The reuse or recycling of waste materials in different aspects of life is served the objective of sustainability and be beneficial to society. In recent years, a wide variety of waste materials were used in pavement construction. One of these materials is glass that generally produces in large quantities and crushed glass can be considered feasible alternative source of aggregate for asphalt mixture production. This study focused on examining the asphalt mixture properties of wearing course using crushed glass as fine aggregates. Fine crushed glass with various percentages by total weight retained on sieve 2.36 mm, 0.3 mm and 0.075 mm was used in the study. The results indicate that mixes containing crushed glass had lower Marshall stabilities and tensile strengths compared to conventional mixes. Moreover, the moisture damage resistance of glass-asphalt mixture was acceptable and satisfy the specification requirements for percentages of glass replacement up to 30 percent. Consequently, adding 30 percent of glass by weight of three sizes is the optimal value which represents about 15.6 percent by weight of total aggregate with maximum size 2.36 mm. The study has concluded that recycling and reuse of waste glass in asphalt mixture could be possible and yield a result which satisfies the specification of asphalt concrete wearing course mixtures.
Background: One of the most common problem associated with the used of soft denture lining material is microorganisms and fungal growth especially Candida albicans, which can result in chronic mucosal inflammation. The aim of this study was to evaluate the influence of chlorhexidine diacetate (CDA) salt Incorporation into soft denture lining material on antifungal activity; against Candida albicans, and the amount of chlorhexidine di-acetate salt leached out of soft liner/CDA composite. Furthermore, evaluate shear bond strength and hardness after CDA addition to soft liner Materials and methods: chlorhexidine diacetate salt was added to soft denture lining material at four different concentrations (0.05%, 0.1% and 0.2% by weight). Four hund
... Show MoreThe crystal compounds Tl2-xAg2-ySryBayCa2Cu3O10+& are successfully prepared in different concentrations (x, y=0.1, 0.2, 0.3, 0.4, 0.5) by solid state reaction process. The samples were then subjected to Nano technique under hydrolic pressure 8 ton/cm2. samples have been annealed in (850 C0) for 72 hours. The results show a best value at x, y=0.3 ratio of Ag, Ba. Electrical resistivity at x, y= 0.3 of Ag, Ba are obtained when the best value of Tc= 141 K. Samples morphology were also observed by AFM (in three dimensions), the best value of Nano is 91.74 nm at x, y= 0.3. Morphological structures of the surface were also observed by (SEM) and (EDX) show that there are dark regions and light which indicate the presence of heavy elements a
... Show MorePorous silicon (P-Si) has been produced in this work by photoelectrochemical (PEC) etching process. The irradiation has been achieved using diode laser of (2 W) power and 810 nm wavelength. The influence of various irradiation times on the properties of P-Si material such as P-Si layer thickness, surface aspect, pore diameter and the thickness of walls between pores as well as porosity and etching rate was investigated by depending on the scanning electron micrograph (SEM) technique and gravimetric measurements.
This paper reports an evaluation of the properties of medium-quality concrete incorporating recycled coarse aggregate (RCA). Concrete specimens were prepared with various percentages of the RCA (25%, 50%, 75%, and 100%). The workability, mechanical properties, and durability in terms of abrasion of cured concrete were examined at different ages. The results reveal insignificant differences between the recycled concrete (RC) and reference concrete in terms of the mechanical and durability-related measurements. Meanwhile, the workability of the RC reduced vastly since the replacement of the RCA reached 75% and 100%. The ultrasound pulse velocity (UPV) results greatly depend on the porosity of concrete and the RC exhibited higher poros
... Show MoreThe research aimed at studying the inhibitive effect of the hot watery dry and ethanolic ginger(85%) and fragrant oil which are added in concentrates of o.o25, o.o5o and 0.1g / 100g respectively in the growth of bacteria and molds. The results of the initial chemical diagnosis showed containment of ginger roots extract on. Alkaloids, Glycosides, Flavonoids and Suponins. The highest inhibitive effect of the bacteria reached the concentrate . 0.1% of the oil extract then the concentrate 0.050% of the ethanolic hot extract follows it. While 0.1% was the least inhibitive concentrate for the hot watery extract. But the inhibitive effect of the hot oily and alcoholic extracts in the numbers of molds colonies was 0.025%, when the concentrate 0.1%
... Show MoreAO Dr. Ali Jihad, Journal of Physical Education, 2021
Affinity is a term used to describe the amount of the adhesion bond between asphalt binder and aggregate. Adhesion force may be used as indicator to the amount of energy or work required to breakdown the adhesive bond between asphalt binder and aggregate. In order to study affinity between asphalt binder and aggregate, a modified device is manufacture locally similar to Rolling Bottle Test (RBT) to Predicted the degree of affinity between asphalt binder and aggregate; taking into consideration mineral composition with physical properties of asphalt binder to measure required force to separate asphalt binder from aggregate surface. In this study, suggest new parameters to represent the stripping or affinity phenomena (aff
... Show MoreThe study area soils suffer from several problems appear as tkhesvat and cracks in the roads and waterlogging which reduces the susceptibility of soil to withstand pressure, this study was conducted on the soil of the Karkh district based on field study that included (6) samples of soil physical analyses contain different ratios of (mud, sand, silt) as percentages (52%, 45%, 3 #) respectively, and liquidity limit rate (39%) Stroke rate plasticity was (20.6%) The rate coefficient of plasticity total (19.2%)0