In this study, NaOH dissolution method was applied to dissolve cellulose fibers which extracted from date palm fronds (type Al-Zahdi) taken from Iraqi gardens. In this process, (NaOH)-solution is brought into contact with the cellulose fibers at low temperature. Experiments were conducted with different concentrations of NaOH (4%, 6%, 8% and12%) weight percent at two cooling bath temperatures (-15 oC) and (-20oC). Maximum cellulose dissolution was 23 wt% which obtained at 8 wt% concentration of NaOH and at cooling bath temperature of -20oC. In order to enhance the cellulose fibers dissolution, the sample was pretreated with Fenton's reagent which consists of hydrogen peroxide (H2O2), oxalic acid (C2H2O4) and ferrous sulfate (FeSO4). This reagent reacts with cellulose fibers and produces free radicals which increase cellulose dissolution. In this work three variables were studied: cooling bath temperature (-15oCand-20oC), NaOH concentration (4%, 6%, 8% and12%) and time of Fenton's reagent treatment (1-48) hrs. The results showed that the best percent of cellulose dissolution was (42 wt %) which occurred at treatment time (24 hours), temperature (-20oC) and NaOH concentration 8%. In another set of experiments urea was added to NaOH solution as a catalyst with proportion (6%NaOH+4% urea) at two temperatures -15 and -20 oC. The results show that the solubility of cellulose increase to 62% for the sample which treated with Fenton's reagent and to 35% for the untreated sample, both values were obtained at -15oC.
Kombucha(Khubdat Humza) is composed of yeast and acetic acid bacteria especially, Acetobacter xylinum which forms a cellulose pellicle on tea broth. Kombucha(Khubdat Humza) produces bacterial cellulose pellicles, with unique purity and fine structure. It can be used in many forms, such as an emulsifier, stabilizer, dispersing agent, thickener and gelling agent but these are generally subsidiary to its most important use of holding on to water. Recently, bacterial cellulose is used in many special applications such as a scaffold for tissue engineering of cartilages and blood vessels, also for artificial skin for temporary covering of wounds, as well as its used in the clothing industry. The yield of cellulose produced were investiga
... Show MoreAs the bit rate of fiber optic transmission systems is increased to more than , the system will suffer from an important random phenomena, which is called polarization mode dispersion. This phenomenon contributes effectively to: increasing pulse width, power decreasing, time jittering, and shape distortion. The time jittering means that the pulse center will shift to left or right. So that, time jittering leads to interference between neighboring pulses. On the other hand, increasing bit period will prevent the possibility of sending high rates. In this paper, an accurate mathematical analysis to increase the rates of transmission, which contain all physical random variables that contribute to determine the transmission rates, is presen
... Show MoreAt present, numerous novel chemical compounds face challenges related to their limited solubility in aqueous environments. These compounds are classified under the Biopharmaceutical Classification System (BCS) as either class II or class IV substances. Different carriers were used to increase their solubility. Candesartan cilexetil (CC) is one of the most widely used antihypertensive drugs, which belongs to class II drugs. The aim of this research was to enhance the solubility and dissolution rate of CC through a complexation approach involving β-cyclodextrin and its derivatives, specifically hydroxypropyl beta cyclodextrin (HP-β-CD), methyl beta cyclodextrin (M-β-CD), and sulfonyl ether beta-cyclodextrin (SBE-β-CD), serving as
... Show MoreThe development of a meaningful dissolution procedure for drug products with limited water solubility has been a challenge to both the pharmaceutical industry and the agencies that regulate them. Natural surfactants aid in the dissolution and subsequent absorption of drugs with limited aqueous solubility. In vitro, various techniques have been used to achieve adequate dissolution of the sparingly water – soluble or water insoluble drug products such as the use of mechanical methods (i.e., increased agitation and the disintegration method) or hydro alcoholic medium or large volumes of medium. The necessity of assuring the quality of drugs , especially those with low aqueous solubility and in vivo absorption , has led to the development and
... Show MoreEbastine (EBS) is a non-sedating antihistamine with a long duration of action. This drug has predominantly hydrophobic property causing a low solubility and low bioavailability. Surface solid dispersions (SSD) is an effective technique for improving the solubility and dissolution rate of poorly soluble drugs by using hydrophilic water insoluble carriers.
The present study aims to enhance the solubility and dissolution rate of EBS by using surface solid dispersion technique. Avicel® PH101, Avicel® PH 102, croscarmellose sodium(CCS) and sodium starch glycolate(SSG) were used as water insoluble hydrophilic carriers.
The SSD formulations of EBS were prepared by the solvent evaporation method in different drug: carrier
... Show MoreStudy of the development of an activated carbon nanotube catalyst for alkaline fuel cell technology. Through the prepared carbon nanotubes catalyst by an electrochemical deposition technique. Different analytical approaches such as X-ray diffraction (XRD) to determine the structural properties and Scanning Electron Microscope (SEM), were used to characterize, Mesh stainless steel catalyst substrate had an envelope structure and a large surface area. Voltages were also obtained at 1.83 V and current at 3.2 A of alkaline fuel cell. In addition, study the characterization of the electrochemical parameters.
In this paper had been studied the characterization of the nanocatalyst (NiO) Mesh electrodes. For fuel cell. The catalyst is prepared and also the electrodes The structural were studied through the analysis of X-ray diffraction of the prepared nanocatalyst for determining the yielding phase and atomic force microscope to identify the roughness of prepared catalyst surface, Use has been nanocatalyst led to optimization of cell voltage, current densities & power for a fuel cell.
Femtosecond laser pulse propagation in monomode optical fibers is demonstrated and investigated numerically (by simulations) and experimentally in this paper. A passively mode locked Nd:glass laser giving a pulse duration of about 200 fsec at 1053 nm wavelength and 120 mW average optical power with 100 MHz repetition rate is used in the experimental work. Numerical simulations are done by solving the nonlinear Schrödinger equation with the aid of Matlab program. The results show that self phase modulation (SPM) leads to compression of the spectral width from 5 nm to 2.1 nm after propagation of different optical powers (34, 43, 86 and 120 mW) in fibers of different length (5, 15, 35 m). The varying optical powers produced a varying
... Show More