Background: to evaluate the effect of different dentifrices on the surface roughness of two composite resins (nanofilled-based and nanoceramic – based composite resins). Materials and methods: Forty specimens (diameter 12 mm and height of 2mm) prepared from different composite resin materials: Z350 (nanofilled composite, and Ceram-X (nanoceramic) .they were subjected to brushing simulation equivalent to the period of 1 year. The groups assessed were a control group brushed with distilled water (G1), Opalescence whitening toothpasteR (G2), Colgate sensitive pro-relief (G3) and Biomed Charcoal Toothpaste (G4). The initial and final roughness of each group was tested by surface roughness tester. The results were statistically analyzed using ANOVA and Tueky test at 0.05 significance level. Results: the surface roughness of the two tested composites brushed with the tested dentifrices was statistically higher than the roughness found in control group. Comparison among the three types of dentifrices showed that there was a statistically high significant difference in the surface roughness among all subgroups. Charcoal Toothpaste showed the highest surface roughness increase. Conclusion: Whitening dentifrices increase the surface roughness of dental composite thereby compromising its durability. Changes in composite depended on the material itself and the dentifrices used.
Background: Fracture of different types of acrylic denture base is a common problem associated with dental prosthesis. Studies suggested that the repair strength may be improved by several means including surface treatment with chemical agents. The aim of the study was to evaluate the effect of surface treatment with acrybond-bonding agent and monomer on fractured denture base in respect to transverse, tensile and shear bond strength and evaluation of the mode of failure by light microscope. Materials and methods: Two hundred seventy specimens were prepared and divided into 3 groups according to the material used (regular conventional, rapid simplified and high impact) heat cure acrylic. The specimen in each groups were prepared specificall
... Show Moreسمير خلف فياض * و محسن طالب د.نوال عزت عبد اللطيف*, مجلة الهندسة والتكنولوجيا, 2010
The fatigue is one of the major reasons for fracture of materials. Aluminum 7204 AA alloy with various heat treatments and (2.0) wt % of SiC nanoparticles were prepared by stir-casting method under rotating bending loading with ratio of stress (R= -1). The composite was strengthened by SiC particles size of) 10 (nanometre. The fatigue strength and life were obtained experimentally by the family of S-N curves for different heat treatments. The endurance limits (107cycles) for 7204 AA/ 2.0wt% SiC nano-composite fatigue strength as related to untreated nanocomposite was enhanced by 72 and 78.5% for T4 and T6, respectively.The improvement 
... Show MoreFiber reinforced polymer composite is an important material for structural application. The diversified application of FRP composite has taken center of attraction for interdisciplinary research. However, improvements on mechanical properties of this class of materials are still under research for different applications. In this paper we have modified the epoxy matrix by Al2O3, SiO2 and TiO2 nano particles in glass fiber/epoxy composite to improve the mechanical and physical properties. The composites are fabricated by hand lay-up method. It is observed that mechanical properties like flexural strength, hardness are more in case of SiO2 modified epoxy composite compare to other nano
... Show MoreThe experiment was conducted at the Agricultural Research Office in Baghdad during July 2020 to test the ability of nanomaterials (ZnO and TiO2) to inhibit ochratoxin A, which is produced by a number of microbiology (fungi) including: Aspergillus ochraceus, A. niger, ,A. steynii, A. carbonarius, Pencillume verrucosum and P. nordicum. The standard ochratoxin A, with known concentration, was treated with different concentrations of nanomaterials (20, 40, 60, and 80 ppm) and two different particle sizes of nanoparticles approximately (15 nm) and (70 nm) for each (ZnO) and TiO2; with 16 transactions. Through an examination of the HPLC, the results showed that all tra
... Show MoreAim: To evaluate the commercial pure titanium disks that structuring by laser in two design (dot and groove) each one with three different laser scan (5, 15 and 25) and comparing with titanium surface that not subjected to any surface structuring (control) through measuring the wettability test and surface roughness test. Materials and methods: Structuring on the surface of the commercial pure titanium (CP Ti) disks was performed via using fiber laser CNC machine in two design (dot and groove) in three different laser scans (5, 15 and 25), then the structuring disks analyzed with the control group by atomic force microscope and water contact angle test. Results: The results of this study showed that the surface roughness and the wettability
... Show MoreThe effect of fiber volume fraction of the carbon fiber on the thermal conductivity of the polymer composite material was studied. Different percentages of carbon fibers were used (5%, 10%, 15%, 20%, and 25%). Specimens were made in two groups for unsaturated polyester as a matrix and carbon fibers, first group has parallel arrangement of fibers and the second group has perpendicular arrangement of fibers on the thermal flow, Lee's disk method was used for testing the specimens. This study showed that the values of the of thermal conductivity of the specimens when the fibers arranged in parallel direction was higher than that when the fibers arranged in the perpendicular direction
 
... Show MoreThis work involves the development of ceramic coating to steel surfaces (enamel).This enamel high quality consisted of two ceramic layers to ensure excellent bonding with the steel surfaces. The first is called the ground coat which proved bonding between the steel base and the second outer layer called the cover coat. Various concentrations of TiO2 were separately added to the mixture of the cover coat, resulting in to much better densification of the ceramic outer layer, the hardness, thermal shock resistances, and glossiness were improved also .Moreover this addition has raised the corrosion resistances of the ceramic in harsh acidic environment and at higher temperatures Also this enamel was used to protect the surfaces of steels whi
... Show MoreIn this research Epoxy resin was reinforced by nano alumina (AL2O3) particles in grain size(25-30 nm) with two weight ratios (2,4)% then compared with pure Epoxy. Four mechanical tests were performed on these materials include Hardness, flexural, impact & compression strengths before and after immersion in tap water and chemical solutions (CH3COOH) acid, (KOH) base at (0.5N) ,The diffusivity coefficients of all prepared samples were calculate after immersion in water and chemical solutions mentioned above , the results were showed that the Flexural, Impact & Hardness increase after addition the ceramic particles (AL2O3) while the immersion process results showed illustrated different values from sample to other.
Background: The demand for better esthetic during orthodontic treatment has increased nowadays, so orthodontists starting using esthetic arch wires, brackets and ligatures.Tooth colored brackets were introduced in different types of materials. Sapphire ceramic brackets are one type of esthetic brackets and their color stability remains the main concern for the clinicians and patients at the same time. The present study design to evaluate the effect of three different staining materials (pepsi, black tea and cigarette smoke) on the stainability of sapphire ceramic brackets bonded with three types of light cure orthodontic adhesives which include: Resilience, Enlight and Transbond. Materials and Methods: The sample consisted of three hundre