Background: The aim of this study was to measure the radiopacity (RO) of modified microhybrid composite resins by adding 2 types of nanofillers (Zinc Oxide and Calcium Carbonate) in two concentrations 3% and 5% and comparing them to unmodified microhybrid composite resins and to nanofilled composite resin. Materials and Methods: Two types of composite resin were used (Microhybrid composite MH Quadrent anterior shine and Nanofilled composite resin Filtek Z350 XT), for each tested group five disk-shaped specimens (1-mm-thick and 15 mm diameter) were fabricated. The material samples were radiographed together with the aluminum step wedge. The density of the specimens was determined with a transmission densitometer and was expressed in term of
... Show MoreBackground: The aim of this study is to evaluate the color change ∆E of the dental enamel following treatment with 2 kinds of protector (icon infiltrant, clinpro varnish) before fixed orthodontic treatment to avoid the possible white spot lesions. Materials and Methods: Fifty four subjects treated with fixed appliances were divided into 3 groups: the 1st group was control, while the 2nd and 3rd groups were treated with icon infiltrant and clinpro varnish before bonding procedure, respectively. Color parameters (L,a,b) were recorded for the middle and gingival thirds before and after bonding procedure to get the ∆E of each group. Results: One-way ANOVA test showed a non-significant difference in ∆E between the 3 groups a
... Show More
Background: One of the major problems in endodontics is micro-leakage of root canal fillings which might contribute to the failure of endodontic treatment. To avoid this problem, a variety of sealers have been tested. The objective of this, in vitro, study was to evaluate the shear bond strength of four resin based sealers (AH plus, silver free AH26, RealSeal SE and Perma Evolution permanent root canal filling material) to dentin. Materials and Methods: Forty non-carious extracted lower premolars were used. The 2mm of the occlusal surfaces of teeth were sectioned, to expose the dentin surface. The exposed dentin surfaces of teeth were washed with 5ml of 2.5% NaOCl solution followed by 5ml of 17 % EDTA then rinsed by deionized water to remov
... Show MoreBackground: Studying and investigating the transverse strength(Ts), impact strength(Is), hardness (Hr) and surface roughness(Ra) of conventional and modified autopolymerizing acrylic resin with different weight percentages of biopolymer kraftlignin, after curing in different water temperatures; 40°C and 80°C. Material and Methods: Standard acrylic specimens were fabricated according to ADA specification No.12 for transverse strength, ISO 179 was used for impact testing, Shore D for hardness and profilometerfor surface roughness. The material lignin first dispersed in the monomer, then the powder PMMA is immediately added. Ligninadded in different weight percentages. Then cured using pressure pot (Ivomet) in two temperatures;40°C a
... Show MoreThe present paper analyzes the signal emitting from the Reticle during changing the spot size of laser falling on the disk and shows the optimum frequency and the amount of energy window in different patterns of modulator (Reticle). All results are obtained by establishing a special program named “Disk optical modulator version 3" using the language visual basic 6 ahich contains many parameters. All models of optical modulator consist of twenty sectors, ten sectors are opaque and other ten sectors are transmitted for the laser. The number of sectors depends on several factors as chopping frequency, power transparent and modulation transfer function. It has been demonstrated by simulations, the optimal
... Show MoreBackground: The objectives of this study are to evaluate the effect of addition of Multi-Wall Carbon Nano Tubes (MWCNTs) of different concentrations (0.05 mg.mL-1,0.25 mg.mL-1,0.5 mg.mL-1and1 mg.mL-1) on dimethyl sulphoxide DMSO and distilled water (DW) on tooth enamel. It intends to evaluate enamel microhardness in (Kg. m-2) pre and post the application of Multi-Wall Carbon Nano Tubes (MWCNTs). Materials and Methods: Thirty specimens prepared for the present study to measure the hardness of the enamel. Results: The results showed that a significant increase in the enamel microhardness for groups 0.05 mg/mL (group B), 0.25 mg/mL (group C), 0.5 mg/mL (group D) and 1 mg/mL (group E) compared with control group (group A) in dimethyl sulphoxi
... Show MoreBackground: This study aimed to compare the surface microhardness (MH) and mineral content of white spot lesions(WSLs) after using bioactive glass (BAG)casein phosphopep-tides-amorphous calcium phosphate(CPP-ACP),and nanohydroxyapatite(Nano-HAP) under pHcycling. Material and method:18 sound maxillary first premolar were used for the study.10 were selected for the vickers microhardness test, For Energy-dispersive X-ray spectroscopy analysis (EDX), the remaining 8 premolar teeth were used, 40 sections of enamel blocks (Four from each tooth) were produced from the middle part of the buccal and palatal surfaces of teeth for MH test while 48 sections of enamel blocks (Six from each tooth) were produced for EDX analysis. Enamel slabs were divi
... Show MoreThis search aim to measure Hardness for Epoxy resin and for unsaturated Polyester resin as base materials for composite Hybrid and the materials used is Hybrid fiber Carbon-Kevlar. The Hand Lay-up method was used to manufacture plates of Epoxy resin (EP) and unsaturated Polyester EP,UPE backed by Hybrid fiber (Carbon-Kevlar) and with small volume fraction 5,10 and 15 for every there are Layer of fibers (1,2 and 3). The hardness test was count for material EP, UPE resin and there composites and that we notice that the Hardness (HB) decreased with increase of temperatures.