Impact of a mixture of nanofiller and intrinsic pigment on tear strength and hardness of two types of maxillofacial silicone elastomers
...Show More Authors

Background: The ideal maxillofacial prosthesis should have fine and thin boundaries that bindwith the surrounding facial structures and possess high tear strength.This study aims to determinethe best percentages of nanofiller (TiO2) and intrinsic pigment (silicone functional intrinsic) thatcould be mixed in as additives to improve the tear strength of Cosmesil M511 andVST50F siliconeelastomers with the least effect on their hardness.Materials and Methods: In this in vitro experimental study, a total of 80 samples, 40 for eachelastomer, were fabricated. Each elastomer sample was split into two equal groups to test for tearstrength and Shore A hardness. Each group consisted of 20 samples, including 10 control sampleswithout additives and 10 experimental samples with additives (mixtures of 0.2 wt% nano‑TiO2 + 0.25wt% intrinsic pigment and 0.25 wt% nano‑TiO2 + 0.25 wt% intrinsic pigment for the CosmesilM511 and VST50F silicone elastomers, respectively).Two‑way ANOVA and Tukey test were usedfor comparison; P < 0.05 was considered statistically significant.Results: Significant differences in tear strength were found among all tested groups (P < 0.05).The tear strength of the experimental subgroups significantly increased compared with the controlsubgroups (P < 0.05). Significant differences in Shore A hardness were also observed among alltested groups (P < 0.05) except between the experimental subgroups of both materials, where anonsignificant difference was obtained (P > 0.05).Conclusion: Incorporation of select percentages of TiO2 nanofiller and intrinsic pigment intoCosmesil M511 andVST50F silicone elastomers yields improvements in tear strength with a slightincrease in hardness (PDF) Impact of a mixture of nanofiller and intrinsic pigment on tear strength and hardness of two types of maxillofacial silicone elastomers. Available from: https://www.researchgate.net/publication/343647971_Impact_of_a_mixture_of_nanofiller_and_intrinsic_pigment_on_tear_strength_and_hardness_of_two_types_of_maxillofacial_silicone_elastomers [accessed Apr 05 2023].

Scopus Crossref
View Publication
Publication Date
Fri May 01 2020
Journal Name
European Journal Of General Dentistry
Effect of plant-extract disinfectant solutions on the specific properties of reinforced maxillofacial silicone elastomers with nanofiller and intrinsic pigment
...Show More Authors
Abstract<p> Objective This study aimed to evaluate the effects of disinfectant solutions, namely, the alcoholic extract of Salvadora persica L. (A1 = 10% and A2 = 15%) and chlorhexidine digluconate (A3 = 2%), on the tear strength and hardness of room temperature vulcanizing (RTV) VST50F and heat temperature vulcanizing (HTV) Cosmesil M511 silicone elastomers before and after reinforcement with nanofillers (TiO2) and intrinsic pigment. Materials and Methods: A total of 320 specimens were prepared, with 160 specimens each for RTV and HTV silicone. Forty specimens were evaluated before disinfection and divided into two equal groups, namely, control (without additive) and experimental (with ad</p> ... Show More
View Publication
Scopus (4)
Crossref (5)
Scopus Crossref
Publication Date
Fri Dec 01 2017
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of Polyamide (Nylon 6) Micro-Particles Incorporation into RTV Maxillofacial Silicone Elastomer on Tear and Tensile Strength
...Show More Authors

View Publication
Crossref (6)
Crossref
Publication Date
Fri Dec 15 2017
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of Polyamide (Nylon 6) Micro-Particles Incorporation into RTV Maxillofacial Silicone Elastomer on Tear and Tensile Strength
...Show More Authors

Background: The longevity of any prosthesis depends on the materials from which it was fabricated, that is why, defects in the material properties may reduce the service life of prosthesis and necessitate its replacement. The aim of this study was to evaluate the effect of adding different concentrations of Polyamide-6 (Nylon-6) on the tear and tensile strength of A-2186 RTV silicone elastomer. Materials and Methods: 80 samples were fabricated by the addition of 0%, 1%, 3% and 5% by weight PA-6 micro-particles powder to A-2186 platinum RTV silicone elastomer. The study samples were divided into four (4) groups, each group containing 20 samples. One control group was prepared without PA-6 micro particles and three experimental groups were pr

... Show More
View Publication Preview PDF
Crossref (6)
Crossref
Publication Date
Fri Jun 01 2018
Journal Name
Journal Of Taibah University Medical Sciences
Effect of nano-titanium oxide addition on some mechanical properties of silicone elastomers for maxillofacial prostheses
...Show More Authors

Objective This study evaluated the effects of adding titanium oxide (TiO2) nanofillers on the tear strength, tensile strength, elongation percentage, and hardness of room-temperature-vulcanized (RTV) VST50F and high-temperature-vulcanized (HTV) Cosmesil M511 maxillofacial silicone elastomers. Methods Two types of maxillofacial elastomers, VST50F RTV and Cosmesil M511 HTV, were used. Nano-TiO2 powder was applied as a nanofiller. A total of 120 specimens were fabricated, 60 each of VST50F and Cosmesil M511. The specimens of each type of elastomer were divided into three equal groups on which tests were conducted for tear strength, tensile strength, and hardness i.e., 20 specimens were used for each test. Each group of 20 specimens was further

