This study shows how the structural and dielectric properties of (SnO2)1-x(Mn2O3)x, (where x=0.00, 0.03, 0.05,0.07, and 0.09) prepared using the solid state reaction technique, are affected by the doping of semiconducting metal oxide Mn2O3. Structural analysis of the composites was carried out using information from the composite samples obtained from X-ray diffraction (XRD). The diffraction peak shifting in XRD patterns indicated that Mn ions were successfully incorporated into the SnO2 crystal lattice. Mn ions were successfully doped in the Tin oxide matrix lattice with the subsequent increase of doping levels. The average crystal size evaluated using Scherrer's equation was found to vary from 33 to 37 nm, and the lattice constants were a=4.68-3.69 and c=3.166-3.173. This work also tested the dielectric characteristics of (SnO2)1-x(Mn2O3) x composites. The effects of Mn doping were interpreted and discussed. The effects of Mn doping on the σa.c(ω), exponent (s), dielectric constant, dielectric loss, relaxation time, and polarizability were also studied.
Sheets of Epoxy (EP) resin with addition of TiO2 of grain size (1.5μm, and 50nm) and weight percentage (1%, 3%, and 5%) were prepared. Discs of 20mm diameter and 3mm thickness were cut for dielectric measurements. Dielectric properties (dielectric constant, dispassion factor and electrical conductivity) over the frequency range 102 -106 Hz were measured.
Comparison was made between the effect of micro and nano particles of TiO2 on the dielectric properties of EP composites with different weight percentage. Epoxy composites with micro sized particles of TiO2 were observed to have the better values of dielectric properties.
The effects of BaCl2 dopant on the optical properties of poly (vinyl alcohol) have been investigated. Pure and BaCl2 doped PVA films were prepared using solvent casting method. These films were characterized using UV/VIS technique in order to estimate the kind of transition which was found to be indirect transition. The value of the optical energy gap was decrease with increasing dopant concentration.
Refractive index, extinction coefficient and Urbach tail have been also investigated; it was found that all the above parameters affects by doping.
Abstract
Semiconductor-based gas sensors were prepared, that use n-type tin oxide (SnO2) and tin oxide: zinc oxide composite (SnO2)1-x(ZnO)x at different x ratios using pulse laser deposition at room temperature. The prepared thin films were examined to reach the optimum conditions for gas sensing applications, namely X-ray diffraction, Hall effect measurements, and direct current conductivity. It was found that the optimum crystallinity and maximum electron density, corresponding to the minimum charge carrier mobility, appeared at 10% ZnO ratio. This ratio appeared has the optimum NO2 gas sensitivity for 5% gas concentration at 300 °C working temperat
... Show MoreIn this study, thin films of pure titanium dioxide (TiO2) and titanium dioxide dual mixed with zinc oxide (ZnO) and magnesium oxide (MgO) with varying concentrations of (ZnO: MgO)x ranging from 0 to 30 wt% undoped and doped gold nanoparticles (AuNPs) were prepared on glass using the chemical spray pyrolysis (CSP) technique. The morphological, structural, and sensing properties of the prepared thin films were examined. Atomic Force Microscopy (AFM) analysis revealed that these films exhibit a consistent structure before and after doping. Initially, the roughness of these films was observed to increase upon the introduction of impurities (ZnO: MgO)x. This trend reversed at x=0.20, where a decrease in roughness occurred. Interestingly, a sub
... Show MoreIn this study, thin films of pure titanium dioxide (TiO 2 ) and titanium dioxide dual mixed with zinc oxide (ZnO) and magnesium oxide (MgO) with varying concentrations of (ZnO: MgO) x ranging from 0 to 30 wt% undoped and doped gold nanoparticles (AuNPs) were prepared on glass using the chemical spray pyrolysis (CSP) technique. The morphological, structural, and sensing properties of the prepared thin films were examined. Atomic Force Microscopy (AFM) analysis revealed that these films exhibit a consistent structure before and after doping. Initially, the roughness of these films was observed to increase upon the introduction of impurities (ZnO: MgO) x . This trend reversed at x = 0.20, where a decrease in roughness occurred. Interestin
... Show Morethe structrual and mechanical properties of thin Ni films of different thicknesses deposited on coring glass substrate using lonbeam sputtering(IBS) technique under vacuum torr have been studied the TEM and electron
Thin films of tin sulfide (SnS) were prepared by thermal evaporation technique on glass substrates, with thickness in the range of 100, 200 and 300nm and their physical properties were studied with appropriate techniques. The phase of the synthesized thin films was confirmed by X-ray diffraction analysis. Further, the crystallite size was calculated by Scherer formula and found to increase from 58 to 79 nm with increase of thickness. The obtained results were discussed in view of testing the suitability of SnS film as an absorber for the fabrication of low-cost and non toxic solar cell. For thickness, t=300nm, the films showed orthorhombic OR phase with a strong (111) preferred orientation. The films deposited with thickness < 200nm deviate
... Show More|
Ferrite with the general formula CuLayFe2-yO4 (where y=0.02, 0.04, 0.06, 0.08 and 0.1), were prepared by standard ceramic technique. The main cubic spinel structure phase for all samples was confirmed by x-ray diffraction patterns with the appearance of small amount of secondary phases. The lattice parameter results were 8.285-8.348 Å. X-ray density increased with La addition and showed values between 5.5826 – 5.7461gm/cm3. The Atomic Force Microscopy (AFM) showed that the average grain size was decreasing with the increase in La concentration. The Hall coefficient was found to be positive. It de |