Zinc Oxide nanoparticles were prepared using pulsed laser ablation process from a pure zinc metal placed inside a liquid environment. The latter is composed of acetyltrimethylammonium bromide (CTAB) of 10−3 molarity and distilled water. A Ti:Sapphire laser of 800 nm wavelength, 1 kHz pulse repetition rate, 130 fs pulse duration is used at three values of pulse energies of 0.05 mJ, 1.11 mJ and 1.15 mJ. The evaluation of the optical properties for the obtained suspension was applied through ultraviolet–visible absorption spectroscopy test (UV/VIS). The result showed peak wavelengths at 210 nm, 211 nm and 213 nm for the three used pulse energies 0.05 mJ, 1.11 mJ and 1.15 mJ respectively. This indicates a blue shift, which means smaller sizes of prepared nanoparticles, correlated with the decrease in laser energy. The blue shift in the absorption edge refers to the quantum confinement property for the produced nanoparticles. In addition, Fourier Transform Infrared Spectroscopy (FTIR) analysis was utilized to confirm zinc oxide nanoparticles formation represented by the absorption values at 435–445 cm−1. The shape and morphology of ZnO nanoparticles were characterized with scanning electron microscope (SEM).
An acidic environment causes surface changes of resin composites. Filler particlesize and filler distribution also have a direct effect on these surface changes. This invitro study evaluated the influence of Pepsi Cola drink on the surface roughness ofComposan LCM and Composan Ceram over time. Sixteen disc shaped specimens(10mm diameter, 2mm thickness) of each resin composite were fabricated, therebyforming two groups (n= 8). Surface roughness (Ra) was analyzed after 24 hrs beforeexposure to beverage. The specimens were submitted to a five minutes immersion inPepsi Cola three times daily interrupted by immersion in deionized distilled water (37C˚). Surface roughness measurements were done at 10, 30, and 60 days intervals. Datawere
... Show MoreThis research is addressing the effect of different ferrocene concentration (0.00, 2.15x10-3, 4.30x10-3, 8.60x10-3, and 12.9x10-3) on the bulk free radical polymerization of methyl methacrylate monomer in benzene using benzoyl peroxide as initiator. The polymerization was conducted at 60º C under free oxygen atmosphere. The resulting polymers were characterized by FTIR. The results were compared with the presence and absence of ferrocene at 10% conversion. The %conversion was 3.04% with no ferrocene present in the polymerization medium and its increase to 9.06 with a first lowest ferrocene concentration added, i.e. 2.15 x10-3mol/l. This was positively reflected on the poly(methyl methacrylate) molecular weight measured by viscosity techniq
... Show MoreA friction stir spot welding (FSSW) process is an emerging solid state joining process in which the material that is being welded does not melt. In this investigation an attempt has been made to understand the effect of tool shoulder diameter on the mechanical properties of the joint. For this purpose four welding tools diameter (10,13, 16 and 19) mm at constant preheating time and plunging time were used to carry
out welding process. Effect of tool diameter on mechanical properties of welded joints was investigated using shear stress test and Microhardness of joint which welded was studied. Based on the stir welding experiments conducted in this study the results show that aluminum alloy (1200) can be welded using (FSSW) process with
Experimental research was carried out to investigate the effect of fire flame (high temperature) on specimens of short columns manufactured using SCC (Self compacted concrete). To simulate the real practical fire disasters, the specimens were exposed to high
temperature flame, using furnace manufactured for this purpose. The column specimens were cooled in two ways. In the first the specimens were left in the air and suddenly cooled using water, after that the specimens were loaded to study the effect of degree of
temperature, steel reinforcement ratio and cooling rate, on the load carrying capacity of the reinforced concrete column specimens. The results will be compared with behaviour of columns without burning (control specime
Background: Feeding is a complicated process that involves the coordination of cardiovascular, respiratory, gastrointestinal (GI), and oropharyngeal mechanisms, with support from the musculoskeletal and craniofacial systems. The practice of feeding could be correlated with eruption stage and nutritional status in infants. Aim of the study: This study aimed to assess the relation of feeding patterns to a selected oral variable (stage of the eruption of primary teeth) and growth parameters among clinically healthy infants. Subjects and Methods: A cross-sectional comparative study on a sample of (300) infants aged between 6 and 18 months was performed in Karbala City, Iraq. The feeding pattern was investigated using an information sheet ans
... Show MoreObjective(s): The aim of this study is to compare the impact strength of a heat cured denture-base acrylic resin
reinforced with metal wire and glass fibers.
Methodology: Forty five specimens were prepared from pink heat cure acrylic resin. Specimens were grouped into;
group-I (control group) which consists of 15 specimens with no reinforcement, group-II which consists of 15 specimens
reinforced with metal wire, and group-III consists of 15 specimens reinforced with glass fibers. Specimens were tested
by using charpy impact machine.
Results: The result showed that there was a highly significant difference in impact strength value among the testing
groups at (P < 0.001).
Conclusion: The impact str
... Show MoreIn this study, the effect of the combination of micro steel fibers and additives (calcium hydroxide and sodium carbonate) on the size of cracks formation and healing them were investigated. This study aims to apply the use of self-healing phenomenon to repair cracks and to enhance the service life of the concrete structures. Micro steel fibers straight type were used in this research with 0.2% and 0.4% by volume of concrete. A weight of 20 and 30 kg/m3 of Ca(OH)2 and 2 and 3 kg/m3 of Na2CO3 were used as a partial cement replacement. The results confirm that the concrete cracks were significantly self-healed up to 30 days re-curing. Cracks width up to 0.2 mm were comp