Introduction: This study was designed to examine the effects of addition of the combination of polymerized polymethyl methacrylate (PMMA) and zirconia (ZrO2) particles to heat cure PMMA resin on impact strength, surface hardness, and roughness. Methods: The 70% (w/w) of polymerized PMMA powder (particle size: 0.70mm) was mixed with 30% (w/w) of zirconia powder (ZrO2) (1mm) to produce PMMA-ZrO2 filler. Ninety acrylic specimens created were divided into three groups containing 0% wt (Control group), 2% wt, and 4% wt, PMMA-ZrO2 filler. Ten specimens were used for impact strength, surface hardness and roughness test, blindly. Data were analyzed via oneway ANOVA and the Tukey post hoc test using R 3.6.3. Results: There was statistically significant difference among study groups regarding surface hardness and roughness (p < 0.001). Yet, nonsignificant difference was found on the subject of impact strength (p=0.33). Post hoc test showed statistically significant difference for all pairwise comparisons as regards surface hardness and roughness (p < 0.05). Conclusion: The incorporation of PMMA-ZrO2 filler did not improve impact strength (resistance during an unexpected blows or dropping). Yet, increased surface roughness and hardness, concentration-dependently.
Background: Polymethylmethacrylate (PMMA) has relatively unsatisfactory mechanical properties such as low flexural strength and impact strength also dimensional instability. Material and method: Zirconium silicate nanoparticles were coated with a layer of trimethoxysilylpropylmethacrylate (TMSPM) before sonication in monomer (MMA) with the percentages 1% and 1.5% by weight then mixed with powder using conventional procedure, (150) samples were prepared and divided into three groups, each group consisted of (50) samples, the first group prepared from PMMA without addition (control), another group with the addition of 1% wt Zrsio4 nanoparticles (experimental) and the third one with 1.5% wt Zrsio4 nanoparticles (experimental). Each group
... Show MoreAn experimental study is carried out on the effect of vortex generators (Circular and square) on the flow and heat transfer at variable locations at (X = 0.5, 1.5, 2.5 cm) ahead of a heat exchanger with Reynolds number ranging from 62000< Re < 125000 and heat flux from 3000 ≤ q ≤ 8000 W/m2 .
In the experimental investigation, an apparatus is set up to measure the velocity and temperatures around the heat exchanger.
The results show that there is an effect for using vortex generators on heat transfer. Also, heat transfer depends on the shape and location. The circular is found t
... Show MoreThe spectral characteristics and the nonlinear optical properties of the mixed donor (C-480) acceptor (Rh-6G) have been determined. The spectral characteristics are studied by recording their absorption and fluorescence spectra. The nonlinear optical properties were measured by z-scan technique, using Q-switched Nd: YAG laser with 1064 nm wavelength. The results showed that the optimum concentration of acceptor is responsible for increasing the absorption and the emission bandwidth of donor to full range and to 242 nm respectively by the energy transfer process, also the efficiency of the process was increased by increasing the donor and acceptor concentration. The obtained nonlinear properties results of the mixture C-480/ Rh-6G showed
... Show MoreBackground: The mechanical and physical properties of Polymethyl methacrylate (PMMA) don’tfulfill the entire ideal requirements of denture base materials. The purpose of this study was to produce new modified polymer nanocomposite (PMMA /ZrO2-TiO2) andassess itsimpact strength, transverse strength and thermal conductivity in comparison to the conventionalheat polymerized acrylic resin. Materials and Methods: Both ZrO2 and TiO2nano fillers were silanized with TMSPM (trimethoxysilyl propyl methacrylate) silane coupling agent before beingdispersed by ultrasonication with the methylmethacrylate (monomer) and mixed with the polymer by means of 2% by weight in (1:1) ratio, 60 specimens were constructed by conventional water bath processing
... Show MoreBackground: The polymethyl methacrylate is the most reliable material for the construction of complete and partial dentures, despite satisfying esthetic demand itsuffered from having unsatisfactory properties like impact strength and transverse strength. This study was designed to improve the impact strength and transverse strength of heat cure acrylic resin by adding untreated and oxygen plasma treated polypropylene fibers and investigate the effect of this additive on some properties of acrylic resin materials. Materials and methods: Untreated and oxygen plasma treated polypropylene fibers was added to PMMA powder by weight 2.5 %. Specimens were constructed and divided into 5 groups according to the using tests; each group was subdivided
... Show MoreThis research is addressing the effect of different ferrocene concentration (0.00, 2.15x10-3, 4.30x10-3, 8.60x10-3, and 12.9x10-3) on the bulk free radical polymerization of methyl methacrylate monomer in benzene using benzoyl peroxide as initiator. The polymerization was conducted at 60º C under free oxygen atmosphere. The resulting polymers were characterized by FTIR. The results were compared with the presence and absence of ferrocene at 10% conversion. The %conversion was 3.04% with no ferrocene present in the polymerization medium and its increase to 9.06 with a first lowest ferrocene concentration added, i.e. 2.15 x10-3mol/l. This was positively reflected on the poly(methyl methacrylate) molecular weight measured by viscosity techniq
... Show MoreABSTRACT Background: Bracket rebonding is a common problem in orthodontics which may result in many drawbacks. The aims of this study were to evaluate the effects of application of two enamel protective agents “Icon†and “ProSeal†on shear bond strength before and after rebonding of stainless steel orthodontic brackets using conventional orthodontic adhesive and to assess the site of bond failure. Materials and methods: Fifty sound extracted human upper first premolar teeth were selected and randomly divided into two equal groups; the first time bonding and the rebonding groups (n=30). Each group was subdivided into control, Icon and ProSeal subgroups. The enamel protective agents were applied after etching (precondi
... Show MorePurpose: To evaluate the effect of different surface treatments on shear bond strength between dentin and IPS e.max lithium disilicate glass-ceramic. Materials and Methods: Eighteen extracted third molars were embeded in epoxy resin. The tooth was sectioned vertically in mesiodistal direction using a low speed hard tissue microtome. The buccal and lingual surfaces of each section were ground flat using 600 grit Silicone carbide paper. Eighteen ceramic discs consisted of lithium disilicate glass-ceramic were prepared with a diameter of 4.7mm and height of 2.2mm. The discs were divided in two groups (n=10): (1) IPS e.max treated with hydrofluoric acid and Monobond Plus (MBP) and (2) IPS e.max treated with Monobond Etch &Prime (MBEP). The toot