In this study, aluminum nanoparticles (Al NPs) were prepared using explosive strips method in double-distilled deionized water (DDDW), where the effect of five different currents (25, 50, 75, 100 and 125 A) on particle size and distribution was studied. Also, the explosive strips method was used to decorate zinc oxide particles with Al particles, where Al particles were prepared in suspended from zinc oxide with DDDW. Transmission electron microscopy (TEM), UV-visible absorption spectroscopy, and x-ray diffraction are used to characterize the nanoparticles. XRD pattern were examined for three samples of aluminum particles and DDDW prepared with three current values (25, 75 and 125 A) and three samples prepared with the same currents for zinc oxide suspension with aluminum particles and DDDW. It was observed that when increasing the percentage of prepared Al particles in the suspension consisting of zinc oxide and DDDW, the energy gap of zinc oxide gradually decreased in the samples. Transmission electron microscopy (TEM) analysis is conducted to examine the size, shape, and aggregation of the nanoparticles. The TEM images reveal that the Al nanoparticles exhibit a quasi-spherical shape. The particle size distribution analysis shows that the average crystal size of Al decreases with an increase in the detonation current. This method yields particle with average sizes within the range of 20 to 90 nm. When decorating zinc oxide particles by generating Al nanoparticles inside a suspension of zinc oxide and DDDW, the size of the resulting particles increases with increasing current. © ALL RIGHTS RESERVED.
In this paper flotation method experiments were performed to investigate the removal of lead and zinc. Various parameters such as pH, air flow rate, collector concentrations, collector type and initial metal concentrations were tested in a bubble column of 6 cm inside diameter. High recoveries of the two metals have been obtained by applying the foam flotation process, and at relatively short time 45 minutes . The results show that the best removal of lead about 95% was achieved at pH value of 8 and the best removal of zinc about 93% was achieved
at pH value of 10 by using 100 mg/l of Sodium dodecylsulfate (SDS) as a collector and 1% ethanol as a frother. The results show that the removal efficiency increased with increasing initial m
Staphylococcus haemolyticus is one of the most frequently isolated coagulase-negative staphylococci. The ability to form biofilm is considered as one of the most important virulence factors of coagulase negative staphylococci. There is only limited knowledge of the nature of S. haemolyticus biofilms. This study was aimed at evaluating the ability of S. haemolyticus strains to produce biofilm in the presence of copper oxide nanoparticles (CuONPs). The biological synthesis of nanoparticles is an environmentally friendly approach for large-scale production of nanoparticles. Copper oxide nanoparticles were produced in the current study from the S. haemolyticus viable cell filtrate. UV-visible (UV-Vis) spectroscopy, X-ray diffra
... Show MoreA process of bacterial cellulose gold nanocomposite has been investigated based on experimental work and cited literature. A literature review on the production process is carried out in this study. Bacterial cellulose is a high crystalline fabric material generally used in biomedical applications. A Nanocomposite was made by synthesis from gold and bacterial cellulose. The experimental work includes growing, and isolating bacterial cellulose, preparation of gold Nanoparticles and preparation of Nano composite. Nanoparticle’s formation and adsorption on the cellulose tissue have been observed visually, where a colour change was observed. The predicted particle size for the gold nano
This study aimed to develop a stable nanosuspension of repaglinide and improve its dissolution, using the Nano-precipitation method, involving a different concentration of a stabilizer, different co-stabilizers and different solvents. Employment of a systemic approach to optimize the formulation parameters, including stabilizer concentration, solvent choice and co-stabilizer election. Soluplus® (SOL) was used as the primary stabilizer for this research, polyvinyl alcohol (PVA), poloxamer 188 (PXM 188), tween 80 (TW80), and polyvinyl pyrrolidine (PVP k30) were investigated as co-stabilizers to prevent particle agglomeration and ensure long-term stability. In addition to ethanol as a primary solvent, acetone and chloroform were used
... Show MoreChemical spray pyrolysis technique was used at substrate temperature 250 ˚C with annealing temperature at 400 ˚C (for 1hour) to deposition tungsten oxide thin film with different doping concentration of Au nanoparticle (0, 10, 20, 30 and 40)% wt. on glass substrate with thickness about 100 nm. The structural, optical properties were investigated. The X-ray diffraction shows that the films at substrate temperature (250 ˚C) was amorphous while at annealing temperature have a polycrystalline structure with the preferred orientation of (200), all the samples have a hexagonal structure for WO3 and Au gold nanoparticles have a cubic structure. Atomic force microscopy (AFM) was used to characterize the morphology of the films. The optical pr
... Show MoreThe recent studies suggested the possible toxicities or genetic alterations associated with biological and medical applications of silver nanoparticles (AgNPs). The current research is directed to see if AgNPs administration can lead to some changes in expression of BRAF gene in selected body organs tissues. Fifty-six male of musmusculs (Balb/C) mice from the animal house of Al-Nahrain Centre of Biotechnology were used. These animals were divided randomly to seven groups (eight mouse in each group), one of these groups represented the control group, three groups were subjected to different doses of AgNPs (0.25, 0.5and 1 mg/kg of body weight) for one week, and the remaining three groups were subjected to three different doses of AgNP
... Show MoreGold nanoparticles AuNPs have proven to be powerful tools in various nanomedicine applications, because of their photo-optical distinctiveness and biocompatibility. Noble metal gold nanoparticles was prepared by pulsed laser ablation method (1064-Nd: YAG with various Laser power from 200 to 800 mJ and 1 Hz frequency) in distil water. The process was characterized using UV-VIS absorption spectroscopy. Morphology and average size of nanoparticles were estimated using AFM and X-ray diffraction (XRD) analysis which show the nature of gold nanoparticles (AuNPs). Antibacterial activity of gold nanoparticles as a function of particles concentration against gram negative bacterium Escherichia coli and gram positive bacterial Staphylococcus aureu
... Show MoreAcinetobacter baumannii is highly adapted to hospital environments, causing persistent chronic infections due to its ability to form biofilms. In this work, the antibiofilm activity of AuNPs with a subMIC concentration of 9.34 μg/ml was investigated by the microtiter plate method against 80 clinical isolates of A. baumannii. The results revealed that the biofilm was significantly (P< 0.05) reduced by 48.2 – 82.1%.
Ni-Co-Mn-Mg ferrite nanoparticles with the formula (Ni,Co)xMn0.25-xMg0.75Fe2O4 were synthesized in this work by employing the sol-gel auto-combustion process, with nitrates used as the cations source and citric acid (C6H8O7) as the combustion agent. X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), energy dispersive X-ray (EDX), and a vibrating sample magnetometer (VSM) were used to characterize the structural, morphological, and magnetic properties of ferrite powders. The XRD measurements showed crystallite sizes ranging between 24 - 28 nm. The FE-SEM images show the presence of agglomeration as well as a non-homogeneous distribution of the samples. On the other hand, the stoichiometry of the react
... Show MoreIn this work the fabrication and characterization of poly(3-hexylthiophene) P3HT-metallic nanoparticles (Ag, Al). Pulsed Laser Ablation (PLA) technique was used to synthesis the nanoparticles in liquid. The Fourier Transformer Infrared (FTIR) for all samples indicate the chemical interaction between the polymer and the nanoparticles. Scanning Electron Microscopic (SEM) analysis showed the particle size for P3HT-AgNps samples between 44.50 nanometers as well the spherical structure. While for P3HT-AlNps samples was flakes shape. Energy Dispersive X-ray (EDX) spectra show the existing of amount of metallic nanoparticles.