... Show More
View Publication
Scopus (24)
Crossref (8)
Scopus Clarivate Crossref
Publication Date
Sat Dec 01 2018
Journal Name
Future Dental Journal
Studying some mechanical properties of maxillofacial silicone elastomer before and after incorporation of intrinsic pigments and artificial aging
...Show More Authors

Objective Advantageous properties of silicone elastomer made it one of the favorable materials in maxillofacial prosthesis construction, but these properties may change after months of usage or after pigments addition. This study aimed to define the optimum concentration for a mixture of two types of intrinsic pigments that added to VST-50 maxillofacial silicone material and study their effects on mechanical properties before and after artificial aging. Methods After the pilot study was conducted, 0.1% by weight of rayon flocking and 0. 2% by weight of burnt sienna intrinsic pigment concentration was selected because of improvement in tested mechanical properties of VST-50 maxillofacial silicone. A total of one hundred and eighty samples we

... Show More
View Publication
Crossref (2)
Crossref
Publication Date
Mon Oct 01 2018
Journal Name
The Saudi Dental Journal
Evaluation of some mechanical properties of a new silicone elastomer for maxillofacial prostheses after addition of intrinsic pigments
...Show More Authors

Objective: The approximate life span of a silicone maxillofacial prosthesis is as short as1.5–2 years of clinical service, then a new prosthesis should be fabricated. The most common reasonfor re-making the prosthesis is silicone mechanical properties degradation. The aim of this studywas to assess some mechanical properties of VST-30 silicone for maxillofacial prostheses after addi-tion of intrinsic pigments.Methods: Two types of intrinsic pigments (rayon flocking and burnt sienna); each of them wasincorporated into silicone. One hundred and twenty samples were prepared and split into 4 groupsaccording to the conducted tests (tear strength, hardness, surface roughness, and tensile strengthand elongation percentage) with 30 samples for ea

... Show More
View Publication
Scopus (18)
Crossref (17)
Scopus Clarivate Crossref
Publication Date
Sat Jul 01 2023
Journal Name
Journal Of Taibah University Medical Sciences
Impact of nano-cellulose fiber addition on physico-mechanical properties of room temperature vulcanized maxillofacial silicone material
...Show More Authors

Objectives: Maxillofacial silicone is used to restore abnormalities due to congenital or acquired causes. However, the quality of silicone is far from ideal. This study was aimed at assessing the influence of the addition of cellulose nanofibers (CNFs; several nanometers wide and 2-5 micro m long) on the physical and mechanical characteristics of maxillofacial silicone elastomers. Methods: Two CNF weight percentages (0.5% and 1%) were tested, and 180 specimens were divided into one control and two experimental groups. Each group was subdivided into six subgroups. In each subgroup, ten specimens subjected to each of the following tests: tearing strength, Shore-A hardness, tensile strength, elongation percentage, surface roughness, and color

... Show More
View Publication
Scopus (1)
Crossref (1)
Scopus Clarivate Crossref
Publication Date
Sat Sep 01 2018
Journal Name
International Journal Of Medical Research & Health Sciences
Effect of Silver-Zinc Zeolite Addition on Mechanical Properties of Maxillofacial Silicone
...Show More Authors

Background: Deterioration of maxillofacial silicone properties due to microbial colonization is a common problem and leads to the replacement of the prosthesis. Incorporation of the antimicrobial agent into the silicone could be a solution. The purpose of this study was to evaluate the effect of silver-zinc zeolite addition on some mechanical properties of a maxillofacial silicone (VST-50). Materials and methods: Total 120 specimens were fabricated and divided into 3 groups: 40 specimens for tear strength test, 40 specimens for tensile and percentage of elongation tests and 40 specimens for Shore A hardness and surface roughness. Each group was divided into 4 subgroups according to the amount of zeolite added (0% “control”, 0.5%, 1% and

... Show More
View Publication Preview PDF
Publication Date
Wed Dec 14 2016
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of Disinfection on Some Properties of Heat-Vulcanized Maxillofacial Silicone Elastomer Reinforced by Nano Silicone Dioxide
...Show More Authors

Background: The daily cleaning routine of the silicone maxillofacial prostheses by the patient may cause some alteration in the materials properties. The purpose of the present study was to investigate the effect of different disinfection procedures on some properties of silicon dioxide reinforced Cosmesil M511 HTV maxillofacial silicone. Materials and Methods: One hundred and sixty (160) specimens were prepared by mixing 5% SiO2 nano particles and 0.5% intrinsic cream color into the silicone polymer according to manufacturer's instructions. Specimens were divided into 4 groups according to the performed test (tear strength, surface hardness, surface roughness and color) with 40 specimens each. Each group was further subdivided according to

... Show More
View Publication Preview PDF
Crossref (7)
Crossref
Publication Date
Fri Jan 01 2021
Journal Name
Materials Today: Proceedings
Evaluation of mechanical properties and cytotoxicity of maxillofacial silicone material after incorporation of zirconia nanopowder
...Show More Authors

Resilient polymeric materials such as silicone elastomers are currently used for maxillofacial prostheses construction but the strength of these materials and their clinical performance need to be optimized with the addition of reinforcing fillers. This study investigates the effect of zirconia nanopowder addition on tear strength, tensile strength, elongation at break, Shore A hardness, surface roughness and cytotoxicity of VST-50 maxillofacial silicone. Silicone base was mixed with different amounts (1%, 2% and 3%) of zirconia nanopowder using a vacuum mixer. Silicone without filler was used as control for comparison. Scanning Electron Microscopy and Atomic Force Microscopy were utilized to assess the efficiency of high-shear vacuum mixin