Photobiomodulation (PBM) is a form of the use of visible red and Near-infrared (NIR) light at low power, where a laser light photon is absorbed at the electronic level, without heat production. PBM can be applied in wide range of treatment to help the wound, inflammation, edema, and pain reduction. However, there is a lack of scientific documentation regarding its actual effects. Objectives: This study assesses the impact of PBM on the release of M1-related cytokine in monocyte cells with particular emphasis on interleukin-1β (IL-1β) and Tumour Necrosis Factor α (TNF-α). Methods: Tamm-Horsfall Protein 1 (THP-1) macrophages M1 cells have been exposed to the light from the diode laser of 850nmat different doses (0, 0.6, 1.2 and 3.6 J/cm2). The release of cytokines was determined by enzyme-linked immunosorbent assay, after different periods of incubation (0, 12, 24, and 48 hours) post-irradiation. The proliferation of fibroblast cells suspended in irradiated M1-supernatent was evaluated for the same periods of incubation. Results: The results showed that PBM significantly enhanced M1-related cytokine release (p < 0.05). Obviously, IL-1β increased post-irradiation at 1.2 J/cm2 more than other doses for all incubation periods. TNF-α was decreased significantly after two days of irradiation (p < 0.005) for all doses. A significant increase in fibroblast proliferation (p < 0.005) was observed concomitant with the boost of cytokine release. Conclusion: This in vitro study has demonstrated that the PBM of the 850 nm diode laser therapy can enhance M1-related cytokine release, which in turn increases the proliferation of fibroblast cells. Moreover, PBM at 850 nm plays an anti-inflammatory role, which manifested by decreasing the level of TNF-α. Therefore, this therapy may be able to accelerate the wound healing process.
Two grades of paving asphalt with penetration of 46 and 65 are studied for determining changes in their physical and chemical properties caused by ageing.
The ageing process has been conducted on two petroleum paving asphalt cement using thin film oven test at 150, 163 and 175 C, and ageing time 5, 10,15, 20, 25 and 30 hours. The effect of ageing time and temperature on penetration, kinematic viscosity, softening point, solubility in trichloroethylene, heat loss and changes in chemical composition are investigated. The results of thin film oven test process indicte that the asphaltenes concentration of all aged asphalt increases with increasing ageing time, while the opposite was observed for polar-aromatic and naphthene-aromatic. The
Sand dunes are spread in multiple places in the world especially in a desert area as a result of economic development and construction processes, there was a need to study the behavior of sand dunes and make it suitable for construction. This paper aims to study the effect of adding sodium silicate on the cohesion strength of sand dune and its behavior. The results show that the cohesion strength increase as a percentage of sodium silicate increase (addition 8% Sodium silicate show the higher cohesion) and the cohesion between sand dune particles increase excepted when using 10% sodium silicate the cohesion began to decrease. However, the effect of curing time is significant and shows
Chitosan (CH) / Poly (1-vinylpyrrolidone-co-vinyl acetate) (PVP-co-VAc) blend (1:1) and nanocomposites reinforced with CaCO3 nanoparticles were prepared by solution casting method. FTIR analysis, tensile strength, Elongation, Young modulus, Thermal conductivity, water absorption and Antibacterial properties were studied for blend and nanocomposites. The tensile results show that the tensile strength and Young’s modulus of the nanocomposites were enhanced compared with polymer blend [CH/(PVP-co-VAc)] film. The mechanical properties of the polymer blend were improved by the addition of CaCO3 with significant increases in Young’s modulus (from 1787 MPa to ~7238 MPa) and tensile strength (from 47.87 MPa to 79.75 MPa). Strong interfacial
... Show MoreEP/ metal composites were prepared as adhesives between two steel rods. Epoxy resin (EP) was used as a matrix with metal as fillers (Al, Cu, Fe,).
The preparation method for tensile adhesion tests includes two steel rods with adhesive composites between the rods to measure adhesion strength Sad and adhesion toughness Gad.
Results of tensile adhesion tests show that EP/ metals composite have maximum strength Sad for certain weight percentage of metals 2.95 and 9MPa at 10% for EP/Al and EP/Cu composite and 8.2MPa at 40% for EP/Fe composites
A hand lay-up method was used to prepare Epoxy/ metal composites. Epoxy resin (EP) was used as a matrix with metal particles (Al, Cu, and Fe) as fillers.
The preparation method includes preparing square panels of composites with different weight percentage of fillers (10, 20, 30, 40, and 50%). Standard specimens (88mm in diameter) for thermal conductivity tests were prepared to measure thermal conductivity kexp.The result of experimental thermal conductivity kexp, for EP/metal composites show that, kexp increase with increasing weight percentage, For EP/ Al and EP/Cu composites, and it have have maximum values of 0.33 and 0.35 W/m.K, respectively. While kexp for EP/ Fe composite show slight increase with maximum value of 0.186 W/m.K.
This study is concerned with the effect of Deep Cryogenic Treatment (DCT) at liquid nitrogen temperature (-196 o C) on the mechanical properties and performance of low carbon steel (A858). The tests specimens were divided in to two groups, the first group was subjected to the conventional heat treatment of normalizing, and the second group was also normalized then subjected to (DCT). The results have shown that after (DCT), the Hardness, Tensile properties and the impact energy absorbed were all slightly increased. However the fatigue test showed some positive improvement in fatigue limit by 20(N/mm2 ), and the volume wear rates at different loads were significantly decreased after (DCT). The changes in microstructure due to (DCT) were c
... Show MoreSheets of Epoxy (EP) resin with addition of TiO2 of grain size (1.5μm, and 50nm) and weight percentage (1%, 3%, and 5%) were prepared. Discs of 20mm diameter and 3mm thickness were cut for dielectric measurements. Dielectric properties (dielectric constant, dispassion factor and electrical conductivity) over the frequency range 102 -106 Hz were measured.
Comparison was made between the effect of micro and nano particles of TiO2 on the dielectric properties of EP composites with different weight percentage. Epoxy composites with micro sized particles of TiO2 were observed to have the better values of dielectric properties.
The present investigation considers the effect of curing temperatures (30, 40, and 50˚C) and curing compound method on compressive strength development of high performance concrete, and compares the results with concrete cured at standard conditions and curing temperature (21˚C). The experimental results showed that at early ages, the rate of strength development at high curing temperature is greater than at lower curing temperature, the maximum increasing percentage in compressive strength is 10.83% at 50C˚ compared with 21C˚ in 7days curing age. However, at later ages, the strength achieved at higher curing temperature has been less, and the maximum percentage of reduction has been 5.70% at curing temperature 50C˚ compared with 21
... Show More