Self-compacting concrete (SCC) is an innovative concrete that does not require vibration for placing and compaction. It is able to flow under its own weight, completely filling formwork and achieving full compaction, even in the presence of congested reinforcement. The effect of external sulfate attack was studied-Es (very sever exposure SO4>10000ppm) according to ACI 318-11. The mix design method of SCC used is according to EFNARC 2002, and then must satisfy the criteria of filling ability, passing ability and segregation resistance. The experimental program focuses to study two different chemical composition of sulfate resistance Portland cement with different percentage of silica fume replacement by weight of cement and W/cm (0.3 and 0.35). The SCC mixes with cement type 1(C3S= 46.39 and C3S/C2S = 1.78) shows more resistance to Es than mixes with cement type 2 (C3S= 61.22 and C3S/C2S =4.44). The SCC mixes containing 10% SF as replacement of cement shows more resistance to external sulfate attack. The percentage of increase is 17.95% for SCC mixes with type 1 cement and W/cm =0.3 and 17.88% for SCC mixes with type 2 cement and W/cm =0.3 compared to reference concrete mixes
The researcher used the experimental approach due to its suitability and the nature of the research problem. The research community was represented by the eighth-grade students in the Rozak Elementary Mixed School affiliated with the General Directorate of Education in Erbil / the center, for the academic year (2021-2022), the number is (96) students, and the research sample consisted of (63) male and female students, with (31) in the experimental group, and (32) in the control group, and (11) students were excluded by (5) students from the experimental group, and (6) students from the control group, as the excluded, are students who failed and were absent from the lessons, and accordingly, the research sample became composed of (52) mal
... Show MoreIn this article, the influence of group nano transition metal oxides such as {(MnO2), (Fe2O3) and (CuO)} thin films on the (ZnO-TiO2) electric characteristics have been analyzed. The prepared films deposited on glass substrate laser Nd-YAG with wavelength (ℷ =1064 nm) ,energy of (800mJ) and number of shots (400). The density of the film was found to be (200 nm) at room temperature (RT) and annealing temperature (573K).Using DC Conductivity and Hall Effect, we obtained the electrical properties of the films. The DC Conductivity shows that that the activation energies decrease while the σRT at annealing temperature with different elements increases the formation of mixed oxides. The Hall effect, the elec
... Show MoreThe effect of short range correlations on the inelastic Coulomb form factors for excited +2 states (1.982, 3.919, 5.250 and 8.210MeV) and +4 states (3.553, 7.114, 8.960 and 10.310 MeV) in O18 is analyzed. This effect (which depends on the correlation parameterβ) is inserted into the ground state charge density distribution through the Jastrow type correlation function. The single particle harmonic oscillator wave function is used with an oscillator size parameter .b The parameters β and b are adjusted for each excited state separately so as to reproduce the experimental root mean square charge radius of .18O The nucleusO18 is considered as an inert core of C12 with two protons and four neutrons distributed over 212521211sdp−− activ
... Show MoreThe effect of gamma radiation at the doses (0 , 5 , 10 or 15 ) Gray on the callus of four Triticum aestivum immature embryos genotypes (AL-Hashmiya , AL-Noor AL-Zahraa and AL-Mellad ) were studied . The fresh and dry weight for callus and shoot tips beside numbers and lengths of the shoots were used as indicators after 8 weeks . Results revealed that (AL-Noor and AL-Zahraa ) was superior by giving highest fresh and dry weight reached 274.2 and 269.2 mg and 26 and 24.3 mg respectively as compared with AL-Hashmiya and AL-Mellad. Moreover, the control treatment and the dose 10 Gray gave highest fresh weight reached 277.4 and 259.1 mg while the dry weight was highest in the control treatment and the dose 5 Gray. addition 10 Gra
... Show MoreABSTRACT:In this paper, Cd10–xZnxS (x = 0.1, 0.3, 0.5) films were deposited by using chemical spray pyrolysis technique, the molar concentration precursor solution was 0.15 M/L. Depositions were done at 350°C on cleaned glass substrates. X-ray dif- fraction technique (XRD) studies for all the prepared film; all the films are crystalline with hexagonal structure .The optical properties of the prepared films were studied using measurements from VIS-UV-IR spectrophotometer at wave- length with the range 300 - 900 nm; the average transmission of the minimum doping ratio (Zn at 0.1%) was about 55% in the VIS region, it was decrease at the increasing of Zn concentration in the CdS films, The band gap of the doped CdS films was varied as 3.7, 3
... Show More