Permanent deformation, fatigue and thermal cracking are the three typical distresses of flexible pavement. Using hydrated lime (HL) into the conventional limestone mineral additive has been widely practiced, including in Europe, to improve the mechanical properties of hot mix asphalt (HMA) concrete and as the result the durability of the constructed pavement. Large number of experimental studies have been reported to find the optimum addition of HL for the improvement on HMA concrete mechanical properties, moisture susceptibility and fatigue resistance. Pavement in service is under complex thermomechanical stress-strain conditions due to coupled atmospheric and surrounding environment temperature variation and the traffic loading. To predict and analyse the performance of pavement structures the data only from uniaxial compressive test for the resilient modulus and permanent deformation would be not enough. However, so far, the data of HL modified HMA concrete under complex loading conditions are still not well informatively complete. To contribute new knowledge, this paper reports an experimental study of both uni- and tri-axial tests for the asphalt concrete using HL into mineral additive for the mixes designed for the applications of wearing, levelling, and base layers, respectively. All the tests were conducted under three controlled temperatures and four stress deviations. The test results have showed that, for all three types of mixes, the permanent deformation of the HL mixes is less than the ones of no HL addition. The degree of the improvement on permanent deformation resistance using HL is much pronounced at high stress deviation states. The results have also showed that the resilient modulus strongly depends on the temperature and stress deviation while the mixes of HL addition demonstrate higher rigidity. At last, mathematical characterization models have been proposed for the measured material properties. A numerical simulation case study has been performed to test and demonstrate the application of the proposed unified property model
In this work, silver (Ag) self-metallization on a polyimide (PI) film was prepared through autocatalytic plating. PI films were prepared through the solution casting method, followed by etching with potassium hydroxide (KOH) solution, sensitization with tin chloride (SnCl2), and the use of palladium chloride (PdCl2) to activate the surface of PI. Energy-dispersive X-ray analysis (EDX) showed the highest peak in the (Ag) region and confirmed the presence of AgNPs. The diffraction peaks at 2θ = 38.2°, 44.5°, 64.6°, and 78.2° represented the 111, 200, 220, and 311 planes of Ag, respectively. The FT–IR an
... Show MoreThe purpose of present work is to study the relationship of the deformed shape of the nucleus with the radioactivity of nuclei for (Uranium-238 and Thorium-232) series. To achieve our purposes we have been calculated the quadruple deformation parameter (β2) and the eccentricity (e) and compare the radioactive series with the change of the and (e) as indicator for the changing in the nucleus shape with the radioactivity. To obtain the value of quadruple deformation parameter (β2), the adopted value of quadruple transition probability B (E2; 0+ → 2+) was calculated from Global Best fit equation. While the eccentricity (e) was calculated from the values of the minor and major ellipsoid axis’s (a & b). From the results, it is obvi
... Show MoreThe removal of turbidity from produced water by chemical coagulation/flocculation method using locally available coagulants was investigated. Aluminum sulfate (alum) is selected as a primary coagulant, while calcium hydroxide (lime) is used as a coagulant aid. The performance of these coagulants was studied through jar test by comparing turbidity removal at different coagulant/ coagulants aid ratio, coagulant dose, water pH, and sedimentation time. In addition, an attempt has been made to examine the relationship between turbidity (NTU) and total suspended solids (mg/L) on the same samples of produced water. The best conditions for turbidity removal can be obtained at 75% alum+25% lime coagulant at coagulant dose of 80 m
... Show MoreIn the present work, a d.c. magnetron sputtering system was designed and fabricated. The chamber of this system was includes from two copper coaxial cylinders where the inner one used as a cathode (target) while the outer one used as the anode with Solenoid magnetic coil located on the outer cylinder (anode). The axial profile of magnetic field for various coil current (from 2A to 14 A) are shown. The plasma characteristics in the normal glow discharge region are diagnostics by the 2.2mm diameter Langmuir probe with different length along the cathode and located at different radial positions 1cm and 2cm from the cathode surface. The result of this work shows that, the electron energy distributions at different radial positions along the
... Show MoreThe five-a- Side Soccer for simple mental disability is as interesting and caring as many other sporting events. Therefore, the researchers believe that their basic skills tests are compatible with then level of the tested individuals in terms of age and mental ability. As a means of selecting those who are qualified to practice this game in a simple way, the problem of research has been identified in the design and standardization of two scoring skills that belong to this category and are approved by the training staff during the initial selection process. The research community is determined by people with mental disabilities who belong to the governmental and private institutes and the Special Olympics Union in Baghdad and for the year 2
... Show MoreThirty nine (12.8%) isolates of Staphylococcus aureus were isolated from 304 healthy human (Nasal swabs). It was found that percentage of males that have S. aureus is more than female's percentage. These isolates (39) were tested with different tests. Twenty seven isolates (69.23 %) were positive for Staphylococcus protein —A (SPA) ,thirty seven ( 94.8 %) were positive for tube coagulase , thirty five ( 89.7 % ) were positive with clumping factor and thirty two ( 82.05 %) had 13 — hemolytic on blood agar. It was found that 100% of the isolates (39 isolates) were positive with one, two or three tests (tube coagulase, clumping factor and SPA).
To achieve sustainability, use waste materials to make concrete to use alternative components and reduce the production of Portland cement. Lime cement was used instead of Portland cement, and 15% of the cement's weight was replaced with silica fume. Also used were eco-friendly fibers (copper fiber) made from recycled electrical. This work examines the impact of utilizing sustainable copper fiber with different aspect ratios (l/d) on some mechanical properties of high-strength green concrete. A high-strength cement mixture with a compressive strength of 65 MPa in line with ACI 211.4R was required to complete the assignment. Copper fibers of 1% by volume of concrete were employed in mixes with four different aspect ratios
... Show MoreFor design purposes, it`s necessary to know the compression rate of soil layers which might be happened when it`s subjected to effective stresses. Also, it`s essential to know the rate of flow through soil mass specially for the design of marine structures or earth embankment. These two important behavior could be predicted from the coefficient of consolidation (Cv) and the coefficient of permeability (k). This study shows the effect of cutback asphalt stabilization on Cv and k and other compressibility factors, the investigation was done for silty clay samples, specimens were prepared by mixing the soil with different percentage of asphalt from (0-10)% and subjected to one-dimensional consolidation test of 50mm diameter and 20mm height wer
... Show MoreMoisture damage is one of the most significant troubles that destroy asphaltic pavement and reduces road serviceability. Recently, academics have noticed a trend to utilize fibers to enhance the efficiency of asphalt pavement. This research explores the effect of low-cost ceramic fiber, which has high tensile strength and a very high thermal insulation coefficient, on the asphalt mixture's characteristics by adding three different proportions (0.75%, 1.5%, and 2.25%). The Marshall test and the Tensile Strength Ratio Test (TSR) were utilized to describe the impact of ceramic fiber on the characteristics of Marshall and the moisture susceptibility of the hot mix asphalt mixture. The Field Emission Scanning Electron Microsc
... Show More