Biofilm formation is one of the biggest challenges of scientists. Role of heavy metals in forming biofilm is not clear enough. Here, the effect of lead on biofilm formation by Bacillus spp. isolated from soil in terms of biofilm formation and remove was studied. In present study, 10 isolates of Bacillus spp were isolated from soil. The ability of all isolates to form biofilm was evaluated. The effect of lead on biofilm formation was studied by adding lead (pb) before forming biofilm. In another experiment the lead was added after biofilm formation to study the effect of lead on biofilm remove. The current study, showed the ability of all studied isolates to form biofilm. Maximum biofilm formation by Bacillus spp isolate number 8 (B8) followed by B1 and B3. The lowest biofilm formation was found in case of isolate 4 (B4). The lead (50 ppm) reduced biofilm formation by B8, B1 and B3 isolates when the lead was used before biofilm formation (P <0.05). In another experiment the lead (50 ppm) was added after biofilm formation, it was observed that the biofilm formation was higher when the lead was added (after biofilm formation) as compared with control (serial distilled water) and the difference was significant (P<0.05). It can be concluded that the lead effect negatively on biofilm formation and positively on stability of biofilm.
In this search, Ep/SiO2 at (3, 6, 9, 12 %) composites is prepared by hand Lay-up method, to measure the change in the thermal conductivity and Impact Strength of epoxy resin before and after immersion in H2SO4 Solution with a 0.3N for 10 days. The results before immersion decreases with the increase of the weight ratios of the reinforcement material (SiO2), It changed from (82.6×10-2 to 38.7×10-2 W/m.°C) with change weight ratios from (3 to 12) % respectively, but after immersion time in the chemical solution where it was (65.6×10-2 W/m.°C) at the weight ratios (6 %) and became (46.6 × 10-2 W/m.°C) after immersion in sulfuric acid. The results of the Impact strength decreased by increasing the percentage weight ratio, it changed f
... Show MoreThis work describes, selenium (Se) films were deposited on clean glass substrates by dc planar magnetron sputtering technique.The dependence of sputtering deposition rate of Se film deposited on pressure and DC power has been studied. The optimum argon pressure has range (4x10-1 -8x10-2 )mbar. The optical properties such as absorption coefficient (α) was determined using the absorbance and transmission measurement from UnicoUV-2102 PC spectrophotometer, at normal incidence of light in the wavelength range of 200-850 nm. And also we calculated optical constants(refractive index (n), dielectric constant (εi,r), and Extinction coefficient (κ) for selenium films.
Studies were conducted to evaluate the biological effects of the non-steroidal ecdysone agonist (Methoxyfenozide), on different developmental larval stages of cotton leafworm Spodoptera littoralis (Boisd.) in the laboratory. The results showed that the early larval stages were the most susceptible to Methoxyfenozide which caused 100% mortality within 4-6 days after treatment at all used concentrations, while such percentage of mortality was achieved within 6 days after treatment for late larval stages when the highest concentration was used (0.2)g (ai) /L. Several morphological deformations were noticed on pupal stage, the results showed that the highest percentage of deformations was 1
... Show MoreThis study investigated the outcome of Alstonia boonei stem bark on liver enzymes after inducing the Wistar albino rats with carbon tetrachloride (CCl4). This effect of plant extract was compared with silymarin – a drug commonly used for the treatment of chronic hepatocyte disorder. The plant sample was extracted with ethanol; acute toxicity study of the extract was performed on eighteen Wistar mice, while 30 rats were sacrificed for liver enzymes assay. The rats were divided into six clusters: each cluster has five rats, culster 1 served as control and was given 2 mL/kg b.w - distilled water; clusters 2 – 6 were CCl4 induced. Cluster 2 was untreated but served as the negative control while cluster 3 wa
... Show MoreThe Cu2SiO3 composite has been prepared from the binary compounds (Cu2O, and SiO2) with high purity by solid state reaction. The Cu2SiO3 thin films were deposited at room temperature on glass and Si substrates with thickness 400 nm by pulsed laser deposition method. X-ray analysis showed that the powder of Cu2SiO3 has a polycrystalline structure with monoclinic phase and preferred orientation along (111) direction at 2θ around 38.670o which related to CuO phase. While as deposited and annealed Cu2SiO3 films have amorphous structure. The morphological study revealed that the grains have granular and elliptical shape, with average diameter of 163.63 nm. The electrical properties which represent Hall effect were investigated. Hall coeffici
... Show MoreIn this research, the study effect of irradiation on structural and optical properties of thin film (CdO) by spray pyrolysis method, which deposited on glasses substrates at a thickness of (350±20)nm , The flow rate of solution was 5 ml/min and the substrate temperature was held constant at 400˚C.The investigation of (XRD) indicates that the (CdO) films are polycrystalline and type of cubic. The results of the measuring of each sample from grain size, micro strain, dislocation density and number of crystals the grain size decreasing after irradiation with gamma ray from(27.41, 26.29 ,23.63)nm . The absorbance and transmittance spectra have been recorded in the wavelength range (300-1100) nm in order to study the optical properties. the op
... Show MoreCopper oxide thin films were deposited on glass substrate using Successive Ionic Layer Adsorption and Reaction (SILAR) method at room temperature. The thickness of the thin films was around 0.43?m.Copper oxide thin films were annealed in air at (200, 300 and 400°C for 45min.The film structure properties were characterized by x-ray diffraction (XRD). XRD patterns indicated the presence of polycrystalline CuO. The average grain size is calculated from the X-rays pattern, it is found that the grain size increased with increasing annealing temperature. Optical transmitter microscope (OTM) and atomic force microscope (AFM) was also used. Direct band gap values of 2.2 eV for an annealed sample and (2, 1.5, 1.4) eV at 200, 300,400oC respect
... Show MoreIn this research, the study effect of irradiation on structural and optical properties of thin film (CdO) by spray pyrolysis method, which deposited on glasses substrates at a thickness of (350±20)nm , The flow rate of solution was 5 ml/min and the substrate temperature was held constant at 400˚C.The investigation of (XRD) indicates that the (CdO) films are polycrystalline and type of cubic. The results of the measuring of each sample from grain size, micro strain, dislocation density and number of crystals the grain size decreasing after irradiation with gamma ray from(27.41, 26.29 ,23.63)nm . The absorbance and transmittance spectra have been recorded in the wavelength range (300-1100) nm in order to study the optical properties.
... Show MoreA thin CdS Films have been evaporated by thermal evaporation technique with different thicknesses (500, 1000, 1500 and 2000Å) and different duration times of annealing (60, 120 180 minutes) under 573 K annealing temperature, the vacuum was about 8 × 10-5 mbar and substrate temperature was 423 K. The structural properties of the films have been studied by X- ray diffraction technique (XRD). The crystal growth became stronger and more oriented as the film thickness (T) and duration time of annealing ( Ta) increases.
Titanium alloy (Ti-6Al-4V or Gr.23) was widely used as a dental alloy. In the current study, polymerization of eugenol (PE) on Gr.23 titanium alloys was conducted by an electrochemical process before and after being treated by Micro Arc Oxidation (MAO). The formed films were characterized by scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDS), and X-ray diffraction (XRD). The corrosion behavior of Gr.23 alloy in an artificial saliva environment at a temperature range of 293–323 K has been studied and assessed by means of electrochemical polarization and impedance spectroscopy techniques. Three cases are taken into consideration; bare Gr.23, Gr.23 coated by PE, and Gr.23 coated by PE after MAO treatment. The maxi