Preferred Language
Articles
/
UxY5GocBVTCNdQwC-jfr
Efficiency of CFRP torsional strengthening technique for L-shaped spandrel reinforced concrete beams
...Show More Authors
Abstract<p>The present study aims to get experimentally a deeper understanding of the efficiency of carbon fiber-reinforced polymer (CFRP) sheets applied to improve the torsional behavior of L-shaped reinforced concrete spandrel beams in which their ledges were loaded in two stages under monotonic loading. An experimental program was conducted on spandrel beams considering different key parameters including the cross-sectional aspect ratio (<italic>i.e.</italic>, web height/web thickness), and the availability of the CFRP strengthening system. The ledge of the spandrel beams was exposed during testing to a very high eccentric load, which was transferred to the web of the spandrel beam causing high shear, torsion, and bending moments. Consequently, the applied load resulted in in-plane and out-of-plane deformations of the web accompanied by flexural and shear cracks. This article demonstrates the advantage of using CFRP sheets to strengthen the mentioned members. The applied CFRP sheets increased the failure torsional load by about 37% compared to the identical L-spandrels without strengthening. The outcomes indicate that using CFRP sheets show improvement in restricting the deflections and rotation of L-spandrels due to increasing spandrel stiffness. The reduction in the degree of rotation attained more than 33% in comparison to the spandrel beams without strengthening. The experimental program confirmed the applicability of the proposed strengthening technique for compacted and slender L-shaped spandrel-reinforced concrete beams.</p>
Crossref
View Publication
Publication Date
Thu Sep 01 2016
Journal Name
Journal Of Engineering
Response of Laced Reinforced Concrete One Way Slab to Repeated Loading
...Show More Authors

Test results of nine reinforced concrete one way slab with and without lacing reinforcement are reported. The tests were designed to study the effect of the lacing reinforcement on the flexural response of one way slabs. The test parameters were considered is the lacing steel ratios of (0, 0.0025, 0.0045, and 0.0065), flexural steel ratios of (0.0025, 0.0045, and 0.0065) and span to the effective depth ratios of (11, 13, and 16). Two specimens had no lacing reinforcement and the remaining seven specimens had the lacing reinforcement. Four point bending test were carried out, one of the specimens was tested under the static load applied gradually up to failure and the other specimens were tested under repeated load (5 cyc

... Show More
View Publication Preview PDF
Publication Date
Fri Nov 13 2020
Journal Name
Mechanics Of Advanced Materials And Structures
Enhancing the strength of reinforced concrete columns using steel embedded tubes
...Show More Authors

This paper demonstrates an experimental and numerical study on the behavior of reinforced concrete (RC) columns with longitudinal steel embedded tubes positioned at the center of the column cross-section. A total of 12 pin-ended square sectional columns of 150 × 150 mm having a total height of 1400 mm were investigated. The considered variables were the steel tube diameters of 29, 58, and 76 mm and the load eccentricity (0, 50, and 150) mm. Accordingly, these columns were divided into three groups (four columns in each group) depending on the load eccentricity (e) to column depth (h) ratio (e/h = 0, 1/3, and 1). For each group, one column was solid (reference), and the other three columns contained steel tubes with hollow rat

... Show More
Crossref (12)
Crossref
Publication Date
Wed Aug 05 2020
Journal Name
Advances In Structural Engineering
Strength compensation of deep beams with large web openings using carbon fiber–reinforced polymer sheets
...Show More Authors

This article presents the results of an experimental investigation of using carbon fiber–reinforced polymer sheets to enhance the behavior of reinforced concrete deep beams with large web openings in shear spans. A set of 18 specimens were fabricated and tested up to a failure to evaluate the structural performance in terms of cracking, deformation, and load-carrying capacity. All tested specimens were with 1500-mm length, 500-mm cross-sectional deep, and 150-mm wide. Parameters that studied were opening size, opening location, and the strengthening factor. Two deep beams were implemented as control specimens without opening and without strengthening. Eight deep beams were fabricated with openings but without strengthening, while

... Show More
View Publication
Crossref (15)
Crossref
Publication Date
Wed Aug 05 2020
Journal Name
Advances In Civil Engineering
Strength compensation of deep beams with large web openings using carbon fiber–reinforced polymer sheets
...Show More Authors

This article presents the results of an experimental investigation of using carbon fiber–reinforced polymer sheets to enhance the behavior of reinforced concrete deep beams with large web openings in shear spans. A set of 18 specimens were fabricated and tested up to a failure to evaluate the structural performance in terms of cracking, deformation, and load-carrying capacity. All tested specimens were with 1500-mm length, 500-mm cross-sectional deep, and 150-mm wide. Parameters that studied were opening size, opening location, and the strengthening factor. Two deep beams were implemented as control specimens without opening and without strengthening. Eight deep beams were fabricated with openings but without strengthening, while

... Show More
Scopus (15)
Crossref (15)
Scopus Clarivate Crossref
Publication Date
Wed Oct 09 2019
Journal Name
Engineering, Technology &amp; Applied Science Research
Numerical Analysis of Segmental Post Tensioned Concrete Beams Exposed to High Fire Temperature
...Show More Authors

