In this study, the physical, and mechanical properties of low-cost and biocomposites were evaluated. The walnut shell and date palm frond fibers were thermally treated in an oven at a temperature of 70°C and then chemically treated with NaOH and distilled water solution, after these treatments, the biocomposite materials will be thermally treated again at 50°C. This procedure was performed for three types of biocomposite; Walnut shell Fiber Reinforced Polymer (WFRP), Date palm Fiber Reinforced Polymer (DFRP), and Hybrid Fiber Reinforced Polymer (HFRP), whereas the biocomposite sheets consisting of 30% biofibers and 70% unsaturated polyester, the mechanical test specimens were cut by a CNC machine according to ASTM standards. The effect of fiber type was analyzed in terms of the mechanical properties (tensile, compression, and density). The tensile test results showed that the DFRP composite had the best results comparable with WFRP and HFRP, the ultimate tensile strength, was increased by 28.6%, and 12.5% respectively, furthermore, the compression strength of the WFRP composite was increased by 21.5%, and 10.3% compared with DFRP and HFRP composites respectively. The WFRP composite revealed the lowest value of density 4.60 g/cm3 rather than DFRP and HFRP composites.
Recently, there has been a major trend towards environmental issues and concern for the green product because traditional products cause serious environmental impacts such as reduced resources, global warming, energy consumption, emissions and other environmental damage. Under these developments, economic units are looking for cost-effective technologies that reduce the cost of a green product that has four main dimensions: reducing energy, reducing resource consumption, preventing pollution, and using renewable energy while not compromising quality and satisfying customers in order to enhance competitive advantage.
This research will address one of the most important cost-effective green technologies, Gr
... Show MoreThe printed circuit heat exchanger is a plate type heat exchanger with a high performance and compact size. Heat exchangers such as this need a unique form of bonding and other techniques to be used in their construction. In this study, the process of joining plates, diffusion bonding, was performed and studied. A special furnace was manufactured for bonding purposes. The bonding process of copper metal was carried out under specific conditions of a high temperature up to 700 oC, high pressure of 3.45 MPa, and in an inert environment (Argon gas) to make tensile samples. The tensile samples are cylindrical shapes containing groves representing the flow channels in the printed circuit heat exchanger and checking their tensile st
... Show MoreMembrane manufacturing system was operated using dry/wet phase inversion process. A sample of hollow fiber membrane was prepared using (17% wt PVC) polyvinyl chloride as membrane material and N, N Dimethylacetamide (DMAC) as solvent in the first run and the second run was made using (DMAC/Acetone) of ratio 3.4 w/w. Scanning electron microscope (SEM) was used to predict the structure and dimensions of hollow fiber membranes prepared. The ultrafiltration experiments were performed using soluble polymeric solute poly ethylene glycol (PEG) of molecular weight (20000 Dalton) 800 ppm solution 25 °C temperature and 1 bar pressure. The experimental results show that pure water permeation increased from 25.7 to 32.2 (L/m2.h.bar) by adding aceton
... Show Moreِabstract:In this research we prepared nanofibers by electrospinning from poly (Vinyl Alcohol) /TiO2. The spectrum of the solution (Emission) was studied and found to be at 772 nm, several process parameters were such as concentration of TiO2 , and the effect of distance from nozzle tip to the grounded collector (gap distance). The result of the lower concentration of, the smaller the diameter of nanofiber is. Increasing the gap distance will affect nanofibers diameter.
In this research we prepared nanofibers by electrospinning from
poly (Vinyl Alcohol) /TiO2. The spectrum of the solution (Emission)
was studied and found to be at 772 nm, several process parameters
were such as concentration of TiO2 , and the effect of distance from
nozzle tip to the grounded collector (gap distance). The result of the
lower concentration of, the smaller the diameter of nanofiber is.
Increasing the gap distance will affect nanofibers diameter
Membrane manufacturing system was operated using dry/wet phase inversion process. A sample of hollow fiber membrane was prepared using (17% wt PVC) polyvinyl chloride as membrane material and N, N Dimethylacetamide (DMAC) as solvent in the first run and the second run was made using (DMAC/Acetone) of ratio 3.4 w/w. Scanning electron microscope (SEM) was used to predict the structure and dimensions of hollow fiber membranes prepared. The ultrafiltration experiments were performed using soluble polymeric solute poly ethylene glycol (PEG) of molecular weight (20000 Dalton) 800 ppm solution 25 °C temperature and 1 bar pressure. The experimental results show that pure water permeation increased from 25.7 to 32.2 (L/m2.h.bar) by adding a
... Show MoreRutting is one of the most complex and widespread types of distress. The rutting is frequently observed on Iraqi roads, especially at the checkpoints, forming a significant hazard on the asphalt layers. Factors such as heavy loads and high temperatures contribute to this distress. Adding fibers to a hot mix asphalt (HMA) effectively improves performance and extends the lifespan of the flexible pavement. This article used glass, steel, and basalt fibers. The wheel tracking test assessed the fibre-asphalt mixture for rutting resistance and compared it with the mix without adding fibers (control HMA). Meanwhile, the microscopic structure of fibres and asphalt mixture modified with fibers was examined using the Field Emission Scanning E
... Show More