Objective: This study evaluated the effect of immediate dentin sealing on the marginal adaptation of lithium disilicate overlays with three different types of resin-luting agents: preheated composite, dual-cure adhesive resin, and flowable composite. Materials and Methods: Forty-eight maxillary first premolars of similar size were prepared with a butt joint preparation design. The teeth were separated into two primary groups, each with twenty-four teeth: Group DDS: Delay dentin sealing (non-IDS) teeth were not treated. Group IDS: dentin sealing was applied immediately after teeth preparation. Each group was subsequently separated into three separate subgroups. Subgroups (DDS+Phc, IDS+Phc): cemented with preheated composite (Enamel plus HRi, Micerium, Italy), Subgroups (DDS+Dcrs, IDS+Dcrs): cemented with dual-cured resin cement (RelyX Ultimate, 3M ESPE, Germany) and Subgroups (DDS+Fc, IDS+Fc): Cemented with flowable composite (Filtek supreme flowable, 3M ESPE, USA). Using a digital microscope with a magnification of 230x, the marginal gap was measured before and after cementation at four different locations from each surface of the tooth, and the mean of measurements was calculated and analyzed statistically using the independent t-test, one-way ANOVA test, Bonferroni correction at a significance level of 0.05. Results: The samples that were immediately sealed with dentin bonding agent showed lower marginal gaps than delayed dentin sealing, both pre-and post-cementation for all subgroups, with a statistically significant difference (p < 0.01). The marginal gap was significantly lower in the IDS+Fc (48.888 ± 5.5 micro m) followed by the IDS+Dcrs group (53.612 ±5.8 micro m) and IDS+Phc (79.19 9±6.9 micro m) respectively, while the largest marginal gaps were observed in the DDS+Phc group (86.505 ± 5.4 micro m). Conclusion: Generally, the teeth with IDS showed better marginal adaptation than teeth without IDS. The marginal gap was smaller with flowable composite and dual-cure resin cement than with preheated composite.
Resin-modified glass ionomer cement tends to shrink due to polymerization of the resin component. Additionally, they are more prone to syneresis and imbibition during the setting process. This
This study was conducted to evaluate the efficiency of some chemicals and biological agents to induce systemic resistance (ISR) against to wheat common bunt disease caused by the two species of fungus Tilletia tritici (Bjerk.) Wint (T. caries (Dac.) Tul.) and T. laevis Kuhn (T. foetida (Wall.) Liro. Trails in the efforts to find an alternative, safe and environmentally friendly means to control the disease. Results of this study which carried out during two consecutive seasons for the years 2012 - 2013 and 2013 - 2014 at two different environmental locations. Seed treatment by (SA 100 and 200 mg/L, 500 ?–aminobutyric acid (BABA) and 1000 mg/L, Effective Microorganisms (EM1) 40 and 150 ml/kg seeds) have led to high significant redu
... Show MoreThis research studied the effect of magnetized water in concrete preparation and its effect on the presenting of cement in concrete mixtures also to find the ability of reducing the amount of cement in preparing one cubic meter, this is not exceed than 10% in one mixture , The experiments showed the preparation of standard cubes from the concrete which was used two kind of water magnetized water which was prepared by passing the tap water through the systems of different magnetic strength in terms of (6000,9000) Gauss and the ordinary water . The velocity of water through the magnetic field, which gives us the highest value for the compressive strength, was up to 1m/sec. to determine the best magnetic intensity, we examined The comp
... Show MoreBackground: The present in-vitro study was undertaken to evaluate and compare fracture resistance of weakened endodontically treated premolars with class II MOD cavities restored with different bulk fill composite restorations (EverX posterior, Alert, Tetric EvoCeram Bulk Fill, and SDR). The type and mode of fracture were also assessed for all the experimental groups. Materials and Method: Forty-eight human adult maxillary premolar teeth were selected for this study. Standardized extensive class II MOD cavities with endodontic treatment were prepared for all teeth, except those that were saved as intact control. The teeth were divided into six groups of eight teeth each (n=8): (Group 1) intact control group, (Group 2) unrestored teeth with
... Show MoreRoller-Compacted Concrete is a no-slump concrete, with no reinforcing steel, no forms, no finishing and wet enough to support compaction by vibratory rollers. Due to the effect of curing on properties and durability of concrete, the main purpose of this research is to study the effect of various curing methods (air curing, 7 days water curing, and permanent water curing) and porcelanite (local material used as an Internal Curing agent) with different replacement percentages of fine aggregate (volumetric replacement) on some properties of Roller-Compacted Concrete and to explore the possibility of introducing practical Roller-Compacted Concrete for road pavement with minimum requirement of curing. Specimens were sawed fro
... Show MoreTwo field experiments were carried out for cultivating yellow maize crop Zea mays L. during the autumn planting season 2019 in two sites with soils of different textures. The first site is a loamy texture in one of the fields of the Medhatia Agriculture Division, Babylon Governorate. The second was silty loam by an alluvial mixture in one of the fields of Al-Nouriah Research Station, Ministry of Agriculture located in Al-Nouriah sub-district, Al-Qadisiyah governorate. It was found through the results that the uniformity, efficiency, and adequacy of the irrigation efficiency of the sprinkler irrigation method is better than that of the sprinkler irrigation method, and it ranged between (88.6-88.7) for uniformity and (84-86)% of the irrigatio
... Show MoreThis work investigates generating of pure phase Faujasite-type zeolite Y at the ranges chosen for this study via a static aging step in the absence of seeds synthesis. Nano-sized crystals may result when LUDOX AS-40 is used as a silica source for gel composition of range 6 and the crystallization step may be conducted for a period of 4 to 19 hr at 100 ⁰C. Moreover, large-crystals with high crystallinity pure phase Y zeolite can be obtained at hereinabove conditions but when hydrous sodium metasilicate is used as a silica source. The other selected ranges also offer pure phase Y zeolite at the same controlled conditions.
This work investigates generating of pure phase Faujasite-type zeolite Y at the ranges chosen for this study via a static aging step in the absence of seeds synthesis. Nano-sized crystals may result when LUDOX AS-40 is used as a silica source for gel composition of range 6 and the crystallization step may be conducted for a period of 4 to 19 hr at 100 ⁰C. Moreover, large-crystals with high crystallinity pure phase Y zeolite can be obtained at hereinabove conditions but when hydrous sodium metasilicate is used as a silica source. The other selected ranges also offer pure phase Y zeolite at the same controlled conditions.
The world is keeping pace with evolution in all its fields as a result of scientists' pursuit of continuous scientific and technological development. This evolution included the sports field, which had a large space in the aspect of development and for all disciplines, Therefore, it's reflected today in what we see of records and advanced achievements in sporting events and activities. The development in the field of sports was the result of scientific research (Hussein and Jawad., 2022), where the interest in the training process has become one of the most important pillars of the development of achievement (Neamah and Altay., 2020). The shooting sport has also witnessed a remarkable development due to the diversity and development of its
... Show MoreNano gamma alumina was prepared by double hydrolysis process using aluminum nitrate nano hydrate and sodium aluminate as an aluminum source, hydroxyle poly acid and CTAB (cetyltrimethylammonium bromide) as templates. Different crystallization temperatures (120, 140, 160, and 180) 0C and calcinations temperatures (500, 550, 600, and 650) 0C were applied. All the batches were prepared at PH equals to 9. XRD diffraction technique and infrared Fourier transform spectroscopy were used to investigate the phase formation and the optical properties of the nano gamma alumina. N2 adsorption-desorption (BET) was used to measure the surface area and pore volume of the prepared nano alumina, the particle size and the