Preferred Language
Articles
/
PRYUw4cBVTCNdQwCt2AQ
STUDY THE STRUCTURAL AND ELECTRICAL PROPERTIES OF CdTe:Ag THIN FILMS
...Show More Authors

The influence of silver doped n-type polycrystalline CdTe film with thickness of 200 nm and rate deposition of 0.3 nm.s -1 prepared under high vacuum using thermal co-evaporation technique on its some structural and electrical properties was reported. The X- ray analysis showed that all samples are polycrystalline and have the cubic zinc blend structure with preferential orientation in the [111] direction. Films doping with impurity percentages (2, 3, and 4) %Ag lead to a significant increase in the carrier concentration, so it is found to change from 23.493 108 cm -3 to 59.297 108 cm -3 for pure and doped CdTe thin films with 4%Ag respectively. But films doping with impurity percentages above lead to a significant decrease in the electrical conductivity and Hall mobility, so they are found to change from 6.3 10-7( .cm)-1 to 1.59 10-7( .cm)-1 , and from 16.759 102 cm 2 .(V.sec)-1 to 1.675 102 cm 2 .(V.sec)-1 respectively, for pure and doped CdTe thin films with 4%Ag. And also the doping lead to change the kind of conductivity for thin films obtain, so we found that pure CdTe thin film is n-type and then convert to p-type when thin film doped with (2, 3, and4) %Ag.

Publication Date
Thu Nov 19 2020
Journal Name
Indonesian Journal Of Chemistry
Determination of Eugenol in Personal-Care Products by Dispersive Liquid-Liquid Microextraction Followed by Spectrophotometry Using <i>p</i>-Amino-<i>N,N</i>-dimethylaniline as a Derivatizing Agent
...Show More Authors

Two simple methods for the determination of eugenol were developed. The first depends on the oxidative coupling of eugenol with p-amino-N,N-dimethylaniline (PADA) in the presence of K3[Fe(CN)6]. A linear regression calibration plot for eugenol was constructed at 600 nm, within a concentration range of 0.25-2.50 μg.mL–1 and a correlation coefficient (r) value of 0.9988. The limits of detection (LOD) and quantitation (LOQ) were 0.086 and 0.284 μg.mL–1, respectively. The second method is based on the dispersive liquid-liquid microextraction of the derivatized oxidative coupling product of eugenol with PADA. Under the optimized extraction procedure, the extracted colored product was determined spectrophotometrically at 618 nm. A l

... Show More
View Publication Preview PDF
Scopus (5)
Crossref (6)
Scopus Clarivate Crossref