he paper presents the results of exposure of normal concrete to high temperatures (400 and 700°C). In addition to the exposure of steel reinforcement bar Ø 12 mm, where two types of steel reinforcement burning situations were performed. Directly exposed to high temperatures (400 and 700°C) and others were covered by concrete layer (15 mm). From the experimental results of fire exposure for 1 hour of 400 and 700°C and gradually cooled, it was found that the residual average percentage of compressive strength of concrete was 85.3 and 41.4%, while the residual average percentage of modulus of elasticity of concrete was 75 and 48%, respectively. The residual average percentage of yielding tensile stress (Ø 12 mm) after burning and cooling at the same conditions was 96.6 and 86.4% for bars covered by concrete and 93.4 and 81.3% for uncovered bars, while the residual average percentage of the ultimate tensile strength (Ø 12 mm) was 94 and 81%, for bars covered by concrete and 91 and 76% for uncovered bars, respectively.
Unused and expired pharmaceutical drugs are a novel type of organic corrosion inhibitor. They are less expensive, more effective, and less harmful than conventional organic corrosion inhibitors. This study investigated the effects of concentration, adsorption mechanism and thermodynamic parameters of enalapril malate (ENAP) as a corrosion inhibitor for carbon steel in a saline solution (3.5 % NaCl). The polarization method was used to determine the corrosion rate and inhibition efficiency. Field emission scanning electron microscopy (FE-SEM) and atomic force spectroscopy (AFM) were used to investigate the surface morphology and topography of carbon steel after immersion in both uninhibited and inhibited media for 24 h. Fourier transform inf
... Show MoreThis study deals with the corrosion inhibition of metal corrosion process of medium carbon steel using 1M HCl for kinetic studies and rate reaction determination. The weight loss method is applied to pieces of Medium carbon steel divided to Cubans with dimensions (0.4*2*2.4) cm , and use Tafel Extrapolation Method, the samples were polished using carbide silicon paper with dimensions of (180,200,400,600,800,1000). The samples were immersed in the alcoholic medium ethanol at a temperature 293K for 3hr. Natural inhibitor Kujarat Tea (Hibiscus sabdarriffa L.) is used which is extracted in aqueous and alcoholic medium, different concentrations (1000،2000, 3000) ppm have been used ; The best concentration found through the results is a
... Show MoreThis study deals with the corrosion inhibition of metal corrosion process of medium carbon steel using 1M HCl for kinetic studies and rate reaction determination. The weight loss method is applied to pieces of Medium carbon steel divided to Cubans with dimensions (0.4*2*2.4) cm , and use Tafel Extrapolation Method, the samples were polished using carbide silicon paper with dimensions of (180,200,400,600,800,1000). The samples were immersed in the alcoholic medium ethanol at a temperature 293K for 3hr. Natural inhibitor Kujarat Tea (Hibiscus sabdarriffa L.) is used which is extracted in aqueous and alcoholic medium, different concentrations (1000،2000, 3000) ppm have been used ; The best concentration found through the results is a conce
... Show MoreThe effect of time (or corrosion products formation) on corrosion rates of carbon steel pipe in aerated 0.1N NaCl
solution under turbulent flow conditions is investigated. Tests are conducted using electrochemical polarization
technique by determining the limiting current density of oxygen reduction in Reynolds number range of 15000 to 110000
and temperature range of 30 to 60oC. The effect of corrosion products formation on the friction factor is studied and
discussed. Corrosion process is analyzed as a mass transfer operation and the mass transfer theory is employed to
express the corrosion rate. The results are compared with many proposed models particularly those based on the
concept of analogy among momentum, heat,
In this study we focused on the determination of influence the novel synthesized thiosemicarbazide derivative "2-(2-hydroxy-3-methoxybenzylidene) hydrazinecarbothioamide" (HMHC) influenced the corrosion inhibition of mild steel (MS) in a 1.0 M hydrochloric acid acidic solution.This is in an effort to preserve the metal material by maintaining it from corrosion.The synthesized inhibitor was characterized using elemental analysis, and NMR-spectroscopy. Then the corrosion inhibition capability of (HMHC) was studied on mild steel in an acidic medium by weight loss technique within variables [temperature, inhibitor concentration, and time]. The immersion periods were [1:00, 3:00, 5:00, 10:00, 24:00, and 72:00] hours and the tem
... Show MoreThis work includes preparation of Az, Qz, and Tz derivatives from the reaction of Schiff base (Sb) derivative with anthranilic acid, chloroacetyl chloride, and sodium azide, as well as, the characterization via FT-IR, 1H-NMR, and 13CNMR. The anticorrosion inhibition of these compounds was studied and the measurements of carbon steel (CS) corrosion in sodium chloride solution 3.5% (blank) and inhibitor in solutions were calculated at a temperature range of 293-323 K by the technique of electrochemical polarization. In addition, some thermodynamic and kinetic activation parameters for inhibitor and blank solutions (Ea⋇, ΔH⋇, ΔS⋇, and ΔG⋇) were determined. The results showed high inhibition efficacy for all the prepared compounds,
... Show MoreThe main objective of this study is to understand the work of the pile caps made of lightweight aerated foam concrete and study the many factors affecting the ability and the capacity of the shear. The study was done by analyzing previous practical and theoretical experiences on the reinforced concrete pile caps. The previous practical results indicated that all specimens failed by shear diagonal compression or tension modes except one specimen that failed flexural-shear mode. Based on test specimens' practical results and behavior, some theoretical methods for estimating the ultimate strength of reinforced concrete pile caps have been recommended, some of which evolved into the design documents available on the subject.
... Show MoreNanoferrite materials have been synthesized by sol-gel auto combustion method. The effect of doping different percentages of Y2O3 (0.34 µm) on the physical and mechanical properties of selected mixed ferrite [(Li2.5Fe0.5) 0.9(Co4Fe2O4) 0.1] by adding 10% Cobalt ferrite was studied. Physical properties (i.e. .density, porosity and water absorption) were affected by the doping, where the density increased about 32% at 6 wt% Y2O3, while porosity has a drastically decreased about 80% at 6% Y2O3 and has a correlation effect on the mechanical properties(Splitting tensile strength and Vicker
... Show MoreAbstract
The toughening of epoxy resins with the addition of organic or inorganic compounds is of great interest nowadays, considering their large scale of applications. In the present work, composites of epoxy are synthesized with kaolin particles having different particle sizes as reinforcement. Composites of epoxy with varying concentration (0 to 40 weight %) of kaolin was prepared by using hand lay method. The variation of mechanical properties such as modulus of elasticity, yield, tensile, and compressive strength with filler content was evaluated. The composite showed improved modulus of elasticity and compressive properties on addition of filler. In contrast, the tensile and yield strength of the composite
... Show MoreThin films of tin sulfide (SnS) were prepared by thermal evaporation technique on glass substrates, with thickness in the range of 100, 200 and 300nm and their physical properties were studied with appropriate techniques. The phase of the synthesized thin films was confirmed by X-ray diffraction analysis. Further, the crystallite size was calculated by Scherer formula and found to increase from 58 to 79 nm with increase of thickness. The obtained results were discussed in view of testing the suitability of SnS film as an absorber for the fabrication of low-cost and non toxic solar cell. For thickness, t=300nm, the films showed orthorhombic OR phase with a strong (111) preferred orientation. The films deposited with thickness < 200nm deviate
... Show More