Purpose: This study aimed to assess the thickness of alveolar bone of maxillary and mandibular incisors from orthodontics perspective. Materials and Method: A total of 73 Cone beam computed tomography for Iraqi patients (47 females and 26 males) were included in this study. The selected images were captured and imported to AutoCAD database software to perform the measurement. To measure alveolar bone thickness, a reference line was drawn through the long axis of each incisor, from the incisal edge to the root apex. Then, labial and lingual/palatal perpendicular lines were drawn to the reference line at 3, 6, and 9mm apically from the cemento-enamel junction (CEJ). Results: The buccal bone is generally thinner than the lingual/palatal bone. The bone gets relatively thicker closer to the apex. The buccal bone for all lower incisors was less than 1 mm at 3- and 6-mm distance. It was slightly thicker at the central incisor as compared to the lateral at 9-mm distance. Genders have a difference in the thickness of the palatal alveolar bone in their right and left lateral incisors, which are 3mm and 9mm, respectively. Alveolar bone thickness is significantly positively correlated with several teeth. Conclusions: Males and females in this study showed comparable alveolar bone thickness. The alveolar bone thickness increased with increasing age. It is essential to assess the thickness of alveolar bone pre-orthodontic treatment (especially for patients with thin biotype, and those cases that involve labial proclination of the lower incisors).
Find cares studying ways in the development of industrial products and designs: the way the progressive development (how typical) and root development (jump design), was the aim of the research: to determine the effectiveness of the pattern and the jump in the development of designs and industrial products. After a process of analysis of a sample of research and two models of contemporary household electrical appliances, it was reached a set of findings and conclusions including:1-leaping designs changed a lot of entrenched perceptions of the user on how the product works and its use and the size and shape of the product, revealing him about the possibilities of sophisticated relationships with the product, while keeping the typical desi
... Show MoreAbstract Rasha Hameid Jehad Baghdad University Background: The high reactivity of hydrogen peroxide used in bleaching agents have raised important questions on their potential adverse effects on physical properties of restorative materials. The purpose of this in vitro study was to evaluate the effect of in-office bleaching agents on the microhardness of a new Silorane-based restorative material in comparison to methacrylate-based restorative material. Materials and method: Forty specimens of Filtek™ P90 (3M ESPE,USA) and Filtek™ Supreme XT (3M ESPE, USA) of (8mm diameter and 3m height) were prepared. All specimens were polished with Sof-Lex disks (3M ESPE, USA). All samples were rinsed and stored in incubator 37˚C for 24 ho
... Show MoreThis study depicts the removal of Manganese ions (Mn2+) from simulated wastewater by combined electrocoagulation/ electroflotation technologies. The effects of initial Mn concentration, current density (C.D.), electrolysis time, and different mesh numbers of stainless steel screen electrodes were investigated in a batch cell by adopting Taguchi experimental design to explore the optimum conditions for maximum removal efficiency of Mn. The results of multiple regression and signal to noise ratio (S/N) showed that the optimum conditions were Mn initial concentration of 100 ppm, C.D. of 4 mA/cm2, time of 120 min, and mesh no. of 30 (wire/inch). Also, the relative significance of each factor was attained by the analysis of variance (ANO
... Show MoreThis study depicts the removal of Manganese ions (Mn2+) from simulated wastewater by combined electrocoagulation/ electroflotation technologies. The effects of initial Mn concentration, current density (C.D.), electrolysis time, and different mesh numbers of stainless steel screen electrodes were investigated in a batch cell by adopting Taguchi experimental design to explore the optimum conditions for maximum removal efficiency of Mn. The results of multiple regression and signal to noise ratio (S/N) showed that the optimum conditions were Mn initial concentration of 100 ppm, C.D. of 4 mA/cm2, time of 120 min, and mesh no. of 30 (wire/inch). Also, the relative significance of each factor was attained by the analysis
... Show MoreBackground: This in vitro study was carried out to evaluate the effects of various veneering dentin ceramic thicknesses and repeated firings on the color of lithium disilicate glass-ceramic (IPS e.max Press) and zirconium-oxide (IPS ZirCAD) all-ceramic systems, measured by clinical spectrophotometers (Easyshade Advance 4.0) . Materials and methods: The 72specimens cube-shaped have the dimension of about 11 mm in width, 14 mm in length, 1mm in thickness, these cores divided into 3 groups according to the type of material each group have (24)core specimens. Each group had been divided into three sub-groups (each having 8 specimens) according to veneering with dentin ceramic thicknesses: as 0.5, 1, or 2 mm (n=8). IPS e.max press and ZirCAD c
... Show MoreABSTRACT Background:- White spot lesions are common esthetic problem that compromise the success of orthodontic treatment. This study aimed to assess white spot lesions in patients with fixed orthodontic appliance at different time intervals. Materials & Methods:- Thirty two patients (24 females and 8 males) were included in this study and they underwent clinical examination for white spot lesions using enamel decalcification index at four time intervals: (2-3 weeks after appliance insertion, 2, 4 and 6 months). Results:- The patients were free of white spot lesions at the appliance insertion visit. The mean of white spot lesions was 2.22 which were increased significantly during six months to reach 24.59 at the end of study. There was a si
... Show MoreObjective To evaluate recently developed acidic calcium-phosphate (CaP) pastes as conservative enamel-conditioning systems for bracket bonding and investigate their effects on the shear bond strength, adhesive residues, and enamel damage in comparison to a conventional 37 % phosphoric acid (PA) gel. Materials and methods Two experimental etchant pastes consisting of hydroxyapatite and monocalcium phosphate monohydrate were prepared by mixing them with 37 % and 10 % PA solutions, respectively. These were characterized using X-ray diffraction. Metal brackets were bonded to 90 freshly extracted human premolars and assigned to three groups, depending on etchant type: 37 % PA-gel (control) and the two experimental (HPA and MPA) pastes. Shear bon
... Show MoreBackground: The ideal force-delivery system must: provide optimal tooth moving forces that elicit the desired effects, be comfortable and hygienic for the patient, require minimal operator manipulation and patient cooperation and provide rapid tooth movement with minimal mobility during orthodontic therapy, the elastomeric chains have the greatest potential to fulfill these requirements. Materials and Methods: This in vitro study was designed to determine the effect of three different mechanisms for canine retraction : (6-3 , 6-5-3 and chain loop ) on the load relaxation behavior of three types of elastomeric chains : (maximum clear , maximum silver and extreme silver) from the same company (Ortho Technology company) with two different bran
... Show MoreBackground: The purpose of this study was to evaluate the effect of in vitro long-term simulation of oral conditions on the bond strength of PEEK CAD/CAM lingual retainers.
Material and methods: The sample consisted of 12 PEEK CAD/CAM retainers each composed of 2 centrally perforated 3x4mm pads joined by a connector. They were treated by 98% sulfuric acid for 1 minute and then conditioned with Single Bond Universal and bonded to the lingual surface of premolar teeth by 3M Transbond TM System. Half of the retainers were artificially aged using a 30-day water storage and 5000 thermocycling protocol before bond strength testing to compare with the non-aged specimens.
Results: The artificially aged retainers showed a marginally
... Show More