The increasing discharge of dye-containing wastewater has become a serious environmental problem, requiring efficient and sustainable treatment technologies. In this study, poultry litter–derived biochar (BC) was prepared via pyrolysis at 550 °C and subsequently modified with chitosan to produce a composite adsorbent (BC/CS) for the removal of Congo Red (CR) from aqueous solutions. The materials were characterized using SEM, BET, XRD, FTIR, and XPS analyses. BET results showed that chitosan modification slightly decreased the specific surface area from 8.28 to 8.18 m²/g and pore volume from 0.035 to 0.030 cm³ /g, while introducing abundant amine and hydroxyl functional groups on the surface. Maximum adsorption occurred at pH 3, with equilibrium achieved within 35 min. The BC/CS composite exhibited a maximum adsorption capacity of 35.36 mg/g, which is approximately two times higher than that of raw BC (17.83 mg/g). Adsorption kinetics followed the pseudo-second-order model (R² > 0.999), indicating that the adsorption process may involve chemical interactions, while equilibrium data were well described by the Langmuir isotherm model (R² > 0.99), suggesting monolayer adsorption. In competitive adsorption experiments involving CR, MB, MR, and MO dyes, the CR adsorption capacity decreased by only 7.5% for BC/CS, indicating good selectivity. Furthermore, regeneration studies showed that BC/CS retained approximately 86% of its initial adsorption capacity after six adsorption–desorption cycles. These results demonstrate that chitosan-modified poultry litter biochar is an effective, low-cost, and sustainable adsorbent for the removal of anionic dyes from wastewater.
The main challenge is to protect the environment from future deterioration due to pollution and the lack of natural resources. Therefore, one of the most important things to pay attention to and get rid of its negative impact is solid waste. Solid waste is a double-edged sword according to the way it is dealt with, as neglecting it causes a serious environmental risk from water, air and soil pollution, while dealing with it in the right way makes it an important resource in preserving the environment. Accordingly, the proper management of solid waste and its reuse or recycling is the most important factor. Therefore, attention has been drawn to the use of solid waste in different ways, and the most common way is to use it as an alternative
... Show MoreIn this research, CNRs have been synthesized using pyrolysis of plastic waste(pp) at 1000 ° C for one hour in a closed reactor made from stainless steel, using magnesium oxide (MgO) as a catalyst. The resultant carbon nano rods were purified and characterized using energy dispersive X-ray spectroscopy (EDX), X-ray powder diffraction (XRD). The surface characteristics of carbon rods were observed with the Field emission scanning electron microscopy (FESEM). The carbon was evenly spread and had the highest concentration from SEM-EDX characterization. The results of XRD and FESEM have shown that carbon Nano rods (CNRs) were present in Nano figures, synthesized at 1000 ° C and with pyrolysis temperature 400° C. One of t
... Show MorePorous materials play an important role in creating a sustainable environment by improving wastewater treatment's efficacy. Porous materials, including adsorbents or ion exchangers, catalysts, metal–organic frameworks, composites, carbon materials, and membranes, have widespread applications in treating wastewater and air pollution. This review examines recent developments in porous materials, focusing on their effectiveness for different wastewater pollutants. Specifically, they can treat a wide range of water contaminants, and many remove over 95% of targeted contaminants. Recent advancements include a wider range of adsorption options, heterogeneous catalysis, a new UV/H2O
This study focused on treatment of real wastewater rejected from leather industry in Al-Nahrawan city in Iraq by Electrocoagulation (EC) process followed by Reverse Osmosis (RO) process. The successive treatment was applied due to high concentration of Cr3+ ions (about 1600 ppm) rejected in wastewater of this industry and for applying EC with moderate power consumption and better results of produced water. In Electrocoagulation process (EC), the effect of NaCl concentration (1.5, 3 g/l), current density (C.D.) (15-25 mA/cm2), electrolysis time (1-2 h), and distance between electrodes (E.D.) (1-2 cm) were examined in a batch cell by implementing Taguchi experimental design. According to the results obtained from multiple regression and signa
... Show More