This investigation was undertaken to evaluate the effectiveness of using Hydrated lime as a (partial substitute) by weight of filler (lime stone powder) with five consecutive percentage namely (1.0, 1.5, 2.0, 2.5, 3.0) % by means of aggregate treatment, by introducing dry lime on dry and 2–3% Saturated surface aggregate on both wearing and binder coarse. Marshall design method, indirect tensile test and permanent deformation under repeated loading of Pneumatic repeated load system at full range of temperature (20, 40, 60) C0 were examined The study revealed that the use of 2.0% and 1.5 % of dry and wet replacement extend the pavement characteristics by improving the Marshall properties and increasing the TSR%. Finally, increase permanent deformation distress form by exhibiting mixture with lower slope value and flatter curve trend of intercepts plus the improvement in resilient modulus properties. The test result indicated that despite the less effect of wet method in Marshall Properties, it seems to most effective in reduce the premature of combined moisture damage and permanent deformation that were considered the major distress form currently, better than dry method of replacement
In this paper, the time-history responses of a square plan two-story reinforced concrete prototype building, considering the elastic and inelastic behavior of the materials, were studied numerically. ABAQUS software was used in three-dimensional (3D) nonlinear dynamic analysis to predict the inelastic response of the buildings. Concrete Damage Plasticity Model (CDPM) has been used to model the inelastic behavior of the reinforced concrete building under seismic excitation. The input data included geometric information, material properties, and the ground motion. The building structure was designed only for gravity load according to ACI 318 with
... Show MoreConcrete is widely used in construction materials since early 1800's. It has been known that concrete is weak in tension, so it requires some addition materials to have ductile behavior and enhance its tensile strength and strain capacity to improve their uses. In this study reactive powder concrete (RPC) was used with steel fiber by using different types of cement; (Ordinary Portland cement (OPC) and/or Portland- Limestone cement (PLC)) with three types of mixtures (OPC at the first mix, 50 % OPC and 50 % PLC at the second mix and PLC at the third mix). The behavior of RPC with steel fibers on compressive strength and tensile strength of concrete with different ages of curing (7, 14, 28 and 60) days and shrinkage have been studied. The clo
... Show MoreTest results of six half-scale reinforced concrete flat plates connections with an opening in the vicinity of the column are reported. The test specimens represent a portion of a slab bounded by the lines of contraflexure around the column. The tests were designed to study the effect of openings on the punching shear behavior of the slab-column connections. The test parameters were the location and the size of the openings. One specimen had no opening and the remaining five had various arrangements of openings around the column. All specimens were cast with normal density concrete of approximately 30 MPa compressive strength. The openings in the specimens were square, with the sides parallel to the sides of the column. Three sizes of ope
... Show MoreA long-span Prestressed Concrete Hunched Beam with Multi-Quadrilateral Opening has been developed as an alternative to steel structural elements. An experimental program was created and evaluated utilizing a single mid-span monotonic static load on simply supported beams, which included six beams with openings and the solid control beam without openings, to investigate the performance of such beams. The number and height of the quadrilateral openings are the variables to consider. According to test results, the presence of openings in the prestressed concrete hunched beam with multi-quadrilateral opening did not considerably affect their ultimate load capacity with respect to a contro
Every year, millions of tons of waste glass are created across the globe. It is disposed of in landfills, which is unsustainable since it does not disintegrate into the environment. This study aims to produce reactive powder concrete by using recycled glass powder and determine the influence on the mechanical properties. This study investigated the effect of partial replacement of cement with recycled glass powder at two percentages (0, 20) % by weight of cement on some mechanical properties (Fresh density, Splitting tensile strength, Impact Strength, and voids%) of reactive powder concrete containing 1 % micro steel (MSRPC). Furthermore, using steam curing for (5 hours) at 90 degrees celsius after hardening the sample directly, RPC was
... Show MoreVitamin K is a fundamental enzymatic co-factor implicated in the carboxylation of several vitamin K dependent proteins involved in the pathogenesis of certain age – related diseases. Inflammation is realized as an important factor in such diseases. Vitamin K is recognized to play an anti-inflammatory behavior that is distinct of its action as an enzymatic co- factor by suppressing many signaling pathways mainly the nuclear factor κB (NF-κB) signal transduction pathway. As well as to play a role as an antioxidant versus the generation of reactive oxidative species (ROS). The purpose of this review is to focus on the protective function of vitamin K as an anti-inflammatory agent
... Show MoreIn this work, Soda Lime Glass (S.L.G.) powder was used ,as
fluxe in traditional porcelain instead of feldspar. Two ceramics
porcelain were compared; commercial or traditional porcelain that
content of 50wt % kaolin, 25wt % quartz, and 25wt % feldspar.
Feldspar mass was substituted by scraps soda lime glass yielding a
new porcelain composition, to determine the softening points and
then the effect of glass addition on porcelain firing process.
Eight samples, for each patch, were prepared and 8wt % water
was added. The resulting composite blends were then die pressed at
2N, to produce disk specimens with diameter of 1.5 cm, and then
they were sintered at (1000, 1100, 1200, 1250,1300,1350,1400 and
1450) ˚C,