Preferred Language
Articles
/
WYaRc4YBIXToZYALuIrv
Shear strength of steel fibre RC beams under repeated loads
...Show More Authors

Scopus Clarivate Crossref
Publication Date
Wed Jun 17 2026
Journal Name
Journal Of Baghdad College Of Dentistry
Comparison of regional bond strength among different types of posts luted with different types of cement
...Show More Authors

Background: This in vitro study was carried out to investigate the effect of post space regions (coronal, middle and apical), the effect of post types ( Manually Milled Zirconia post, Prefabricated Fiber post, prefabricated Zirconia post) and the type of cement used (GIC, self-adhesive resin cement) on the bond strength between the posts and root dentin by using push-out test. Material and methods: Forty eight mandibular premolars extracted for orthodontic reasons (single rooted) were instrumented with ProTaper system (hand use) and obturated with gutta percha for ProTaper using AH26® root canal sealer following the manufacturer instructions. After 24 hours, post space was prepared using Zirix and Glassix drills no.3 creating 8 mm dept

... Show More
View Publication Preview PDF
Publication Date
Sun Jan 01 2006
Journal Name
J Bagh College Of Dentistry
Assessment of diametral tensile strength and microhardness of Glass ionomer reinforced by different amounts of Hydroxyapatite
...Show More Authors

Back ground: Glass ionomer materials lack resistance to wear and pressure and are susceptible to moisture during the initial stages of setting and dehydration. So this study was done to assess diametral tensile strength and microhardness of glass ionomer reinforced by different amounts of hydroxyapatite. Materials and methods: In this study a hydroxyapatite material was added to glass monomer cement at different ratios: 10%, 15%, 20%, 25% and 30% (by weight). The diametral tensile strength test described by the British standard specification for zinc polycarboxylate cement was used in this study and the microhardness test was performed using Vickers microhardness testing machine and the microhardness values were calculated and statistical c

... Show More
View Publication Preview PDF
Publication Date
Sun Mar 21 2021
Journal Name
Periodicals Of Engineering And Natural Sciences (pen)
Estimation of the reliability system in model of stress- strength according to distribution of inverse Rayleigh
...Show More Authors

View Publication
Scopus (11)
Crossref (7)
Scopus Crossref
Publication Date
Sun Dec 09 2018
Journal Name
Baghdad Science Journal
Anticorrosion Behavior of Deposited Magnetite on Galvanized Steel in Saline Water Using RF-Magnetron Sputtering
...Show More Authors

Thin films of Magnetite have been deposited on Galvanized Steel (G-S) alloy using RF-reactive magnetron sputtering technique and protection efficiency of the corrosion of G-S. A Three-Electrodes Cell was used in saline water (3.5 % NaCl) solution at different temperatures (298, 308, 318 & 328K) using potentiostatic techniques with. Electrochemical Impedance Spectroscopy (EIS) and fitting impedance data via Frequency Response Analysis (FRA) were applied to G-S alloy with Fe3O4 and tested in 3.5 % NaCl solution at 298K.Results taken from Nyquist and Bode plots were analyzed using software provided with the instrument. The results obtained show that the rate of corrosion of G.S alloy increased with increasing the temperatures from 298 t

... Show More
View Publication Preview PDF
Scopus Clarivate Crossref
Publication Date
Sat Aug 21 2021
Journal Name
Engineering, Technology & Applied Science Research
The Response of a Highly Skewed Steel I-Girder Bridge with Different Cross-Frame Connections
...Show More Authors

Braces in straight bridge systems improve the lateral-torsional buckling resistance of the girders by reducing the unbraced length, while in horizontally curved and skew bridges, the braces are primary structural elements for controlling deformations by engaging adjacent girders to act as a system to resist the potentially large forces and torques caused by the curved or skewed geometry of the bridge. The cross-frames are usually designed as torsional braces, which increase the overall strength and stiffness of the individual girders by creating a girder system that translates and rotates as a unit along the bracing lines. However, when they transmit the truck’s live load forces, they can produce fatigue cracks at their connection

... Show More
View Publication
Crossref (5)
Crossref
Publication Date
Wed Dec 01 2010
Journal Name
Al-khwarizmi Engineering Journal
Improvement of Surface Roughness Quality for Stainless Steel 420 Plate Using Magnetic Abrasive Finishing Method
...Show More Authors

     An experimental study was carried out to improve the surface roughness quality of the stainless steel 420 using magnetic abrasive finishing method (MAF). Four independent operation parameters were studied (working gap, coil current, feed rate, and table stroke), and their effects on the MAF process were introduced. A rotating coil electromagnet was designed and implemented to use with plane surfaces. The magnetic abrasive powder used was formed from 33%Fe and 67% Quartz of (250µm mesh size). The lubricant type SAE 20W was used as a binder for the powder contents. Taguchi method was used for designing the experiments and the optimal values of the selected parameters were found. An empirical equation representing the r

... Show More
View Publication Preview PDF
Publication Date
Wed May 06 2015
Journal Name
International Journal Of Engineering Research And General Science
Use Reed Leaves as a Natural Inhibitor to Reduce the Corrosion of Low Carbon Steel
...Show More Authors

Publication Date
Tue Feb 01 2022
Journal Name
Journal Of Engineering Science And Technology
CORROSION of STEEL REINFORCEMENT in INTERNALLY CURED SELF-COMPACTING CONCRETE USING WASTE BRICK and THERMOSTONE
...Show More Authors

Internal curing is a method that has been advised to decrease the primary age cracking, mainly of concrete mixes using low (water to cementitious materials - w/cm) ratios corresponding to the self-compacting concrete-(SCC). This research aims to study the effect of the internal curing using saturated lightweight aggregate- (LWA) on the steel reinforcing corrosion in SCC. In this research, crushed bricks or thermostone were partially replaced by (20%) by the weight of sand and volumetrically measured. The results showed that the steel reinforcement of internally cured concrete showed a slight increase in corrosion up to 300 days of exposure to the saline solution (containing 3.5% NaCl). The ability of using the crushed bricks or thermostone

... Show More
Publication Date
Fri May 01 2020
Journal Name
International Journal Of Geomate
METHODOLOGY FOR MONITORING THE FLEXURAL BEHAV-IOR OF STRUCTURAL CONCRETE MEMBERS WITH UNBONDED INTERNAL STEEL
...Show More Authors

View Publication
Scopus (3)
Crossref (2)
Scopus Clarivate Crossref
Publication Date
Wed Mar 19 2025
Journal Name
Chemical Papers
Natural deep eutectic solvents as a green inhibitor of carbon steel corrosion in sulphuric acid
...Show More Authors

View Publication
Scopus (3)
Crossref (3)
Scopus Crossref