The main objective of this study is to characterize the main factors which may affect the behavior of segmental prestressed concrete beams comprised of multi segments. The 3-D finite element program ABAQUS was utilized. The experimental work was conducted on twelve simply supported segmental prestressed concrete beams divided into three groups depending on the precast segments number. They all had an identical total length of 3150mm, but each had different segment numbers (9, 7, and 5 segments), in other words, different segment lengths. To simulate the genuine fire disasters, nine beams were exposed to high-temperature flame for one hour, the selected temperatures were 300°C (572°F), 500°C (932°F) and 700°C (1292°F) as recomm

... Show More
View Publication Preview PDF
Crossref (3)
Crossref
Publication Date
Tue Jan 19 2021
Journal Name
Sn Applied Sciences
Post-fire serviceability and residual strength of composite post-tensioned concrete T-beams
...Show More Authors
Abstract<p>In this study, the response of ten composite post-tensioned concrete beams topped by a reinforced concrete deck with adequate reinforcing shear connectors is investigated. Depending on the concrete compressive strength of the deck slab (20, 30, and 40 MPa), beams are grouped into three categories. Seven of these beams are exposed to a fire attack of 700 and 800 °C temperature simultaneously with or without the presence of a uniformly distributed sustained static loading. After cooling back to ambient temperature, these composite beams are loaded up to failure, using a force control module, by monotonic static loading in a four-point-bending setup with two symmetrical concentrated loads applied in </p> ... Show More
View Publication Preview PDF
Scopus (3)
Crossref (3)
Scopus Clarivate Crossref
Publication Date
Fri May 01 2020
Journal Name
Civil Engineering Journal
Post-Fire Behavior of Post-Tensioned Segmental Concrete Beams under Monotonic Static Loading
...Show More Authors

This paper presents a study to investigate the behavior of post-tensioned segmental concrete beams that exposed to high-temperature. The experimental program included fabricating and testing twelve simply supported beams that divided into three groups depending on the number of precasting concrete segments. All specimens were prepared with an identical length of 3150 mm and differed in the number of the incorporated segments of the beam (9, 7, or 5 segments). To simulate the genuine fire disasters, nine out of twelve beams were exposed to a high-temperature flame for one hour. Based on the standard fire curve (ASTM – E119), the temperatures of 300◦C (572◦F), 500◦C (932◦F), and 700◦C (1292◦F) were adopted. Consequently,

... Show More
Crossref (1)
Crossref
Publication Date
Tue Jan 19 2021
Journal Name
Sn Applied Sciences
Post-fire serviceability and residual strength of composite post-tensioned concrete T-beams
...Show More Authors
Abstract<p>In this study, the response of ten composite post-tensioned concrete beams topped by a reinforced concrete deck with adequate reinforcing shear connectors is investigated. Depending on the concrete compressive strength of the deck slab (20, 30, and 40 MPa), beams are grouped into three categories. Seven of these beams are exposed to a fire attack of 700 and 800 °C temperature simultaneously with or without the presence of a uniformly distributed sustained static loading. After cooling back to ambient temperature, these composite beams are loaded up to failure, using a force control module, by monotonic static loading in a four-point-bending setup with two symmetrical concentrated loads applied in </p> ... Show More
Crossref (4)
Crossref
Publication Date
Fri May 01 2020
Journal Name
Civil Engineering Journal
Post-Fire Behavior of Post-Tensioned Segmental Concrete Beams under Monotonic Static Loading
...Show More Authors

This paper presents a study to investigate the behavior of post-tensioned segmental concrete beams that exposed to high-temperature. The experimental program included fabricating and testing twelve simply supported beams that divided into three groups depending on the number of precasting concrete segments. All specimens were prepared with an identical length of 3150 mm and differed in the number of the incorporated segments of the beam (9, 7, or 5 segments). To simulate the genuine fire disasters, nine out of twelve beams were exposed to a high-temperature flame for one hour. Based on the standard fire curve (ASTM – E119), the temperatures of 300◦C (572◦F), 500◦C (932◦F), and 700◦C (1292◦F) were adopted. Consequently,

... Show More
View Publication Preview PDF
Scopus (1)
Crossref (1)
Scopus Clarivate Crossref
Publication Date
Fri Sep 01 2023
Journal Name
Journal Of Engineering
The Effect of Cohesive Debonding Elimination on Enhancing the Flexural Performance of Damaged Unbonded Prestressed Concrete Girders Strengthened Using NSM CFRP
...Show More Authors

This manuscript studied the effect of U-CFRP wrapped sheet anchorage on the flexural performance of unbonded post-tensioned PC members subjected to partial strand damage and strengthened using CFRP Near-Surface Mounting techniques. The program includes six girders as a control girder, a girder with strand damage of 14.2%, and four girders strengthened by CFRP laminates using the NSM technique with and without U-CFRP wrapped sheet anchorages. The testing results show that the strand damage of 14.2% has reduced the flexural strength of the girder by 5.71%. The NSM-CFRP laminate has a significant effect on flexural strength by 17.4%. On the other hand, the application of end U-CFRP wrapped sheet anchorages improves flexural

... Show More
View Publication Preview PDF
Crossref