereo- micr
... Show MoreEffects of Ozonated Water on Micro Leakage between Enamel and Fissure Sealants Prepared by Different Etching Technique (An in vitro Study), Baraa M Jabar*, Muna S Khalaf
Resin-modified glass ionomer cement tends to shrink due to polymerization of the resin component. Additionally, they are more prone to syneresis and imbibition during the setting process. This