In this study, poly4-(nicotinamido)-4-oxo-2-butenoic acid (PNOE) was prepared by the electro polymerization of 4-(nicotinamido)-4-oxo-2-butenoic acid (NOE) monomer on a 316 stainless steel (St.St) which acts as an anticorrosion coating. Fourier transforms infrared (FTIR), atomic force microscopy (AFM), scanning electron microscopy (SEM), and cyclic voltammetry were used to diagnose the structure and the properties of the prepared polymer layer. The corrosion behavior of the uncoated and coated 316 St.St were evaluated by using an electro chemical polarization technique in 0.2 M hydrochloric acid solution as a corrosive medium at a temperature range of 293 to 323 K. Nano materials, such as nano ZnO and graphene were added in different concentrations to the monomer solution for improving the corrosion resistance of the 316 St.St surface. The results showed that the values of protection efficiencies of the polymeric coating were increased after adding the nano materials. The kinetic and thermodynamic activation parameters were also calculated and the biological activity of the polymer film against Gram negative and positive bacteria was studied.
In this work, we focused on studying 1,4-naphthoquinones and their derivatives, and knowing the methods of preparing them using different auxiliary agents and forming derivatives containing heterocyclic rings, active groups and saturated rings containing heterogeneous elements . In addition, due to their strong antibacterial, antifungal and anticancer activity, 1,4-naphthoquinone compounds biological importance and are considered a source of various pharmaceutical compounds.
This paper experimentally investigated the dynamic buckling behavior of AISI 303 stainless steel aluminized and as received intermediate columns. Twenty seven specimens without aluminizing (type 1) and 75 specimens with hot-dip aluminizing at different aluminizing conditions of dipping temperature and dipping time (type 2), were tested under dynamic compression loading (compression and torsion), dynamic bending loading (bending and torsion), and under dynamic combined loading (compression, bending, and torsion) by using a rotating buckling test machine. The experimental results werecompared with tangent modulus theory, reduced modulus theory, and Perry Robertson interaction formula. Reduced modulus was formulated to circular cross-
... Show MoreAbstract:
Background: Retinol binding protein 4 (RBP4), an adipokine that participate in a lipid metabolism or insulin resistance through a complex regulatory network. Recently, RBP4 was reported to be associated with many cardiovascular diseases (CVDs) risk factors in patients of type 2 diabetes mellitus (T2DM). This study aims to study the correlation of serum RBP4 with some markers of glycemic control, dyslipidemia, hypertension and obesity in T2DM Iraqi patients.
Subjects and Methods: one hundred fifty participants were enrolled in this coss-sectional study, 120 of participants were T2DM patients and 30 were apparently healthy individuals to serve as control gro
... Show MoreAASAH Enass J Waheed, Shatha MH Obaid, Research Journal of Pharmaceutical, Biological and Chemical Sciences, 2019 - Cited by 5
Changes in mechanical properties of material as a result of service in different conditions can be provided by mechanical testing to assist the estimation of current internal situation of these materials, or the degree of deterioration may exist in furnaces serviced at high temperature and exceed their design life. Because of the rarity works on austenitic stainless steel material type AISI 321H, in this work, ultimate tensile strength, yield strength, elongation, hardness, and absorbed energy by impact are evaluated based on experimental data obtained from mechanical testing. Samples of tubes are extracted from furnace belong to hydrotreaterunit, also samples from un-used tube material are used to make comparisons between these properti
... Show MoreObjective: Evaluation of the poly ether keton keton polymer (PEKK) coating material on the commercial pure titanium disks (CP Ti) with or without laser surface structuring. Design: In vitro experimental study of PEKK polymer coated material on the CP Ti disks with or without laser surface structuring. Materials and methods: coating the surface of the commercial pure titanium (CP Ti) disks with PEKK polymer was performed via using frictional mode CO2 laser, then the samples disks analyzed by using FESEM. Results: the FESEM reveal good adherence and distribution of the PEKK coated material over the CP Ti substrate by using the frictional mode CO2 laser at 2 watt and 6 ms pulse duration. Conclusion: the frictional mode CO2 laser considered an
... Show MoreBackground: This study aimed to compare the mechanical properties between four groups of newly fabricated combination wires according to their method of union, according to the gauges of wires and a comparison were made between them and their originals. Materials and method: A total of 60 stainless steel combination wires were fabricated , divided into four groups according to gauge of wires and their method of union, each of them with 15 samples, the groups were welded (0.016x0.022-0.016 and 0.016x0.022-0.018) and soldered (0.016x0.022-0.016 and 0.016x0.022-0.018), samples were made according to certain parameters which were : for the welded samples: length,weight, duration of pulsation and size of copper electrode tips used; for the sold
... Show MoreAbstract
The present study investigates the effect of acetic acid on corrosion behavior and its potential of hydrothermally sealed anodized AA2319-Al-alloys. Anodizing treatment was performed in stagnant phosphoric acid electrolyte with or without addition of acetic acid. Hydrothermal sealing was carried out in boiling water for each anodized specimen. The open circuit potential of the unsealed and sealed anodized samples was examined using open circuit potential measurement for the purpose of starting in scanning polarization diagrams. The potentiostatic polarization technique measurements were performed to assess corrosion behavior and sealing quality (i.e., degree of sealing) of
... Show MoreIn this research we investigated the corrosion behavior of the commertialy pure titanium and Ti-6Al-4V alloy that coated with hydroxyapatite by electrochemical deposition with applied voltage (6,9,12) Volt from aqueous solution containing Ca(NO3)2.H2O =7.0 gm/l , (NH4)2HPO4 =3.5 gm/l , Na(NO3)2 = 8.5 gm/l in order to improve the bonding strength of hydroxyapetite and medical metals and alloys and increasing the biocompatibility. The coating layer morphology was investigated by XRD, Optical microscope , and SEM tests, the corrosio tests was made by use senthesys simulated body fluid (SBF) , and we found that the propreate voltage for coatint on Ti was 9 Volt and for Ti-6Al-4Vwas12Volt.