ZnO nanostructures were synthesized in one step reaction at 80℃ without any extra treatments.(Zn (NO₃) ₂. 6H2O) and (NaOH) were used for synthesis. Production of ZnO nanostructures occurred relatively in short time. The obtained ZnO nanostructures were characterized by X-ray diffraction (XRD) and the atomic force microscope AFM. Carboxymethyleted PVA (CPVA) has been prepared and characterized.(CPVA) were composite with different ZnO nanoparticles concentrations. The composites are cast into films. The dielectric constant properties of the films were measured with hp LCR meter.
الهدف من الدراسه تحضير فئه جديده من بوليمرات السليكون P1-P4 والتي تمت على اساس استحدام ثنائي مثيل ثنائي كلورو سيلان((DCDMS مع بعض المركبات العضويه التي تحتوي مجاميع الهيدروكسيل الطرفيه والتي حضرت لاول مره M1-M4، بأستخدم البلمره التكثيفيه .كما تم تحضير متراكباتها النانويهP′1-P′4 بوجود جسيمات الفضه النانويه (Ag-NPs) باستخدام طريقة صب المحاليل. شخصت جميع التراكيب للمونمرات والبوليمرات المحضره باستخدام مطيافية
... Show MoreThe work concerned with studying the effect of (SiO2) addition as a
filler on the adhesive properties of (PVA). Samples were prepared as
sheets by using casting method. The mechanical properties showed
that increase in tensile strength from (34MPa) to (68MPa) when
(SiO2) added to (PVA). The adhesive strength showed that joint
properties depend upon specific adhesive characteristic of material
(PVA) and (SiO2\PVA)composites at different concentrations (1.5%,
2.5%, 3.5%, 4.5wt%), the cohesive strength of the adhesive material,
the joint design, and adherent type (Sponge Rubber(SR), Natural
leather (NL), Vulcanized Rubber(VR), and Cartoon). The results
proved the tensile strength increased with (SiO2) ratio, so
In this study, thin film of pure zinc oxide (ZnO) and ZnO doped with Ga2O3 films with different concentrations (0, 0.03, 0.05, 0.07 and 0.09)wt% were prepared by pulsed laser deposition. The powder mixture was then sintered in a furnace at 1273 K for 5 h. The resulting powders were thoroughly ground and then pressed using a special press to form discs with a diameter of 1 cm and a thickness of 0.5 cm. The deposition was carried out under a vacuum of 2.5×10−2 mbar on various substrates, including glass for AFM measurements and n-type crystalline silicon wafers for the gas sensor. AFM results revealed a progressive increase in both grain size and roughness with moderate doping and irregularity at high doping levels. Gas-sensing meas
... Show MoreIn this research, Zinc oxide (ZnO)/epoxy nanocomposite was synthesized by simple casting method with 2wt. % ZnO concentration. The aim of this work was to study the effect of pH and composite dosage on the photocatalytic activity of ZnO/ epoxy nanocomposite. Scanning electron microscopy (SEM) technique images proof the homogeneous distribution of ZnO nanoparticles in epoxy. A synthesized nanocomposite samples were characterized by Fourier Transform Infrared spectrometer (FTIR) measurements. Two spectra for epoxy and 2wt.% ZnO/epoxy nanocomposites were similar and there are no new bonds formed from the incorporation of ZnO nanoparticles. Using HCl and NaOH were added to Methylene blue (MB) dye (5ppm) to gat pH values 3 and 8. The degradat
... Show MoreThis study synthesized nanocomposite photocatalyst materials from a mixture of Cu2O nanoparticles, ZnO nanoparticles, and graphene oxide (GO) through coprecipitation and hydrothermal methods. This study aims to determine the optimum composition of Cu2O/ZnO/GO nanocomposites in degrading methylene blue. The nanocomposite was synthesized in two steps: 1 the synthesis of Cu2O and ZnO nanoparticles through the coprecipitation method and the preparation of GO through the modified Hummer method. 2 The preparation of Cu2O and ZnO nanoparticles mixtures with GO through the hydrothermal method to form Cu2O/ZnO/GO nanocomposites. The adsorption-photocatalysis process of methylene blue
... Show MoreIn this work, chemical oxidation was used to polymerize conjugated polymer "Polypyrrole" at room temperature Graphene nanoparticles were added by in situ-polymerization to get (PPY-GN) nano. Optical and Electrical properties were studied for the nanocomposites. optical properties of the nanocomposites were studied by UV-Vis spectroscopy at wavelength range (200 -800 nm). The result showed optical absorption spectra were normally determined and the result showed that the maximum absorbance wave length at 280nm and 590nm. The optical energy gap has been evaluated by direct transition and the value has decreased from (2.1 eV for pure PPy) to (1.3 eV for 5 %wt. of GN). The optical constants such as the band tail width ΔE was evaluated, the