Background: White spot lesion considered as irreversible tooth demineralization presenting challenge to orthodontists during treatment schedules, fluoride was the most successfully used measure to overcome this challenge. Materials and method: A total of forty sound human permanent premolars were used in the present study and categorized into four groups, in one group the teeth were bonded with stainless steel brackets using Resin-modified glass ionomer cement (RMGIC) and the other three groups the teeth were bonded with light cured composite Resilience® (Ortho technology Co., USA). Group A; Acidulated phosphate fluoride (APF) topical gel (Mfg by DEEPAK PRODUCTS, INC, USA), fluoride ion 1.23% applied on examine area for four minute. Gro
... Show MoreThis study was conducted in the Tissue Culture laboratory of the Horticultural Department of the Faculty of Agriculture at Karbala University to investigate the effects of a light source (Florescent, LED) and adenine sulfate (Ads) a 0, 40, 80, and 120 mg l-1 on the multiplication and rooting of
Background: White spot lesions are esthetic problems caused by subsurface enamel demineralization that seen as white opacity. Aim of the study: This study aimed to evaluate and to compare the color change after the treatment of the white spot lesions with resin nϔtrton and micro abrasion. Materials and Methods: rtϔ white spot lesions were generated on 48 premolar teeth by the use of a demineralization solution. The teeth were randomly divided using the Diagnodent into three study groups (16 teeth for each group) depending on the depth of the induced lesions: outer enamel, inner enamel and outer dentine. Then each group was fatherly subdivided into two groups (8 teeth for each group) the ϔrst group was treated wit
... Show MoreBackground: The marginal fit is the most characteristic that closely related to the longevity or success of a restoration, which is absolutely affected by the fabrication technique. The objective of present in vitro study was to evaluate the effect of four different CAD/CAM systems on the marginal fit of lithiµm disilicate all ceramic crowns. Materials and Methods: Adentoform tooth of a right mandibular first molar was prepared to receive all ceramic crown restoration with deep chamfer finishing line (1mm) and axial reduction convergence angle of 6 degree, dentoform model duplicated to have Nickel-Chromiµm master die. Thirty two stone dies produce from master die and distributed randomly in to four groups (8 dies for each group) accor
... Show MoreProduction of the steroidal saponin digitonin in multiplied shoots of Digitalis purpurea , (var. Excelsior Mixed) has been achieved in vitro by two experiments. In the experiment 1, shoot tips ( 1cm length ) explants from the sterilized seedlings were excised and cultured on MS medium ( Murashige and Skoog medium) supplemented with 0.5 mg/L TDZ (thidiazuron) and cholesterol at the concentrations 0.0, 0.1, 0.3, 0.5, 1.0, 1.5, 2.0 or 4.0 mg/L. After 45 day, results showed that the treatment with 0.5 mg/L TDZ and 2.0mg/L cholesterol had a positive effected on increasing the dry weight of multiplied shoots and their production of digitonin when compared with other treatments, where this treatment gave 2
... Show MoreCopper oxide nanoparticles (CuO NPs) were synthesized by two methods. The first was chemical method by using copper nitrate Cu (NO3)2 and NaOH, while the second was green method by using Eucalyptus camaldulensis leaves extract and Cu (NO3)2. These methods easily give a large scale production of CuO nanoparticles. X-ray diffraction pattern (XRD) reveals single phase monoclinic structure. The average crystalline size of CuO NPs was measured and used by Scherrer equation which found 44.06nm from chemical method, while the average crystalline size was found from green method was 27.2nm. The morphology analysis using atomic force microscopy showed that the grain size for CuO NPs was synthesized by chemical and green methods were 77.70 and 89.24
... Show MoreThese days, the world is facing a global environmental and sustainability problem due to the increasing generation of large amounts of waste through construction and demolition work, which causes a serious problem for the environment. Therefore, this research was conducted to get rid of the waste disposal problems, including old glass and concrete, which were used as recycled fine aggregates. Seven different mixtures were prepared. The first mixture was with the used sand, which is glass sand, and it was adopted as a reference mixture (ORPC), and three mixtures were prepared for each of the recycled materials (waste concrete and glass) and partially replaced by glass sand in different proportions (25, 50, and 75) %. Some
... Show MoreThe effect of internal acoustic excitation on the leading-edge, separated boundary layers and the aerodynamic performance of NACA23015 cross section airfoil are examined as a function of excitation location with ranging frequency range (50-400) Hz of the introduced acoustic. Tests are separately conducted in two sections, open type wind tunnels at the Reynolds number of 3.3x105 for measurement at angle of attack (0, 3, 6, 9 &12) deg. and 3x104 for the visualization at angle of attack (12) deg. based on the airfoil chord. Results indicated that the excitation frequency and the excitation location are the key parameters to alter the flow properties and thus to improve the aerodynamic performance. The most effective excitation frequency
... Show MoreToday technology using nanoparticle when treatment pathogentic microorganism and we focused on this here. It was found that the species of streptococcus used in present study were sensitive to erythromycin. In present study focusing biofilm formation by Streptococcus spp was evaluated. Species S. mutans was found that highest amount of biofilm compare with the other species. The aim of report effect (SNPs) on ability of biofilm form different species of streptococcus. The anti-biofilm effect of SNPs was in concentration dependent manner. The highest effect of SNP against biofilm formation was found the concentration 160 μg/ml, while the lowest effect was found the lowest used concentration (80 μg/ml) of SNPs. In vivo study revealed that s
... Show More