Carbon fibre reinforced polymers are widely used to strengthen steel structural elements. These structural elements are normally subjected to static, dynamic and fatigue loadings during their life-time. A number of studies have focused on the characteristics of CFRP sheets bonded to steel members under static, dynamic and fatigue loadings. However, there is a gap in understanding the bonding behaviour between CFRP laminates and steel members under impact loading. This paper shows the effect of different load rates from quasi-static to 300 × 103 mm/min on this bond. Two types of CFRP laminate, CFK 150/2000 and CFK 200/2000, were used to strengthen steel joints using Araldite 420 epoxy. The results show a significant bond strength enhancement under impact loading, whereas the high loading rates have little influence on the effective bond length.
loaded reinforced concrete circular short columns. An experimental investigation into the behavior
of 24 short reinforced concrete columns with and without steel fibers was carried out. The columns
had a circular section (200 mm diameter and 900 mm long). Test variables include concrete
strength, spacing of spiral reinforcement, and inclusion of steel fibers. The axial stress and axial
strains were obtained and used to evaluate the effects of the presence of steel fibers. It was found
that the addition of steel fibers slightly improves the load carrying capacity of the tested columns
whereas it significantly enhances the ductility of these specimens. Test results also indicated that for
the same confinement parameter
Potentiostatic polarization and weight loss methods have been used to investigate the corrosion behavior of carbon steel in sodium chloride solution at different concentrations (0.1, 0.4 and 0.6) M under the influence of temperatures ( 293, 298, 303, 308 and 313) K. The inhibition efficiency of the amoxicillin drug on carbon steel in 0.6 M NaCl has also been studied based on concentration and temperature. The corrosion rate showed that all salt concentrations ( NaCl solution) resulted in corrosion of carbon steel in varying ratio and 0.6 M of salt solution was the highest rate (50.46 g/m².d). The results also indicate that the rate of corrosion increases at a temperature of 313 K.. Potentiodynamic polarization studi
... Show MoreIn this research a theoretical study has been carried out on the behavior and strength of simply supported composite beams strengthened by steel cover plate taking into consideration partial interaction of shear connectors and nonlinear behavior of the materials and shear connectors. Following the procedure that already has been adopted by Johnson (1975), the basic differential equations of equilibrium and compatibility were reduced to single differential equation in terms of interface slip between concrete slab and steel beam. Furthermore, in order to consider the nonlinear behavior of steel, concrete and shear connectors, the basic equation was rearranged so that all terms related to materials are isol
... Show MoreIn this study, the effect of fire flame on the punching shear strength of steel fiber reinforced concrete flat plates was experimentally investigated using nine half-scale specimens with dimensions of 1500×1500 mm and a total thickness of 100 mm. The main investigated variables comprised the steel fiber volume fraction 0, 1, and 1.5% and the burning steady state temperature 500 and 600 °C. The specimens were divided into three groups, each group consists of three specimens. The specimens in the first group were tested with no fire effect to be the reference specimens, while the others of the second and third groups were tested after being exposed to fire-flame effect. The adopted characteristics of the fire test were; (one hour) b
... Show MoreABSRTACT Background: Soft liner material is become important in dental prosthetic treatment. They are applied to the surface of the dentures to achieve more equal force distribution , reduce localized pressure and improve denture retention by engaging undercut . So the aim of the study is to evaluate the effect of different surface treatment by air-abrasion AL2O3 and laser treatment with CO2 laser on improving the shear bond strength of the denture liner to acrylic denture base material . Materials and methods: the 30 specimens of heat cured acrylic denture base material (high Impact acrylic )and heat cured soft liner (Vertex ,Nether Lands )were prepared for this study .They were designed and divided according to type of the s
... Show MoreAim: To evaluate the effect of ultrasonic agitation for retrograde biodceramic root repair, MTA and biodentine filling materials on push-out bond strength to dentine walls. Materials and Methods: Ninety extracted human teeth with single straight roots were selected randomly. After disinfection and cleaning, the coronal portions were sectioned to standardize the root canal length at 15mm. following root canal shaping, obturation and apical roots resection, retrograde cavities were prepared. Teeth were categorized depending on the filling material used into three groups, 30 teeth each. Group A filled with bioceramic root repair material, B with MTA and C with Biodentine material. These groups were divided in to three subgroup (n= 10). Subgrou
... Show MoreThis study examines the impact of different curing methods on the compressive strength of concrete. It investigates techniques such as air curing, periodic water spraying, full water submersion, and polyethylene encasement. Artificial neural network models were employed to evaluate the compressive strength under each curing condition. A model for calculating compressive strength that considers surrounding conditions was created using an artificial neural network. The current study’s figures were generated using this model. The research thoroughly examined the impact of curing environments and concrete mix components on strength properties, taking into account factors such as tempera