The cost-effective carbon cross-linked Y zeolite nanocrystals composite (NYC) was prepared using an eco-friendly substrate prepared from bio-waste and organic adhesive at intermediate conditions. The green synthesis method dependent in this study assures using chemically harmless compounds to ensure homogeneous distribution of zeolite over porous carbon. The greenly prepared cross-linked composite was extensively characterized using Fourier transform infrared, nitrogen adsorption/desorption, Field emission scanning electron microscope, Dispersive analysis by X-ray, Thermogravimetric analysis, and X-ray diffraction. NYC had a surface area of 176.44 m2/g, and a pore volume of 0.0573 cm3/g. NYC had a multi-function nature, sustained at a long-exposure time during the adsorption process of methyl violet dye (MV) from aqueous solutions and achieved higher removal at normal temperature and pH. The Halsey and the Langmuir models were the most appropriate models for representing the equilibrium data with a maximum adsorption capacity of 108.7 mg/g. The kinetic studies showed that the pseudo-second-order kinetics model and Elovich model were the most suitable models to describe the experimental data which indicated the MV adsorption by NYC has a chemical nature. Also, the interpretation of data by the Boyd model demonstrated that the adsorption process of MV was determined by both film diffusion and intra-particle diffusion. The adsorption process of MV by NYC is spontaneous, feasible, and exothermic. The regeneration performance showed that the NYC can be easily regenerated and reused with keeping an acceptable performance until the fourth cycle. Eventually, this study confirmed that the greenly prepared composite can serve as an adorable adsorbent for the removal of cationic dyes such as methyl violet under mild conditions.
The removal of boron from aqueous solution was carried out by electrocoagulation (EC) using magnesium electrodes as anode and stainless steel electrodes as cathode. Several operating parameters on the removal efficiency of boron were investigated, such as initial pH, current density, initial boron ion concentration, NaCl concentration, spacing between electrodes, electrode material, and presence of carbonate concentration. The optimum removal efficiency of 91. 5 % was achieved at a current density of 3 mA/cm² and pH = 7 using (Mg/St. St. ) electrodes, within 45 min of operating time. The concentration of NaCl was o. 1 g/l with a 0.5cm spacing between the electrodes. First and second order rate equation were applied to study adsorp
... Show MoreThe nanostructured Manganese dioxide/Carbon fiber (CF) composite electrode was prepared galvanostatically using a facile method of anodic electrodeposition by varying the reaction time and MnSO4 concentration of the electrochemical solution. The effects of these parameters on the structures and properties of the prepared electrode were evaluated. For determining the crystal characteristics, morphologies, and topographies of the deposited MnO2 films onto the surfaces of carbon fibers, the X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), and atomic force microscopy (AFM) techniques were used, respectively. It found that the carbon fibers were coated with γ-MnO2 with a density that increased with increasing the de
... Show MoreThe removal of turbidity from produced water by chemical coagulation/flocculation method using locally available coagulants was investigated. Aluminum sulfate (alum) is selected as a primary coagulant, while calcium hydroxide (lime) is used as a coagulant aid. The performance of these coagulants was studied through jar test by comparing turbidity removal at different coagulant/ coagulants aid ratio, coagulant dose, water pH, and sedimentation time. In addition, an attempt has been made to examine the relationship between turbidity (NTU) and total suspended solids (mg/L) on the same samples of produced water. The best conditions for turbidity removal can be obtained at 75% alum+25% lime coagulant at coagulant dose of 80 m
... Show MoreCertain cyclic amine derivatives of metronidazole via acetate spacer were prepared. Cyclic amines used are piperidine and piperazine to improve the physicochemical properties and reduce some of metronidazole side effects. This is believed to be done by modification of its structural features to get prodrugs with improved properties over that of metronidazole. The present work includes esterification of metronidazole with choroacetic acid, N-alkylation of the cyclic amines by the halogenated ester and characterization of their structures by spectral(UV and IR) and elemental(CHN)analysis.The melting points, degree of solubilities and partition coefficients were also determined. Both metronid
... Show MoreAbstract
Nano-crystalline ZSM-5 zeolite was synthesized by hydrothermal method using chelating agent and two gel compositions:Compositionɪ:Al2O3:86SiO2:5.5TPA:12.7Na2O:3.4Trien:3320H2O.Compositionɪɪ:Al2O3:68SiO2:5.4TPA:10Na2O:2.6Trien:2626H2O.Study of hydrothermal reaction factors on characteristics of nano- sized zsm-5 has been carried on ,among them are crystallization temperature, crystallization time and concentration of template ( TPAOH ) solution. Synthesis was accomplished in PTFE lined autoclave ( reactor ) . The product were characterized by X-ray diffraction ( XRD ),Atomic force microsc
... Show More5-((2,4-dibromo-6-((cyclohexyl(methyl)amino)methyl)phenyl)diazenyl)quinolin-8-ol azo ligand (L) has been synthesized through the reaction of diazonium salt for 2,4-dibromo-6-((cyclohexyl(methyl)amino)methyl)aniline with 8-hydroxyquinoline. The azo ligand (L) was characterized utilizing spectroscopic techniques, including FTIR, UV-Vis, 1H and 13C NMR, as well as mass spectrometry and micro-elemental analysis (C.H.N). Metal complexes containing Co(II), Ni(II), Cu(II), and Zn(II) were synthesized and analyzed through mass spectrometry, flame atomic absorption, elemental analysis (C.H.N), infrared and UV-Vis spectroscopy, along with measurements of conductivity and magnetic properties. The experimental findings suggested that all met
... Show MoreIn this work, the nano particles of Na-A zeolite were synthesized by sol –gel method. The samples were characterized by X-ray diffraction (XRD), X-ray luorescence (XRF), Surface area and pore volume, Atomic Force Microscope (AFM) and Fourier Transform Infrared Spectroscopy (FTIR). Results show that the nano A zeolite is with average crystal size is 74.77 nm., Si/Al ratio 1.03, BET surface area was 581.211m2/g and the pore volume for NaA was found equal to 0.355cm3/g.