Objective: The objective of this study was to prepare nanosuspension of a practical water insoluble antiulcer drug which is lafutidine to enhance the solubility, dissolution rate with studying the effect of different formulation variables to obtain the best formula with appropriate physical properties and higher dissolution rate.Methods: Nanosuspension of lafutidine was prepared using solvent anti-solvent precipitation method using Polyvinylpyrrolidone K-90(PVP K-90) as the stabilizer. Ten formulations were prepared to show the effect of different variables in which two formulations showed the effect of stabilizer type, three formulations showed the effect of stabilizer concentration, two formulations showed the effect of combination of polymer with surfactant such as tween 80, three formulations show the effect of stirring speed and three formulations prepare to show the effect of addition of co-surfactant such as tween 20. All these formulations are evaluated for their particle size and entrapment efficiency and in vitro release. The selected one was evaluated for zeta potential, scanning electron microscope, atomic force microscopy, Fourier transforms infrared spectroscopy, differential scanning calorimetry, saturation solubility and stability study.Results: The formulations (F3-F10) were in the nano size. The optimum concentration of the stabilizer was in the formulation when the drug: polymer: surfactant ratio 1:4:4 and the optimum stirring speed was 1500 rpm. Dramatic effect on the particle size reduction was found by the addition of co-surfactant (tween 20) in formulation F7 that has a particle size 15.89±1.8 nm. The selected formula F7 showed an enhanced dissolution profile (10 min) compared to the pure drug at all-time intervals.Conclusion: The results show that the formulation that contains drug: PVP-K90: tween 80: tween 20 in ratio 1:4:2:2 is the best one and can be utilized to formulate lafutidine nanosuspension.
Aqueous Two Phase System (ATPS) or liquid-liquid extraction is used in biotechnology to recover valuable compounds from raw sources. In Aqueous Two-Phase Systems, many factors influence the Partition coefficient, K, (which is the ratio of protein concentration in the top phase to that in the bottom phase) and the Recovery percentage (Rec%). In this research, two systems of ATPS were used: first, polyethylene glycol (PEG) 4000/Sodium citrate (SC), and the second, PEG8000/ Sodium phosphate (SPH), for the extraction of Bovine Serum Albumin (BSA). The behavior of Rec% and K of pure (BSA) in ATPS has been investigated throughout the study by the effects of five parameters: temperature, concentration of polyethylene glycol (P
... Show MoreThe Early – Middle Miocene Ghar and Lower Fars sedimentary succession at the representative oil-well Nu-18 of the Nahr Umr oil field south Iraq; is taken by this study to investigate the sedimentological to reservoir rock facies buildups and related reservoir zonation; as first rock-typing attempt for the both formations. The sedimentological characterization of the Early Miocene Ghar formation is mainly comprised by successive buildups of sands-gravels and sandstones, whereas; the Middle Miocene Lower Fars formation is started by limestone, limestone-marly/marl anhydritic, upgraded into interbedded-series of marl and anhydrite facies, with less-common occurrences of thin-sandstone interlayers, terminated by marl-sandy-secti
... Show MoreSpin coating technique used to prepare ZnPc, CdS and ZnPc/CdS blend thin films, these films annealed at 423K for 1h, 2h and 3h. Optical behavior of these films were examined using UV-Vis. and PL. The absorption spectrum of ZnPc shows a decreasing in absorption with the increase of annealing time while CdS spectrum give a clearly absorption peak at~510 nm. Energy gap of ZnPc increases from 1.41 to 1.52 eV by increasing the annealing time. Eg of CdS decrease by increasing annealing time, from 2.3 eV to 2.2 eV. The intensities of the peaks obtained from PL spectra were strongly dependent on annealing time and confirmed the results obtained from UV-Vis. D.C. conductivity measurement showed that all the thin films have two differen
... Show MorePolyaniline (PANI) and Ag/PANI nanocomposite thin films have prepared by microwave induced plasma. The Ag powder of average particle size of 50 nm, were used to prepare Ag/PANI nanocomposite thin films. The Ag/PANI nanocomposite thin films prepared by polymerization in plasma and characterized by UV-VIS, FTIR, AFM and SEM to study the effect of silver nanoparticles on the optical properties, morphology and structure of the thin films. The optical properties studies showed that the energy band gap of the Ag/PANI (5%wt silver) decreased from 3.6 to 3.2 eV, where the substrate location varied from 4.4 to 3.4 cm from the axis of the cylindrical plasma chamber. Also the optical energy gap decreased systematically from 3.3 to 3 eV with increas
... Show MoreIn this study, Zinc oxide nanostructures were synthesized via a hydrothermal method by using zinc nitrate hexahydrate and sodium hydroxide as a precursor. Three different annealing temperatures were used to study their effect on ZnO NSs properties. The synthesized nanostructure was characterized by X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), Atomic force microscope (AFM), and Fourier Transform Infrared Spectroscopy (FTIR). Their optical properties were studied by using UV -visible spectroscopy. The XRD analysis confirms that all ZnO nanostructures have the hexagonal wurtzite structure with average crystallite size within the range of (30.59 - 34
... Show MoreABSTRACT Fifty extremely halophilic bacteria were isolated from local high salient soils named Al-Massab Al-Aam in south of iraq and were identified by using numerical taxonomy. Fourty strains were belong to the genus Halobacterium which included Hb. halobium (10%). Hb. salinarium (12.5%), Hb.cutirubrum (17.5%), Hb-saccharovorum (12.5%), Hb. valismortis (10%) and Hb. volcanii (37.5%). Growth curves were determined. Generation time (hr) in complex media and logarithmic phase were measured and found to be 10.37±0.59 for Hb. salinarium. 6.49 ± 0.24 for Hb.cutirubrum. 6.70±0.48 for Hb-valismonis, and 11.24 ± 0.96 for Hb. volcanii