Zinc Oxide nanoparticles were prepared using pulsed laser ablation process from a pure zinc metal placed inside a liquid environment. The latter is composed of acetyltrimethylammonium bromide (CTAB) of 10−3 molarity and distilled water. A Ti:Sapphire laser of 800 nm wavelength, 1 kHz pulse repetition rate, 130 fs pulse duration is used at three values of pulse energies of 0.05 mJ, 1.11 mJ and 1.15 mJ. The evaluation of the optical properties for the obtained suspension was applied through ultraviolet–visible absorption spectroscopy test (UV/VIS). The result showed peak wavelengths at 210 nm, 211 nm and 213 nm for the three used pulse energies 0.05 mJ, 1.11 mJ and 1.15 mJ respectively. This indicates a blue shift, which means smaller sizes of prepared nanoparticles, correlated with the decrease in laser energy. The blue shift in the absorption edge refers to the quantum confinement property for the produced nanoparticles. In addition, Fourier Transform Infrared Spectroscopy (FTIR) analysis was utilized to confirm zinc oxide nanoparticles formation represented by the absorption values at 435–445 cm−1. The shape and morphology of ZnO nanoparticles were characterized with scanning electron microscope (SEM).
It is found that hypersensitive teeth have a larger number and wider patent tubules than those of non-sensitive teeth. Objective: The aim of this study is to compare between the effects of diode laser at different power densities, with and without sodium fluoride on the sealing of exposed dentinal tubules and dentin permeability. Materials and methods: 118 teeth were used. Samples were divided into three major groups. The first consisted of 100 teeth used for permeability test. The second consisted of 16 teeth for measuring external surface temperature elevation while irradiation. The third, in turn, consisted of one pair of teeth observed under SEM for dentine surface morphology analysis. Results: For dentin permeability measurement, th
... Show MoreInfrared photoconductive detectors working in the far-infrared region and room temperature were fabricated. The detectors were fabricated using three types of carbon nanotubes (CNTs); MWCNTs, COOH-MWCNTs, and short-MWCNTs. The carbon nontubes suspension is deposited by dip coating and drop–casting techniques to prepare thin films of CNTs. These films were deposited on porous silicon (PSi) substrates of n-type Si. The I-V characteristics and the figures of merit of the fabricated detectors were measured at a forward bias voltage of 3 and 5 volts as well as at dark and under illumination by IR radiation from a CO2 laser of 10.6 μm wavelengths and power of 2.2 W. The responsivity and figures of merit of the photoconductive detector
... Show MoreRock engineers widely use the uniaxial compressive strength (UCS) of rocks in designing
surface and underground structures. The procedure for measuring this rock strength has been
standardized by both the International Society for Rock Mechanics (ISRM) and American Society
for Testing and Materials (ASTM), Akram and Bakar(2007).
In this paper, an experimental study was performed to correlate of Point Load Index ( Is(50))
and Pulse Wave Velocity (Vp) to the Unconfined Compressive Strength (UCS) of Rocks. The effect
of several parameters was studied. Point load test, Unconfined Compressive Strength (UCS) and
Pulse Wave Velocity (Vp) were used for testing several rock samples with different diameters.
The predicted e
In research we prepared electrical conductive polymer mixture wich consisted of three polymers [pectin, poly vinyl acetate and poly Aniline] was prepared then doping silver nanoparticles. Meaning it was conducting research on the three stages the first is Preparing triple polymer blend , Preparing silver nanoparticles and Tchoub mix triple Article nanoparticles in different proportions to get (Nanopolymer composites), and Preparing and making chips complexes in (casting method) for the purpose of measuring electrical conductivity her. Also we examined samples spectrum infrared (FT-IR), X-ray diffraction), SEM microscope and atomic force microscopy AFM. Electrical conductivity of the device chips have been measured (LCR) resul
... Show MoreThis study investigates the constructs and related theories that drive social capital in energy sector from the intention perspectives. This research uses theories of 'social support' and 'planned behaviour' alongside satisfaction and perceived value to propose a research model that drives social capital for energy sectors in Malaysia. The model reveals that the Theories of Planned Behaviour (TPB) and Social Support Theory (SST) alongside satisfaction and perceived value factors promote social capital development in energy sectors. Using PLS-SEM to analyse data gathered from energy sector employees in Malaysia, this research demonstrates that social capital is present when there is trust and loyalty among the users and positively effects en
... Show MoreThe design, synthesis, and characterization of a star shaped 2,4,6-tris-(4`-carboxyphenoxy)-1,3,5-triazine liquid crystalline with columnar discotic mesophase properties establish H-bond interactions with 3,5-dialkoxypyidine were reported. The structures of the synthesized compounds were actually determined by elementary analysis, and FT-IR, ¹HNMR, ¹³CNMR, and mass spectroscopy. The mesomorphic properties of these mesogens were examined using differential scanning calorimetry (DSC) and optical polarizing microscopy (OPM). The synthesized molecules exhibited enantiotropic hexagonal columnar liquid crystal, which depends for the H- bond complex in a 1:3 ratio.
This investigation is a study of the length of time where drops can exist at an oil-water interface before coalescence take place with a bulk of the same phase as the drops. Many factors affecting the time of coalescence were studied in is investigation which included: dispersed phase flow rate, continuous phase height, hole size in distributor, density difference between phases, and viscosity ratio of oil/water systems, employing three liquid/liquid systems; kerosene/water, gasoil/water, and hexane/water. Higher value of coalescence time was 8.26 s at 0.7ml/ s flow rate, 30cm height and 7mm diameter of hole for gas oil/water system, and lower value was 0.5s at 0.3ml/s flow rate, 10 cm height and 3mm diameter of hole for hexane
... Show More