The performance and durability of asphalt pavements are strongly influenced by the rheological properties of asphalt binders, particularly under severe climatic and traffic conditions. This study investigates the synergistic effects of incorporating multi-walled carbon nanotubes (CNTs) at dosages ranging from 0.25% to 1% into AC 40-50 asphalt binders modified with 4% Styrene–Butadiene–Styrene (SBS). A comprehensive experimental program involving physical, rheological, and chemical characterization tests was conducted, including penetration, softening point, viscosity, storage stability, a Dynamic Shear Rheometer (DSR), Multiple Stress Creep Recovery (MSCR), Linear Amplitude Sweep (LAS), Fourier Transform Infrared Spectroscopy (FTIR), and Glover–Rowe (G-R) analysis. Statistical inference using one-way ANOVA was also conducted to evaluate the significance of differences among the binder formulations investigated. The results showed a continuous increase in binder stiffness with increasing CNT content, as indicated by decreasing penetration values, higher softening points, and increased viscosity. Incorporating 1% CNT reduced the softening-point difference from 3.1 °C to 1.6 °C in SBS-modified binders, indicating improved storage stability. Rheological evaluations showed that 0.75% CNT increased the high-temperature performance grade from 82 °C to 88 °C and provided the best rutting resistance, as indicated by MSCR results. In contrast, the 0.5% CNT formulation exhibited superior fatigue resistance and the lowest Glover–Rowe index, indicating improved cracking resistance and durability. Overall, the findings demonstrate that CNTs can effectively enhance the performance of SBS-modified asphalt binders, with 0.75% CNT being optimal for hot-climate applications, while 0.5% CNT exhibited improved fatigue and cracking resistance under moderate-temperature conditions.
This research utilized natural asphalt (NA) deposits from sulfur springs in western Iraq. Laboratory tests were conducted to evaluate the performance of an asphalt mixture incorporating NA and verify its suitability for local pavement applications. To achieve this, a combination of two types of NA, namely soft SNA and hard HNA, was blended to create a binder known as Type HSNA. The resulting HSNA exhibited a penetration grade that adhered to Iraqi specifications. Various percentages of NA (20%, 40%, 60%, and 80%) were added to petroleum asphalt. The findings revealed enhanced physical properties of HSNA, which also satisfied the requirements outlined in the Iraqi specifications for asphalt cement. Consequently, HSNA can serve as an
... Show More
Antimicrobial therapies are desperately needed since the threat posed by multidrug‐resistant (MDR) bacteria only grows. Bacteriocins produced by
Reflection cracking in asphalt concrete (AC) overlays is a common form of pavement deterioration that occurs when underlying cracks and joints in the pavement structure propagate through an overlay due to thermal and traffic-induced movement, ultimately degrading the pavement’s lifespan and performance. This study aims to determine how alterations in overlay thickness and temperature conditions, the incorporation of chopped fibers, and the use of geotextiles influence the overlay’s capacity to postpone the occurrence of reflection cracking. To achieve the above objective, a total of 36 prism specimens were prepared and tested using an overlay testing machine (OTM). The variables considered in this study were the thickness of the
... Show MoreReflection cracking in asphalt concrete (AC) overlays is a common form of pavement deterioration that occurs when underlying cracks and joints in the pavement structure propagate through an overlay due to thermal and traffic-induced movement, ultimately degrading the pavement’s lifespan and performance. This study aims to determine how alterations in overlay thickness and temperature conditions, the incorporation of chopped fibers, and the use of geotextiles influence the overlay’s capacity to postpone the occurrence of reflection cracking. To achieve the above objective, a total of 36 prism specimens were prepared and tested using an overlay testing machine (OTM). The variables considered in this study were the thickness of the
... Show MoreMoisture induced damage in asphaltic pavement might be considered as a serious defect that contributed to growth other distresses such as permanent deformation and fatigue cracking. This paper work aimed through an experimental effort to assess the behaviour of asphaltic mixtures that fabricated by incorporating several dosages of carbon fiber in regard to the resistance potential of harmful effect of moisture in pavement. Laboratory tests were performed on specimens containing fiber with different lengths and contents. These tests are: Marshall Test, the indirect tensile test and the index of retained strength. The optimum asphalt contents were determined based on the Marshall method. The preparation of asphaltic mixtures involved
... Show MoreThe inhibition of mild steel corrosion in 1.0M HCl by 1-propanol and the synergistic effect of potassium iodide (KI) was investigated using weight loss and polarization techniques in the temperature range (30 ‒ 50) ̊ C. A matrix of Doelhert to three factors was used as the experimental design, adopting weight loss results as it permits the use of the response surface methodology which exploited in determination of the synergistic effect as inhibition on the mild steel. The results were confirmed using electrochemical polarization measurements. Experimental results showed that the inhibition efficiency (IE%) increases with increase in concentration of inhibitor and with increasing of temperature. The addition iodide ions t
... Show MoreIn this work, the effect of anodizing duration on the morphology and photoelectrochemical properties of TiO2 nanotubes arrays (NTAs) has been investigated The samples were characterized by X-ray diffraction (XRD) and energy dispersive X-ray (EDX) to characterize their crystalline structure and compositional. Surface morphological and their dimensional variation was examined by field emission scanning electron microscopy (FESEM). The anodizing duration played a significant role in the formation of TiO2 nanotubes arrays. Moreover, the photoelectrochemical properties (PEC) were studied through photocurrent measurements. Optimum anodizing duration of 60 min at 40 V exhibited maximum photocurrent of 0.03 mA cm-2 under illumination of hal
... Show MoreExperimental investigations had been done in this research to demonstrate the effect of carbon fiber and Ceramic fillers contents on the tribological behaviour of (15% volume fraction) carbon-epoxy composite system under varying volume fraction, load, time and sliding distance. The wear resistance were investigated according to ASTM G99-05standard using pin on disc machine to present the composite tribological behaviour. The influence of three ceramic fillers, granite, perlite and calcium carbonate (CaCO3), on the wear of the carbon fabric reinforced epoxy composites under dry sliding conditions has been investigated. The effect of variants in volume fraction, applied load, time and sliding distance on the wear behaviour of po
... Show MoreNanofertilizers offer a promising solution to increase crop yields amid increasing population pressure. Yet there have been safety concerns about their use, particularly in challenging conditions. This work was designed to assess the toxicological effects of a chelated multi-micronutrient nanofertilizer on albino rats (Rattus norvegicus) as non-target organisms, focusing on the liver, which has important metabolic functions. Thirty-five animals were weighed and randomly divided into 5 groups (n=7). A negative control group was included, and four experimental groups (C1-C4) were given the test item. The dosing regimen for the experimental groups was 15 oral doses of nanofertilizer every other day for 29 days. All the groups were
... Show MoreIn the recent years, some of the newly constructed asphalt concrete pavements in Baghdad as well as other cities across Iraq showed premature failures with consequential negative impact on both roadway safety and economy. Frequently, load associated mode of failure (rutting and fatigue) as well as, occasionally, moisture damage in some poorly drained sections are the main failure types found in those newly constructed road.
In this research, hydrated lime was introduced into asphalt concrete mixtures of wearing course in two methods. The first one was the addition of dry lime on dry aggregate and the second one was the addition of dry lime on saturated surface dry aggregate moisturized by 2.0 to 3.0 percent of wa