The performance of flexible pavements is significantly impacted by the permanent deformation (rutting) of asphalt pavements. Rutting shortens the pavement's useful service life and poses significant risks to those using the highway since it alters vehicle handling characteristics.. The aim of this research is to evaluate the permanent deformation of asphalt mixtures under different conditions,to achieve this aim 108 cylindrical specimens has been prepared and tested under repeated loading in uniaxial compression mode. Five factors were considered in this research, these factors represent the effect of environmental condition and traffic loading as well as mixture properties, they include testing temperature, loading condition (stress level and duration), mixture properties (asphalt type and content). The permanent deformation is evaluated in term of the following parameters, accumulation of permanent strain, axial resilient micro strain, initial permanent strain (intercept, a), accumulation rate of permanent deformation (slope, b), rate of decrease in permanent deformation (α) and constant of proportionality between permanent and elastic strains (µ). Based on the repeated load test results, it was found that when the testing temperature increased from 20 to 40◦C, the permanent strain and intercept increased by a factor of 4.8 and 1.9, respectively. Further increase of the testing temperature from 40 to 60◦C, resulted in the permanent strain increment by a factor of 5.13 whereas the intercept by a factor 2.18. In addition, the test data shows the permanent strain value for load duration of 0.4 sec. is 1.64 times the value for 0.1 sec. Finally, the findings showed that the resilient response of the substance is comparatively more sensitive to asphalt content than the plastic response. Furthermore, the rutting resistance is highly affected by the variables considered in this research.
This investigation was undertaken to evaluate the effectiveness of using Hydrated lime as a (partial substitute) by weight of filler (lime stone powder) with five consecutive percentage namely (1.0, 1.5, 2.0, 2.5, 3.0) % by means of aggregate treatment, by introducing dry lime on dry and 2–3% Saturated surface aggregate on both wearing and binder coarse. Marshall design method, indirect tensile test and permanent deformation under repeated loading of Pneumatic repeated load system at full range of temperature (20, 40, 60) C0 were examined The study revealed that the use of 2.0% and 1.5 % of dry and wet replacement extend the pavement characteristics by improving the Marshall properties and increasing the TSR%. Finally, increase permanent
... Show MoreImplementation of Warm Mix Asphalt concrete (WMA) is getting global acceptance due to the restrictions for protecting the environment and the requirements to reduce fuel consumption. In this investigation, two WMA mixtures have been prepared in the laboratory using medium curing cutback (MC-30) and Cationic emulsion asphalt. Hot Mix Asphalt (HMA) was also prepared for comparison. The cylinder specimens (63.5mm) in height and (101.6mm) in diameter were constructed from the mixtures and subjected to indirect tensile strength test to determine the Tensile Strength Ratio (TSR). The cylinder specimens of (101.6mm) in height and (101.6mm) in diameter were also constructed from those mixtures and subjected to static compressive
... Show MoreOne of the most essential components of asphalt pavements is the filler. It serves two purposes. First, this fine-grained material (diameter less than 0.075 mm) improves the cohesiveness of aggregate with bitumen. Second, produce a dense mixture by filling the voids between the particles. Aluminum dross (AD), which is a by-product of aluminum re-melting, is formed all over the world. This material causes damage to humans and the environment; stockpiling AD in landfills is not the best solution. This research studies the possibility of replacing part of the conventional filler with aluminum dross. Three percent of dross was used, 10, 20, and 30% by filler weight. The MarshallMix design method was adopted to obtain the op
... Show MoreRecycled asphalt concrete mixture are prepared, artificially aged and processed in the laboratory to maintain the homogeneity of recycled asphalt concrete mixture gradation, and bitumen content. The loose asphalt concrete mix was subjected to cycle of accelerated aging, (short –term aging) and the compacted mix was subjected to (long -term aging) as per Super-pave procedure. Twenty four Specimens were constructed at optimum asphalt content according to Marshall Method. Recycled mixture was prepared from aged asphalt concrete using recycling agent (soft asphalt cement blended with silica fumes) by (1.5%) weight of mixture as recycling agent content. The effect of recycling agent on aging after recycling process behavior
... Show MoreFailure in asphalt mixture and distress in pavement are major issues to roads infrastructure. Selecting an appropriate chemical composition of asphalt cement is a key component in avoiding these issues. This work aimed to investigate the effect of the chemical composition of different polar fractions on the rheological and physical properties of asphalt cement. Four types of asphalt cement with penetration grades of 20/30, 40/50, 60/70 and 85/100 were divided into four fractions. Complex shear modules, rutting resistance and rotational viscosity of the asphalt cement were determined by using a Dynamic Shear Rheometer and a Rotation Viscometer, respectively. The results show that an increase in the asphaltene content and Gastel index resulte
... Show MorePermanent deformation, fatigue and thermal cracking are the three typical distresses of flexible pavement. Using hydrated lime (HL) into the conventional limestone mineral additive has been widely practiced, including in Europe, to improve the mechanical properties of hot mix asphalt (HMA) concrete and as the result the durability of the constructed pavement. Large number of experimental studies have been reported to find the optimum addition of HL for the improvement on HMA concrete mechanical properties, moisture susceptibility and fatigue resistance. Pavement in service is under complex thermomechanical stress-strain conditions due to coupled atmospheric and surrounding environment temperature variation and the traffic loading. To predic
... Show MoreKombucha(Khubdat Humza) is composed of yeast and acetic acid bacteria especially, Acetobacter xylinum which forms a cellulose pellicle on tea broth. Kombucha(Khubdat Humza) produces bacterial cellulose pellicles, with unique purity and fine structure. It can be used in many forms, such as an emulsifier, stabilizer, dispersing agent, thickener and gelling agent but these are generally subsidiary to its most important use of holding on to water. Recently, bacterial cellulose is used in many special applications such as a scaffold for tissue engineering of cartilages and blood vessels, also for artificial skin for temporary covering of wounds, as well as its used in the clothing industry. The yield of cellulose produced were investiga
... Show MoreLaboratory experience in Iraq with cold asphalt concrete mixtures is very limited. The design and use of cold mixed asphalt concrete had no technical requirements. In this study, two asphalt concrete mixtures used for the base course were prepared in the laboratory using conventional cold-mixing techniques to test cold asphalt mixture (CAM) against aging and moisture susceptibility. Cold asphalt mixtures specimens have been prepared in the lab with cutback and emulsion binders, different fillers, and curing times. Based on the Marshal test result, the cutback proportion was selected with the filler, also based on the Marshal test emulsion. The first mixture was medium setting cationic emulsion (MSCE) as a binder, hydrate
... Show More