The zirconia ceramic restoration (ZCR) is used as substitutes for the metal-ceramic restoration. Clinical studies demonstrating of ZCRs showed a high fracture incidence of veneering layer than metal-ceramic restorations. This attributed to the low bond strength of zirconia to veneering ceramic as a result of lacking of glass content in its matrix. Surface treatment was proposed to improve the bonding strength between zirconia and veneering ceramic. Several studies revealed that some treatment such as airborne particle abrasion (APA) is responsible for generating chipping of veneering ceramic. The study aimed to develop a new zirconia coatings to increase bonding strength between zirconia substrate and veneering porcelain. Three groups of 150 zirconia specimens (discs, rods and crowns) were divided according to the type of surface treatments; Group M1 designated unsintered zirconia specimens coated with a mixture of glaze porcelain powder and partially-sintered zirconia powder prepared at 1100 °C with two particle sizes; A (26 ± 0.3 μm) and size B (47 ± 0.5 μm), group M2 was coated with mixture of ceramic liner paste and same selected particle sizes of partially-sintered zirconia powders. The coated groups (M1 and M2) subdivided according to powder sizes into M1A, M1B, M2A and M2B. APA group (as control) of sintered zirconia specimens abraded with 50 μm aluminium oxide powder. Surface area roughness (Sa) was measured by surface texture analyser. Surface morphology and elemental composition were analysed by scanning electron microscope (SEM). Crystallographic phases were identified by X-ray diffraction (XRD). The coefficient of thermal expansion (CTE) was assessed by a thermomechanical analyser. For shear bond strength (SBS) test was evaluated by a universal testing machine (UTM). The fracture strength (FS) test prepared and measured by Cercon CAD/CAM system and UTM. Fractographic analysis for SBS and FS were examined by a stereomicroscope and SEM. For each test and measurement, 10 specimens were used per group. Finite element analysis (FEA) was used to simulate and predict the iv stress distributions of the static oblique load in coated and non-coated zirconia crown models. The collected data were analysed by one-way ANOVA and Tukey HSD test at (P<0.05). Surface roughness results showed significant differences among all groups (P<0.000). The M1B group exhibited a higher Sa value (10.33 ± 0.59 μm) among the tested groups. XRD analysis showed tetragonal and monoclinic phases in the control group while only tetragonal was detected in the coated groups. The SBS values for coated groups were higher than the control group. The M1B group showed higher and significant differences in SBS value (37.54 ± 4.38 MPa) among other tested groups (P<0.05). The FS test indicated that coated M1B group (647.92 ± 97.33 N) higher than the other groups (P<0.00). FEA showed the coated crown models have lower stress level than the non-coated model. The new coating (M1B) by airbrush spray technique considered as an alternative way to APA treatment to improve the bond strength of zirconia substrate to veneering ceramic and indicating as an applicable surface treatment for improving the clinical performance of the coated ZCR.
The electrospun nanofibers membranes (ENMs) have gained great attention due to their superior performance. However, the low mechanical strength of ENMs, such as the rigidity and low strength, limits their applications in many aspects which need adequate strength, such as water filtration. This work investigates the impact of electrospinning parameters on the properties of ENMs fabricated from polyacrylonitrile (PAN) solved in N, N-Dimethylformamide (DMF). The studied electrospinning parameters were polymer concentration, solution flow rate, collector rotating speed, and the distance between the needle and collector. The fabricated ENMs were characterized using scanning electron microscopy (SEM) to understand the surface morphology and es
... Show MoreSome children are suffering from introversion in kindergartens , so it must be confront and obviated by specialists because it will inevitably lead to unsatisfactory results reflect negatively on the individual and the community together . And the introvert child is a miserable child incapable of social interaction or give - and - take with colleagues , lack of integration of the child to life leads to the obstruction of participation with his peers in various activities. Introversion causes a real emotional deficit to the children of kindergartens which limits of possibility of their intellectual development and mental growth and that because of their isolation and poor focus in education
... Show MoreFiber reinforced polymer composite is an important material for structural application. The diversified application of FRP composite has taken center of attraction for interdisciplinary research. However, improvements on mechanical properties of this class of materials are still under research for different applications. In this paper we have modified the epoxy matrix by Al2O3, SiO2 and TiO2 nano particles in glass fiber/epoxy composite to improve the mechanical and physical properties. The composites are fabricated by hand lay-up method. It is observed that mechanical properties like flexural strength, hardness are more in case of SiO2 modified epoxy composite compare to other nano
... Show MoreThe increasing population growth resulting in the tremendous increase in consumption of fuels, energy, and petrochemical products and coupled with the depletion in conventional crude oil reserves and production make it imperative for Nigeria to explore her bitumen reserves so as to meet her energy and petrochemicals needs. Samples of Agbabu bitumen were subjected to thermal cracking in a tubular steel reactor operated at 10 bar pressure to investigate the effect of temperature on the cracking reaction. The gas produced was analyzed in a Gas Chromatograph while the liquid products were subjected to Gas Chromatography-Mass Spectrometry (GC-MS) analysis. Heptane was the dominant gas produced in bitumen cracking at all temperatures and the r
... Show MoreCdSe alloy has been prepared successfully from its high purity elements. Thin films of this alloy with different thicknesses (300,700)nm have been grown on glass substrates at room temperature under very low pressure (10-5)Torr with rate of deposition (1.7)nm/sec by thermal evaporation technique, after that these thin films have been heat treated under low pressure (10-2)Torr at (473,673)K for one hour. X-ray patterns showed that both CdSe alloy and thin films are polycrystalline and have the hexagonal structure with preferential orientation in the [100] and [002] direction respectively. The optical measurements indicated that CdSe thin films have allowed direct optical energy band gap, and it increases from (1.77- 1.84) eV and from
... Show MoreBackground: Impression materials, impression trays, and poured stone cast have been said to be the main source of cross infection between patients and dentists. However, it was observed that disinfection of the impression is not performed systematically in routine dental practice. Disinfection of alginates either by immersion or spray technique was found to cause dimensional inaccuracies, although with proper disinfection of alginates there were small dimensional changes. A variety of fluoride releasing products designed for topical use is currently available. Following their use, varied amount of fluoride is systemically absorbed depending on the fluoride concentration and the manner of its use. The objective of this study was to evaluate
... Show MoreSamples prepared by using carbon black as a filler material and phenolic resin as a binder. The samples were pressed in a (3) cm diameter cylindrical die to (250)MPa and treated thermally within temperature range of (600-1000)oC for two and three hours. Physical properties tests were performed, like density, porosity, and X-ray tests. Moreover vicker microhardness and electric resistivity tests were done. From the results, it can be concluded that density was increased while porosity was decreased gradually with increasing temperature and treating time. In microhardness test, it found that more temperature and treating time cause more hardness. Finally the resistivity was decreased in steps with temperature and treating time. It can be c
... Show More